21 November 2022 in IEEE Journal of Selected Topics in Quantum Electronics
InP DFB lasers are flip-chip bonded to 300mm Si photonic wafers using a pick-and-place tool with an advanced vision system, realizing high-precision and high-throughput passive assembly. By careful co-design of the InP-Si Photonics electrical, optical and mechanical interface, as well as dedicated alignment fiducials, sub-300nm post-bonding alignment precision is realized in a 25s cycle time. Optical coupling losses of -1.5±-0.5dB are achieved at 1550nm wavelength after epoxy underfill, with up to 40 mW of optical power coupled to the SiN waveguides on the Si photonics wafer. The bonding interface adds less than 10% to the series resistance of the laser diodes and post-bonding thermal resistance is measured to be 76K/W (or 27K.mm/W), mostly dominated by heat spreading resistance in the InP lasers as suggested by in-depth thermal modeling. Although the assembled lasers suffer from significant, unintentional optical backreflection from the fiber grating couplers used for optical characterization, laser linewidths well below 1MHz have been measured under specific drive conditions, as supported by a detailed laser noise analysis. Finally, we demonstrate the ability of bonded laser assemblies to pass early reliability tests.
2 May 2019 in IEEE Photonics Technology Letters
A simple optical circuit made by a cascade of two graphene-on-silicon EAMs of different length is used for the optical pre-emphasis of 10 Gb/s non-return-to-zero (NRZ) signals by delay-inverse-weight compensation. Transmission up to 100 km on single mode fiber (SMF) without dispersion compensation is reported, showing also the large performance advantage (6 dB in back-to back, around 5 dB in transmission) in respect of the conventional single EAM transmitter configuration.
24 February 2013 in Microelectronic Engineering
1 October 2010 in ECS Transactions
High porosity and carbon doing are required to achieve low dielectric constant, k values for ultra low-k (ULK) materials based on silicon dioxide. Those characteristics create new challenges in the integration of ULK materials that are being developed for future interconnect scaling. Four of those challenges based on electrical characterizations of ULK films will be presented in this paper. First, a high concentration of porogen residue is typically present in ULK materials fabricated by Plasma Enhanced Chemical Vapor Deposition (PECVD). The high porogen residue concentration leads to a high leakage current density. Second, ULK materials based on Spin-on Glass (SOG) process demonstrate a low leakage current density. But early dielectric breakdown has been observed in SOG k=2.2 material. Third, PVD TaNTa barrier process can introduce significant damage to ULK materials. The damage level increases as the k value decreases or porosity increases. Four, direct deposition of ALD Ru barrier on ULK films results in a high leakage current density.