Multilayered SiOx/SiO2 and SiOxNy/SiO2 thin films were fabricated using different techniques and subsequently annealed at high temperatures (≥1100 °C) in order to form Si nanocrystals by means of the well-known superlattice approach. The thickness of the SiOx and SiOxNy layers was varied from 1.5 to 5 nm, while for the SiO2 layers it was fixed at 4 nm. Using transmission electron microscopy, we showed that the multilayered structure generally sustains the high temperature annealing for both types of films. However, for samples with ultrathin SiOx or SiOxNy layers a breakdown of the superlattice structure and a complete intermixing of layers were observed at high temperatures. On the contrary, annealing at lower temperature (900 °C) preserves the multilayered structure even of such samples. Theoretical calculations showed that the intermixing of SiOx/SiO2 and SiOxNy/SiO2 superlattices in the ultrathin layers thickness limit may be explained thermodynamically by the gain in the Gibbs free energy, which depends in turn on the annealing temperature.
We report on an in-situ oxidation effect during annealing of SiO2/SiO1.0N0.23 multilayers prepared by plasma enhanced chemical vapour deposition (PECVD). This in-situ oxidation leads to an undesired growth of the tunneling oxide and also affects the silicon nanocrystal (SiNC) size control, i.e., a NC shrinkage. The origin of this oxidation is identified to be a “quasi-wet” oxidation by O–H groups incorporated in the PECVD-SiO2 barrier layers. By varying the thickness of the PECVD-SiO2 layer underneath a single SiO1.0N0.23 layer, the extent of NC oxidation is tuned. The shrinkage of SiNCs is proven by a blueshift of the photoluminescence peak position as well as by transmission electron microscopy.