Irena Paulin

Irena Paulin

Auto-generated profile, based on publicly available information

Irena Paulin

Inst Met & Technol, Lepi Pot 11, Ljubljana 1000, Slovenia

Research Focus & Metrics

Academic Career Length

6Years (2021-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
4 July 2024 in Journal of Materials Research and Technology
Verified
Journal Article
Open access
ABAnna Boukalová
Anna Boukalová
JKJiri Kubasek
Jiri Kubasek
DNDavid Nečas
David Nečas
PMPeter Minárik
Peter Minárik
ČDČrtomir Donik
Črtomir Donik
IPIrena Paulin
Irena Paulin

7 May 2024 in Journal of Materials Research and Technology
Verified
Journal Article
Open access
DVDalibor Viderščak
Dalibor Viderščak
ZSZdravko Schauperl
Zdravko Schauperl
MGMatjaž Godec
Matjaž Godec
ČDČrtomir Donik
Črtomir Donik
IPIrena Paulin
Irena Paulin
DPDaniel Pustički
Daniel Pustički

30 September 2021 in Materiali in tehnologije
Verified
Journal Article
Closed access
PDF file
ALAlenka Šalej Lah
Alenka Šalej Lah
MVMaja Vončina
Maja Vončina
IPIrena Paulin
Irena Paulin
JMJožef Medved
Jožef Medved
PFPeter Fajfar
Peter Fajfar
DVDarja Volšak
Darja Volšak
The influence of chemical composition and heat treatment on the mechanical properties and formability of the selected commercial aluminium alloy EN AW 5454 was investigated. The main properties of alloy 5454 from the AA 5xxx series are very good corrosion resistant and has good formability. From the cast slab a 50 mm thick slice was taken in the width cross section in the slab centre. One half of the slice was homogenised for 10 hours at a temperature of 530 °C. The cast and homogenised samples were investigated using light and scanning electron microscopy. For the study of the influence of the heat treatment, samples in the as-cast state were annealed in the laboratory furnace at a temperature of 530 °C for 4, 6, 8, 10 and 12 hours. To study the influence of chemical composition, four different samples were prepared: the first without additions, the second with an addition of 1 wt% Mn, the third with 3 wt% Mg and the fourth with an addition of both elements, Mn and Mg. The XRF analyses confirmed the desired chemical composition of all four produced alloys. Half of each alloy’s sample was homogenised at the same temperature and time as the base alloy in the as-cast state. The hot deformation behaviour of the different alloys was investigated using cylindrical hot compression tests performed on a Gleeble 1500D thermo-mechanical simulator. By comparing flow curves a high influence of the thermo-mechanical parameters on the alloy formability can be seen. The alloy has good workability and with the addition of Mn and Mg, the stress values are higher than those of the base alloy.

16 April 2024 in Journal of Materials Research and Technology
Verified
Journal Article
Open access
MGMatjaž Godec
Matjaž Godec
JKJakob Kraner
Jakob Kraner
DBDanijela Skobir Balantič
Danijela Skobir Balantič
IPIrena Paulin
Irena Paulin
Damjana DrobneDamjana Drobne
Damjana Drobne
ČDČrtomir Donik
Črtomir Donik

14 February 2026 in Journal of Materials Research and Technology
Verified
Journal Article
Open access
Anna DobkowskaAnna Dobkowska
Anna Dobkowska
KDKalyan Das
Kalyan Das
Mirosław Jakub KruszewskiMirosław Jakub Kruszewski
Mirosław Jakub Kruszewski
AZAleksandra Zielińska
Aleksandra Zielińska
MGMarlene Aydee Gonzalez Garcia
Marlene Aydee Gonzalez Garcia
MGMatjaž Godec
Matjaž Godec

15 July 2025 in Journal of Materials Research and Technology
Verified
Journal Article
Open access
JKJiri Kubasek
Jiri Kubasek
STSelase Torkornoo
Selase Torkornoo
DNDavid Nečas
David Nečas
IMIngrid McCarroll
Ingrid McCarroll
VHVojtech Hybasek
Vojtech Hybasek
JČJaroslav Čapek
Jaroslav Čapek