29 January 2015 in ACS Applied Materials & Interfaces
Molecular monolayer doping (MLD) presents an alternative to achieve doping of silicon in a nondestructive way and holds potential for realizing ultrashallow junctions and doping of nonplanar surfaces. Here, we report the mixing of dopant-containing alkenes with alkenes that lack this functionality at various ratios to control the dopant concentration in the resulting monolayer and concomitantly the dopant dose in the silicon substrate. The mixed monolayers were grafted onto hydrogen-terminated silicon using well-established hydrosilylation chemistry. Contact angle measurements, X-ray photon spectroscopy (XPS) on the boron-containing monolayers, and Auger electron spectroscopy on the phosphorus-containing monolayers show clear trends as a function of the dopant-containing alkene concentration. Dynamic secondary-ion mass spectroscopy (D-SIMS) and Van der Pauw resistance measurements on the in-diffused samples show an effective tuning of the doping concentration in silicon.
14 December 2020 in IEEE Journal of Emerging and Selected Topics in Power Electronics
This paper investigates a novel approach to the integration of multi-layer thin film magnetics embedded in PCB for use in Power Supply in Package (PwrSip) applications. A solenoid inductor structure is formed by sandwiching a multi-layer CZTB magnetic sheet between two distinct PCBs with copper tracks on each which form the upper and lower windings of the device. A solder reflow process, utilizing solder balls mounted on the exposed NiAu pads of one of the PCBs, is used to create the electrical connection between the two boards, hence forming closed current loops for the windings of the inductor. This novel inductor structure enables the use of net 4oz (140 μm) copper to enclose the multi-layer CZTB magnetic sheet, and hence demonstrates very low Rdc. The multi-layer CZTB magnetic sheet was characterized using a Ryowa Permeameter. The magnetic sheet exhibited a permeability of 367. The manufactured Flip-Chip inductor was electrically characterized using a Vector Network Analyser. The device has a footprint of 7.25 mm2 and has an inductance of 52nH. The fabricated PCB embedded inductor achieved a peak quality factor of 23 at 40 MHz.
6 May 2021 in IEEE Journal of Emerging and Selected Topics in Power Electronics
This work presents analytical expressions for the dc inductance of 3-D air-core inductors with circular cross-sectional pillars (CCSPs) and rectangular cross-sectional pillars (RCSPs). We consider the following four types of inductor structures: 1) a toroid with CCSP; 2) a toroid with RCSP; 3) a solenoid with RCSP; and 4) a solenoid with CCSP. For each type, a unique analytical model is developed for obtaining dc inductance. High-frequency (1–100 MHz) effects on inductance are also discussed. The inductance values predicted by the proposed analytical models of the first three types of inductor structures are in an acceptable agreement with numerical finite-element analysis (FEA) solutions, where the maximum difference is 7.3%. Also, our analytical model for the fourth-type inductor reduces the error, when correlated with FEA inductance value, up to $6\times $ compared with previously published models. A comparison of results using the proposed analytical expressions with published measured values as well as our measurement data demonstrates the error ranging from 0.5% to 16.2%, while conventional formulas show errors of up to 143%. The results of the proposed models could serve as a good initial estimate for power supply-on-chip (PwrSoC) and power supply in package (PSiP) applications.
14 October 2021 in Journal of Materials Science: Materials in Electronics
1 March 2023 in AIP Advances
Melt-spun Fe-based ribbons are widely used as the core of transformers and inductors due to their high flux density and low coercivity. However due to their high thickness (∼19 µm) these ribbons are prone to large eddy current losses at MHz frequencies. Despite low yield, ball milling has been widely used to break such ribbons down to thinner flakes to suppress the eddy current losses at high frequency. In this work, we demonstrated an optimized ball milling process with increased yield for flakes in the desired size range (2–4 µm). We have demonstrated that reducing pre milling annealing temperature from 450 to 350 °C increases the yield in desired size range from 2% to 5% and further increasing batch size from 10 to 20 g increases the yield to 21%. The coercivity of the milled flakes increases from 139 to 1352 A/m due to the ball milling process. A post-mill annealing at 350 °C in Ar atmosphere decreases the coercivity to 341 A/m. X-ray diffraction analysis showed no sign of crystallization during ball milling. The result presented here demonstrates an efficient approach to fabricate ultra-thin flakes out of soft magnetic ribbons for high-frequency applications.