Shujing Zhao

Shujing Zhao

Auto-generated profile, based on publicly available information

Shujing Zhao

School of Microelectronics, Xi'an Jiaotong University 1 , Xi'an 710049

Research Focus & Metrics

Academic Career Length

6Years (2021-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
5 October 2021 in IEEE Transactions on Electron Devices
Verified
Journal Article
Closed access
FTFengbin Tian
Fengbin Tian
SZShujing Zhao
Shujing Zhao
HXHao Xu
Hao Xu
JXJinjuan Xiang
Jinjuan Xiang
TLTingting Li
Tingting Li
TYTianchun Ye
Tianchun Ye
We study the impact of different interlayers (ILs) and ferroelectric materials on charge trapping during the endurance fatigue of Si ferroelectric field effect transistor (FeFET) with TiN/Hf x Zr 1-x O 2 / interlayer/Si (MFIS) gate-stack. We have fabricated FeFET devices with different interlayers (SiO 2 or SiON) and Hf x Zr 1-x O 2 materials ( ${x} =0.75$ , 0.6, 0.5) and directly extracted the charge trapping during endurance fatigue. We find that: 1) under the same equivalent oxide thickness (EOT) condition, the increase of dielectric constant and interlayer thickness suppresses charge trapping and improves the endurance characteristics; 2) charge trapping effect is experimentally verified to be the origin of endurance fatigue; and 3) as the spontaneous polarization ( ${P}_{\text {s}}{)}$ of the Hf x Zr 1-x O 2 decreases from $25.9~ \boldsymbol {\mu } \text{C}$ /cm 2 (Hf 0.5 Zr 0.5 O 2 ) to $20.3~ \boldsymbol {\mu } \text{C}$ /cm 2 (Hf 0.6 Zr 0.4 O 2 ), the charge trapping behavior decreases, resulting in the slow degradation rate of memory window (MW) during program/erase cycling; in addition, when ${P}_{\text {s}}$ further decreases to $8.1~ \boldsymbol {\mu }\text{C}$ /cm 2 (Hf 0.75 Zr 0.25 O 2 ), the initial MW nearly disappears (only ~0.02 V). Thus, the reduction of ${P}_{\text {s}}$ could improve endurance characteristics. On the contrary, it can also reduce the MW. Our work helps design the MFIS gate-stack to improve endurance characteristics.

17 January 2022 in IEEE Transactions on Electron Devices
Verified
Journal Article
Closed access
SZShujing Zhao
Shujing Zhao
FTFengbin Tian
Fengbin Tian
HXHao Xu
Hao Xu
JXJinjuan Xiang
Jinjuan Xiang
TLTingting Li
Tingting Li
TYTianchun Ye
Tianchun Ye
We investigate the charge trapping during endurance fatigue of FeFET with TiN/Hf 0.5 Zr 0.5 O 2 /SiO 2 /Si (MFIS) gate structure. We propose a method of experimentally extracting the number of trapped charges during the memory operation, by measuring the charges in the metal gate and Si substrate. We verify that the amount of trapped charges increases during the endurance fatigue process. This is the first time that the trapped charges are directly experimentally extracted and verified to increase during endurance fatigue. Moreover, we model the interplay between the trapped charges and ferroelectric polarization switching during endurance fatigue. Through the consistency of experimental results and simulated data, we demonstrate that as the memory window (MW) decreases: 1) the ferroelectric characteristic of Hf 0.5 Zr 0.5 O 2 is not degraded; 2) the trap density in the upper bandgap of the gate stacks increases; and 3) the reason for MW decrease is increased trapped electrons after program operation but not related to hole trapping/detrapping. Our work is helpful to study the charge trapping behavior of FeFET and the related endurance fatigue process.

18 April 2023 in IEEE Transactions on Electron Devices
Verified
Journal Article
Closed access
XSXianzhou Shao
Xianzhou Shao
JCJun-Shuai Chai
Jun-Shuai Chai
FTFengbin Tian
Fengbin Tian
SZShujing Zhao
Shujing Zhao
JDJiahui Duan
Jiahui Duan
TYTianchun Ye
Tianchun Ye
We propose an in situ ${V}_{\text {th}}$ measurement method to investigate the endurance fatigue mechanism of Si ferroelectric field-effect transistor (FeFET) with HfZrO ferroelectric. The in situ ${V}_{\text {th}}$ measurement method means that a pulsed current-voltage measurement is embedded during the quasi-static capacitance-voltage (QSCV) measurement. Based on this method, the trapped charges can be extracted as a function of the gate voltage ( ${V}_{g}{)}$ . We find that: First, the trapped electrons and holes show asymmetric de-trapping dynamics. Excess electrons continuously de-trap within the ${V}_{g}$ ranging from the maximum positive value to ferroelectric reverse switching. However, the trapped holes do not de-trap when the ${V}_{g}$ changes from the minimum negative value to 0 V. Second, the increase of donor trap density is the key to endurance fatigue. During endurance fatigue, the total amounts of trapped electrons are unchanged near the maximum positive voltage, but the amounts of de-trapped electrons decrease when the ${V}_{g}$ returns to 0 V due to donor trap density increases. In addition, we apply our method in the scaled FeFET to overcome the measurement limitation of gate charges ( ${Q}_{m}{)}$ by the nowadays equipment.

