29 February 2012 in Progress in Natural Science: Materials International
The effect of cooling rate on plastic deformation of Zr-based bulk metallic glasses has been studied. The specimens with the diameters of 3mm, 4mm and 6mm cut from the same ladder-shaped Zr55Al10Ni5Cu30 BMG rod were used in the present investigation. The experimental results indicated that the different plastic strains were induced for the three type compression specimens. The compressive plastic strain increased with the decreasing diameter for the as-cast specimens, which means that the compressive plastic strain increased with the increasing cooling rate. The reason of the difference is attributed to the free volume existed in the BMGs during the rapid solidification, and the larger free volume was contained in the specimen fabricated with the higher cooling rate. It has been found that the prominent serrations and multiple shear bands appeared during the compressive deformation tests of the specimen with smaller diameter of 3mm, indicating that the specimen with smaller diameter exhibits better plasticity due to more free volume content
7 October 2022 in Materials & Design
1 July 2017 in China Foundry
To recycle the returned alloy effectively, effects of returns proportion on alloy composition, microstructure and compression properties of superalloy GH4169 were studied by means of scanning electron microscopy (SEM), energy dispersive spectroscopy (EDS) and thermal-mechanical simulator. The results show that returns addition has no significant effect on the main alloy elements content and the principle precipitates, but increases the volume fraction of Al2O3 inclusions, resulting in the increase of oxygen level of GH4169 alloy. Returns addition does not change the elastic and plastic deformation process at room temperature or at 1,150 °C, but high returns proportion GH4169 alloy shows improved compression strength and yield strength. The alloy with 100% returns shows a maximum compression strength 1,153.45 MPa at room temperature, while the alloy with 80% returns has a maximum value 69.3 MPa at 1,150 °C. Returns addition increases fluctuation range and reduces the stability of yield strength and compression strength of GH4169 alloy at room temperature. It is noted that the volume fraction and the size of Al2O3, and the fraction of Laves phase reach their maximum values in the GH4169 alloy with 60% returns, which exhibits maximum yield strength of 516.65 MPa at room temperature and 62.17 MPa at 1,150 °C.