Long-term thermal storage can decarbonize heat utilization by resolving mismatches between heat supply and demand. However, common heat storage materials cannot store energy for long periods. Here, we report an ultralong-term latent heat storage “glass” based on a ternary eutectic sugar alcohol mixture. The as-prepared material exhibits a solid–liquid phase change and glass transition at 423 and 289 K, respectively, with heat release via cold crystallization at 346 K. Remarkably, the glass transition temperature increases to 313 K after aging at ambient temperature for 12 hours due to structural relaxation. This phase change material (PCM) conserves the latent heat of fusion at 423 K for at least 180 days in the glass state at ambient temperature. These results establish a third-generation latent heat storage mode, retaining the charged state as a kinetically arrested amorphous solid and thereby fundamentally shifting the stability criterion from supercooled-liquid nucleation suppression to glass-transition and structural-relaxation kinetics.
Al–Cu–Si eutectic alloys store 350–420 J g-1 near 520 °C but must be encapsulated to survive melting in air. Dry-coated microencapsulated phase change materials (MEPCMs) are made by high-speed impact blending (HIB) of α-Al2O3 nanoparticles onto the alloy powder and completed by heat oxidation, which builds the shell but consumes Al from the core. However, how the temperature and duration of this step affect the stability of the shell has not been reported in detail for Al–Cu–Si MEPCMs. Here, we oxidize dry-coated Al–26.5Cu–5.4Si@α-Al2O3 MEPCMs in O2 at 950–1200 °C and cycle them 1000 times in air. Rietveld refinement detects α-Al2O3 as the only crystalline oxidation product, and its growth gives an O uptake of 5.7–24.0 wt%. Oxidation at 1000 °C for 6 h gives 7.6 wt% O and a dense α-Al2O3 layer of 0.55–0.59 µm beneath the coat, consistent with the 0.68 µm expected from the O uptake. Up to 7.6 wt% O the Cu-enriched core stores 391–399 J g-1 of metal, and without a nucleating additive its main freezing peak lies 13 K above that of the HIB MEPCMs. At 14.6 wt% O and above, a primary phase crystallizes before the eutectic and the latent heat falls. During cycling the HIB MEPCMs form 20.0 wt% γ-Al2O3 and keep 57% of their latent heat or 76% per gram of metal, against 86–104% or 95–104% for the pre-oxidized MEPCMs. MEPCMs oxidized at 1000 °C for 6 h keep 243 J g-1 after 1000 cycles with an unchanged main freezing peak.