AMEEC team, Laboratory of Renewable Energies and Advanced Materials LERMA, College of Engineering and Architecture, International University of Rabat, Morocco
Auto-generated profile, based on publicly available information
Ismail Khay
AMEEC team, Laboratory of Renewable Energies and Advanced Materials LERMA, College of Engineering and Architecture, International University of Rabat, Morocco
Agitated vessels (or mechanically stirred reactors) are heat exchange devices that are most widely used in many chemical and biochemical process industries, such as anaerobic digestion process. The mixing and heat transfer performances in these vessels are of crucial importance for increasing the energy efficiency in both batch and continuous processes. In this paper, a series of experiments were conducted to investigate heat transfer performance in agitated vessels for various configurations. In fact, this study examines the effects of heat transfer geometry (wall jacket and helical coils), heating power, and stirring speed, on the heating performance of two stirred fluids—water alone and a mixture of water and food waste. The experiments were conducted using a jacketed insulation tank with a helical coil and a propeller agitator. In each experiment, a transient method, based on measuring the temperature dependency on time, and solving the unsteady enthalpy balance, was used to determine the overall heat transfer coefficients between the agitated fluid and the heating surface. Finally, an extensive analysis of the reduced data was conducted based on temperature, heating time, heat transfer rate, heat transfer coefficient, and thermal resistance. The main finding was that the presence of food waste in agitated vessels reduces the heat rate of the agitated fluid with an average of 18.13% and 49.51%, respectively, for the case of JHX and CHX, and creates additional fouling, which further limits the heat transfer.
This article examines the degradation mechanisms and mechanical properties of unfilled and montmorillonite-filled bamboo fiber-composites, under long-term water aging (up to 120 days) at room temperature. The main findings show that the water absorption and hydrolysis processes simultaneously occur during aging. The presence of clay fillers (3 wt %) reduces the water absorption content of composites from 18.69% to 15.68% after 120 aging days. However, their moisture absorption rate increases after adding particles. Scanning electron microscope images confirm the development of structural damage induced by the extra-swelling of particles, enabling more water absorption after long-term aging. Interestingly, the unfilled composites lose about 18.7% and 17.94% of their initial tensile strength and modulus after 120 aging days, which is attributed to the swelling/plasticization mechanisms and the chemical degradation at the interface, respectively. However, the tensile strength and modulus of montmorillonite-filled composites drop by 35.78% and 32.47%, respectively. This poor resilience to aging is attributed to the development of microstructural damage. The results of this work provide a clear insight into the long-term mechanical properties of composite materials and shed light on their systematic aging mechanisms, with a view to their application in harsh environments.