This work presents analytical expressions for the dc inductance of 3-D air-core inductors with circular cross-sectional pillars (CCSPs) and rectangular cross-sectional pillars (RCSPs). We consider the following four types of inductor structures: 1) a toroid with CCSP; 2) a toroid with RCSP; 3) a solenoid with RCSP; and 4) a solenoid with CCSP. For each type, a unique analytical model is developed for obtaining dc inductance. High-frequency (1–100 MHz) effects on inductance are also discussed. The inductance values predicted by the proposed analytical models of the first three types of inductor structures are in an acceptable agreement with numerical finite-element analysis (FEA) solutions, where the maximum difference is 7.3%. Also, our analytical model for the fourth-type inductor reduces the error, when correlated with FEA inductance value, up to $6\times $ compared with previously published models. A comparison of results using the proposed analytical expressions with published measured values as well as our measurement data demonstrates the error ranging from 0.5% to 16.2%, while conventional formulas show errors of up to 143%. The results of the proposed models could serve as a good initial estimate for power supply-on-chip (PwrSoC) and power supply in package (PSiP) applications.
1 June 2020 in Journal of Magnetism and Magnetic Materials
FeSiB based soft magnetic flakes (SMFs; ϕ: 63-106 µm, t: 2-5 µm) coated with optimally thick (∼10 nm) SiO2 were fabricated as the potential magnetic material for pressed cores suitable for use in power inductors operating beyond 10 MHz. Such thin SMFs were produced by mechanical ball milling of commercially available thick (∼27 µm) ribbons followed by an optimized sol-gel coating in presence of a silane coupling agent. Milling helped to reduce ribbon thickness below the skin depth to minimize eddy current loss at high frequencies. The effect of milling (medium, duration, rotation speed, and ball-to-powder ratio) and coating conditions on the soft magnetic properties of the SMFs were investigated. An optimally tiny fraction of the milled flakes was allowed to become nanocrystalline, which augments saturation flux density (BS) and permeability (µ) without incurring additional losses. The results from X-Ray photoelectron spectroscopy and magnetization measurement confirm that a stress-releasing post-annealing process reduced coercivity from ∼62 Oe to ∼6 Oe and enhanced the magnetic saturation moment from 126 emu/g to 142 emu/g without affecting the thin yet robust insulating SiO2 layer.
Melt-spun Fe-based ribbons are widely used as the core of transformers and inductors due to their high flux density and low coercivity. However due to their high thickness (∼19 µm) these ribbons are prone to large eddy current losses at MHz frequencies. Despite low yield, ball milling has been widely used to break such ribbons down to thinner flakes to suppress the eddy current losses at high frequency. In this work, we demonstrated an optimized ball milling process with increased yield for flakes in the desired size range (2–4 µm). We have demonstrated that reducing pre milling annealing temperature from 450 to 350 °C increases the yield in desired size range from 2% to 5% and further increasing batch size from 10 to 20 g increases the yield to 21%. The coercivity of the milled flakes increases from 139 to 1352 A/m due to the ball milling process. A post-mill annealing at 350 °C in Ar atmosphere decreases the coercivity to 341 A/m. X-ray diffraction analysis showed no sign of crystallization during ball milling. The result presented here demonstrates an efficient approach to fabricate ultra-thin flakes out of soft magnetic ribbons for high-frequency applications.