SiCp/6061Al composites have been developed and widely applied in many fields, such as automobile, aerospace, shipping, and so on. Considering heat treatment, service environment, and strength of composites, this paper comprehensively studies the mechanical properties of SiCp/6061Al composites with a large range of SiC mass fractions under T6 treatments and different tensile temperatures. SiCp/6061Al composites were successfully prepared by hot press sintering at various SiC mass fractions (0–30%), and the influences of SiC concentration and T6 treatment on the mechanical properties of composites were characterized via tensile tests at room temperature, 100, and 200 °C. Microstructure and fracture surfaces of composites with various SiC concentrations were further analyzed by optical microscope and SEM. The formula for the biggest critical reinforcement concentration for the saturated distribution of SiC is proposed to reveal the strengthening rule of different SiC concentrations. Results show that the effect of T6 treatment on the mechanical properties of composites is a marked increase in tensile strength and an obvious decrease in elongation. The increase in the SiC mass fraction, except at 30%, is able to bring an increase in tensile strength and a decrease in elongation, and the change of the elongation is insignification in T6-treated specimens. The tensile strength of T6-treated specimens decreases as temperature increases, and the composite has a maximum elongation at 100 °C.
Due to its high specific strength and low coefficient of thermal expansion, Al/SiCp homogenous composites (HC) have become a widely used material in automobile and other fields. The application of components with different internal and external material performance requirements such as automobile pistons and brake disks has promoted the development of functionally graded materials (FGM). Therefore, Al/SiCp composites are expected to be applied on a large scale. Al6061/SiCP composites were prepared by vacuum hot-pressed sintering whose microstructure observation is carried out and mechanical properties are tested. The hardness of the Al/SiC HC increases gradually as the SiC content increases from 0 to 30 wt.%. The hardness values of the T6-treated Al6061/SiCp HC with SiC mass fractions of 0, 5, 10, 15, 20, 25, and 30% are 97, 101, 104, 111, 113, 118, and 125HV, respectively, and it is a maximum increase of 117.48% compared with HC without T6 treatment. The flexural strength increases and the deflection decreases with the increase of SiC content, and T6 heat treatment also improves the flexural strength of all composites with about 30% increase over that without T6 heat treatment. When the load was applied from the layer with high SiC content of FGM whose interlayer difference is 5%, the strength and deflection were superior to those of the HC.