HfO2-based ferroelectric (FE–HfO2) is a promising material for low-power and high-capacity memory technology. Since thinner ferroelectric films are required for low voltage operation, the impact of film thickness on the switching kinetics of FE–HfO2 needs to be studied in detail. In this paper, metal/ferroelectric/metal capacitors are fabricated with several thicknesses of HfZrO2 (HZO) films and characterized to study the switching kinetics based on the nucleation limited switching (NLS) model. Thinner HZO capacitors show slower polarization switching and asymmetry in program and erase operation, although low-frequency polarization charge density is nearly the same for all thicknesses. Slow switching is due to the large variability of the activation field of FE domains and grain boundaries among small FE grains. The asymmetry is caused by the asymmetric interface property at the top and bottom interfaces. High-resolution TEM and electron diffraction mapping methods provide physical evidence for the above discussions.
17 September 2025 in IEEE Transactions on Electron Devices
In this article, we report performance enhancement and reliability improvement of oxide semiconductor FETs (OS FETs) by polycrystalline Ga-doped InOx (poly-IGO). Atomic layer deposition (ALD) and post-deposition annealing (PDA) were employed to achieve crystallization of IGO. A systematic study of bottom-gate (BG) FETs with varied Ga concentrations and film thicknesses identified optimized conditions yielding a mobility up to 81 cm2/V ⋅ s. Low-temperature measurements were conducted to physically understand the mobility improvement. The carrier transport mechanisms were discussed. Then, we developed a novel selective crystallization method in the OS stack for process integration and device operation of gate-all-around (GAA) nanosheet (NS) IGO FETs. The fabricated GAA IGO FETs showed normally-OFF operation, high ON-current of 326 μA/μm, and a steep subthreshold slope of 68 mV/dec. In addition, GAA NS FETs exhibited further improved bias stress stability. This work provides a scalable strategy of poly-OS channels for monolithic 3-D (M3D) integration and 3-D memory such as 3-D DRAM and 3-D NAND.
18 January 2023 in Japanese Journal of Applied Physics
A series resistance extraction method proposed recently, which uses multiple drain current versus gate voltage curves at varied drain voltages, was applied to bulk CMOS devices at low temperatures down to 4 K. A moderate reduction of series resistance compared with 300 K was found. Horizontal field dependence of mobility significantly changed with temperature, which was taken into account during the extraction. Anomalous non-linear series resistance was observed at 4 K only for p-channel FETs, suggesting the need for careful source/drain overlap design for low temperature operations.
10 February 2022 in Japanese Journal of Applied Physics
A simple MOSFET series resistance extraction method using multiple drain current versus gate voltage curves of a single device is proposed, where mobility modulation by a horizontal electric field (i.e., weak velocity saturation) is taken into account. The method is validated using TCAD, where series resistance determined from internal potential distributions was used as a reliable reference. Measurement results were also obtained which further support the validity of the method.
1 April 2022 in Japanese Journal of Applied Physics
We analyzed the operating principle of field-limiting ring edge termination, a technique widely used in vertical Si and SiC power devices, by employing a simplified quasi-2D three-terminal TCAD model representing a vertical stripe region with two half rings. We confirmed that the voltage between adjacent rings corresponds to the punch-through voltage of a horizontal PNP structure, which is determined by both the ring-to-ring spacing and the potential difference between the rings and the cathode. Fixed charge and metal field plates further affect the termination characteristics by modulating the punch-through behavior. This model provides an intuitive explanation for why the ring pitch must gradually increase from the inner to the outer rings to achieve area-efficient termination.