The critical size limit of voltage-switchable electric dipoles has extensive implications for energy-efficient electronics, underlying the importance of ferroelectric order stabilized at reduced dimensionality. We report on the thickness-dependent antiferroelectric-to-ferroelectric phase transition in zirconium dioxide (ZrO2) thin films on silicon. The emergent ferroelectricity and hysteretic polarization switching in ultrathin ZrO2, conventionally a paraelectric material, notably persists down to a film thickness of 5 angstroms, the fluorite-structure unit-cell size. This approach to exploit three-dimensional centrosymmetric materials deposited down to the two-dimensional thickness limit, particularly within this model fluorite-structure system that possesses unconventional ferroelectric size effects, offers substantial promise for electronics, demonstrated by proof-of-principle atomic-scale nonvolatile ferroelectric memory on silicon. Additionally, it is also indicative of hidden electronic phenomena that are achievable across a wide class of simple binary materials.
We demonstrate ferroelectric (FE) memory transistors on a crystalline silicon channel with endurance exceeding 10 10 cycles. The ferroelectric transistors (FeFETs) incorporate a high- $\kappa $ interfacial layer (IL) of thermally grown silicon nitride (SiN x ) and a thin 4.5 nm layer of Zr-doped FE-HfO 2 (HZO) on a ~30 nm silicon on insulator (SOI) channel. The device shows a ~1V memory window (MW) in a DC sweep of just ± 2.5V, and can be programmed and erased with voltage pulses of $\text {V}_{\text {G}}= \pm \,\,3\text{V}$ at a pulse width of 250 ns. The device also shows very good retention behavior. These results indicate that appropriate engineering of the IL layer could substantially improve FeFET device performance and reliability.
We report on negative capacitance FETs (NCFET) with 1.8 nm thick Zr-doped HfO2 gate oxide layer, fabricated on a FDSOI wafer. Hysteresis-free operation is demonstrated. When compared to a baseline that uses HfO2 gate oxide with the same thickness, a subthreshold swing (SS) steeper by more than 20mV/decade and larger than 10X reduction in the OFF current (IOFF) is observed at 30nm channel length, at a constant ION. On the other hand, at matched IOFF, NCFET provides a larger ON current at constant VDD. Our results indicate that the beneficial characteristic offered by NCFETs can be obtained at scaled channel lengths, while using oxide layers whose thickness is comparable to the high-K oxide layer used in ultra-scaled nodes.