3 November 2022 in IEEE Transactions on Electron Devices
Verified
Journal Article
Closed access
JDJiahui Duan
Jiahui Duan
SZShujing Zhao
Shujing Zhao
FTFengbin Tian
Fengbin Tian
JXJinjuan Xiang
Jinjuan Xiang
KHKai Han
Kai Han
TYTianchun Ye
Tianchun Ye
This work investigates trap generation in gate stacks of ferroelectric field-effect transistor (FeFET) with TiN/Hf $_{\text{0.5}}$ Zr $_{\text{0.5}}$ O $_{\text{2}}$ /SiO $_{\textit{x}}$ /Si gate structure during endurance fatigue by using the low-frequency noise method. We find that the traps are generated not only at Hf $_{\text{0.5}}$ Zr $_{\text{0.5}}$ O $_{\text{2}}$ /SiO $_{\textit{x}}$ interface but also in both the Hf $_{\text{0.5}}$ Zr $_{\text{0.5}}$ O $_{\text{2}}$ and SiO $_{\textit{x}}$ . Our work provides evidence of defect generation inside the ferroelectric layer of FeFET during cycling. Furthermore, the traps in the SiO $_{\textit{x}}$ are more detrimental to endurance fatigue. And the trap generation in the SiO $_{\textit{x}}$ is more important than its initial trap density for endurance fatigue. Our work is helpful in deeply understanding the endurance of FeFET.

10 November 2022 in IEEE Transactions on Electron Devices
Verified
Journal Article
Closed access
JCJun-Shuai Chai
Jun-Shuai Chai
HXHao Xu
Hao Xu
JXJinjuan Xiang
Jinjuan Xiang
YZYuanyuan Zhang
Yuanyuan Zhang
SZShujing Zhao
Shujing Zhao
TYTianchun Ye
Tianchun Ye
This work investigates the endurance characteristic of Si FeFET with Hf $_{\text{0.5}}$ Zr $_{\text{0.5}}$ O $_{\text{2}}$ ferroelectric. A fully CMOS-compatible method is shown to improve endurance: insertion of the thin HfO $_{\textit{x}}$ layer ( $\sim$ 2–5 Å) at the Hf $_{\text{0.5}}$ Zr $_{\text{0.5}}$ O $_{\text{2}}$ /SiO $_{\textit{x}}$ interface. The ab initio calculations prove that the HfO $_{\textit{x}}$ insertion can increase the formation energies of oxygen vacancies and suppress their generation in the gate stacks and, consequently, improve the endurance. This method paves a possible path to improve the endurance of Si FeFET.

26 June 2023 in IEEE Transactions on Electron Devices
Verified
Journal Article
Closed access
MLMin Liao
Min Liao
HXHao Xu
Hao Xu
JDJiahui Duan
Jiahui Duan
SZShujing Zhao
Shujing Zhao
FTFengbin Tian
Fengbin Tian
XWXiaolei Wang
Xiaolei Wang
We investigate the impact of saturated spontaneous polarization ( $\textit{P}_{\text{s}}\text{)}$ of the ferroelectric on endurance fatigue of Si FeFET with Metal/Ferroelectric/Interlayer/Si (MFIS) gate structure. We tune the $\textit{P}_{\text{s}}$ in the range of 25.9–6.4 $\mu$ C/cm $^{\text{2}}$ by changing the gate structure, such as the insertion of a dielectric layer and annealing temperature. When the $\textit{P}_{\text{s}}$ decreases from 12.1 to 6.4 $\mu$ C/cm $^{\text{2}}$ , the memory window of the device decreases while the endurance improves. When the $\textit{P}_{\text{s}}$ decreases from 12.1 to 8.1 $\mu$ C/cm $^{\text{2}}$ , the memory window disappears. However, when the $\textit{P}_{\text{s}}$ is lower than 8.1 $\mu$ C/cm $^{\text{2}}$ , the memory window reappears. Smaller $\textit{P}_{\text{s}}$ leads to a smaller memory window, which reduces the read noise margin of the memory and is disadvantageous to endurance. Whereas smaller $\textit{P}_{\text{s}}$ leads to weaker charge trapping behavior, which is advantageous to endurance. Our work shows that the endurance characteristic is determined by the competition between the above two processes.