Technical University of Munich; TUM School of Natural Sciences, Department of Chemistry and Catalysis Research Center, Chair of Technical Electrochemistry, Garching, Germany
Auto-generated profile, based on publicly available information
Leonhard J. ReinschlüsSel
Technical University of Munich; TUM School of Natural Sciences, Department of Chemistry and Catalysis Research Center, Chair of Technical Electrochemistry, Garching, Germany
Operating lithium-ion batteries (LIBs) to high charging cut-off potentials allows us to accommodate a further push in energy density. However, it requires a thorough understanding of the interplay and temperature dependence of parasitic reactions that aggravate the aging of the electrolyte and the cathode/anode electrodes. In the present study we investigated the interplay of the chemical and the electrochemical electrolyte oxidation, how they are related to the dissolution of transition metal (TM) ions from the cathode active material (CAM), and how they shift or accelerate with temperature. Through an optimized electrochemical protocol an excellent potential dependence of the gas evolution of a LiNi0.80Co0.15Al0.05O2 (NCA) charged against a free-standing graphite on a lithium metal electrode in a LP47 electrolyte was achieved. We identified O2 and PF5 gas as suitable proxies for the chemical and electrochemical electrolyte oxidation, respectively. Both processes are separated by at least 300 mV over a temperature range from 10 to 45 °C. Through temperature-dependent operando hard X-ray absorption spectroscopy measurements and their comparison with the gassing results, it will be shown, that the electrochemical oxidation of the electrolyte is directly linked to the dissolution of TMs, while the chemical electrolyte oxidation mainly leaves the transition metal dissolution unaffected.
1 October 2024 in Journal of the Electrochemical Society
Detecting parasitic side reactions is paramount for developing stable cathode active materials (CAMs) for Li-ion batteries. This study presents a method for the quantification of released lattice oxygen and transition metal ions (TMII+ ions). It is based on a 3-electrode cell design employing a Vulcan carbon-based sense electrode (SE) that is held at a controlled voltage against a partially delithiated lithium iron phosphate (LFP) counter electrode (CE). At this SE, reductive currents can be measured while polarizing a CAM working electrode (WE), here a LiNi0.80Co0.15Al0.05O2 (NCA), against the same LFP CE. In voltammetric scans, we show how the SE potential can be selected to specifically detect a given side reaction during CAM charge/discharge, allowing, e.g., to discriminate between lattice oxygen and dissolved TMs. Furthermore, it is shown via online electrochemical mass spectrometry (OEMS) that O2 reduction in the here-used LP47 electrolyte consumes ∼2.3 electrons/O2. Using this value, the lattice oxygen release deduced from the 3-electrode setup upon charging of the NCA WE is in good agreement with OEMS measurements up to NCA potentials >4.65 VLi. At higher potentials, the contributions from the reduction of TMII+ ions can be quantified by comparing the integrated SE current with the O2 evolution from OEMS.
Exposure of cathode active materials (CAMs) to ambient air is particularly detrimental for Ni-rich CAMs, leading to accelerated performance degradation. Upon storage, H2O and CO2 from ambient air react with the CAM, leading to a build-up of contaminants and the formation of a protonated phase (HMO2). Here, their formation mechanism is elucidated for the room-temperature storage of a Ni-rich NCM (LiNi0.94Co0.03Mn0.03O2) and LNO (LiNiO2) under humidified air (50% relative humidity at 25 °C), with and without CO2 (0, 500 and 1500 ppm). X-ray photoelectron spectroscopy reveals that without CO2, surface reactions are self-limiting, whereas with CO2, a continuous contaminant build-up alongside a reduction in nickel oxidation state is observed. Quantification of the HMO2 phase and surface contaminants via thermogravimetric analysis coupled with mass spectrometry (TGA-MS) and acid–base titration reveals distinct pH-driven mechanisms, highlighting the criticality of CO2. Electrochemical charge/discharge cycling of stored LNO|graphite full cells with a Li-RE at 25 °C reveals that a humid and CO2-free atmosphere does not negatively affect cycle life, while the presence of CO2 results in loss of cyclable CAM and inferior cycling performance. These results reveal the detrimental impact of CO2 in combination with H2O as the driving force of ambient-air degradation in Ni-rich CAMs.