20 July 2020 in Applied Physics Letters
Zincblende InGaN/GaN quantum wells offer a potential improvement to the efficiency of green light emission by removing the strong electric fields present in similar structures. However, a high density of stacking faults may have an impact on the recombination in these systems. In this work, scanning transmission electron microscopy and energy-dispersive x-ray measurements demonstrate that one-dimensional nanostructures form due to indium segregation adjacent to stacking faults. In photoluminescence experiments, these structures emit visible light, which is optically polarized up to 86% at 10 K and up to 75% at room temperature. The emission redshifts and broadens as the well width increases from 2 nm to 8 nm. Photoluminescence excitation measurements indicate that carriers are captured by these structures from the rest of the quantum wells and recombine to emit light polarized along the length of these nanostructures.
22 July 2024 in Journal of Applied Physics
Distributed Bragg reflectors (DBRs) based on alternating layers of porous and non-porous GaN have previously been fabricated at the wafer-scale in heteroepitaxial GaN layers grown on sapphire substrates. Porosification is achieved via the electrochemical etching of highly Si-doped layers, and the etchant accesses the n+-GaN layers through nanoscale channels arising at threading dislocations that are ubiquitous in the heteroepitaxial growth process. Here, we show that the same process applies to GaN multilayer structures grown on silicon substrates. The reflectance of the resulting DBRs depends on the voltage at which the porosification process is carried out. Etching at higher voltages yields higher porosities. However, while an increase in porosity is theoretically expected to lead to peak reflectance, in practice, the highest reflectance is achieved at a moderate etching voltage because etching at higher voltages leads to pore formation in the nominally non-porous layers, pore coarsening in the porous layers, and in the worst cases layer collapse. We also find that at the high threading dislocation densities present in these samples, not all dislocations participate in the etching process at low and moderate etching voltages. However, the number of dislocations involved in the process increases with etching voltage.
5 April 2024 in Microscopy and Microanalysis
In this article, porous GaN distributed Bragg reflectors (DBRs) were fabricated by epitaxy of undoped/doped multilayers followed by electrochemical etching. We present backscattered electron scanning electron microscopy (BSE-SEM) for sub-surface plan-view imaging, enabling efficient, non-destructive pore morphology characterization. In mesoporous GaN DBRs, BSE-SEM images the same branching pores and Voronoi-like domains as scanning transmission electron microscopy. In microporous GaN DBRs, micrographs were dominated by first porous layer features (45 nm to 108 nm sub-surface) with diffuse second layer (153 nm to 216 nm sub-surface) contributions. The optimum primary electron landing energy (LE) for image contrast and spatial resolution in a Zeiss GeminiSEM 300 was approximately 20 keV. BSE-SEM detects porosity ca. 295 nm sub-surface in an overgrown porous GaN DBR, yielding low contrast that is still first porous layer dominated. Imaging through a ca. 190 nm GaN cap improves contrast. We derived image contrast, spatial resolution, and information depth expectations from semi-empirical expressions. These theoretical studies echo our experiments as image contrast and spatial resolution can improve with higher LE, plateauing towards 30 keV. BSE-SEM is predicted to be dominated by the uppermost porous layer’s uppermost region, congruent with experimental analysis. Most pertinently, information depth increases with LE, as observed.
9 March 2023 in Journal of Applied Physics
Aberration-corrected scanning transmission electron microscopy techniques are used to study the bonding configuration between gallium cations and nitrogen anions at defects in metalorganic vapor-phase epitaxy-grown cubic zincblende GaN on vicinal (001) 3C-SiC/Si. By combining high-angle annular dark-field and annular bright-field imaging, the orientation and bond polarity of planar defects, such as stacking faults and wurtzite inclusions, were identified. It is found that the substrate miscut direction toward one of the 3C-SiC in-plane directions is correlated with the crystallographic [1–10] in-plane direction and that the {111} planes with a zone axis parallel to the miscut have a Ga-polar character, whereas the {111} planes in the zone perpendicular to the miscut direction have N-polarity. The polarity of {111}-type stacking faults is maintained in the former case by rotating the coordination of Ga atoms by 180° around the polar axes and in the latter case by a similar rotation of the coordination of the N atoms. The presence of small amounts of the hexagonal wurtzite phase on Ga-polar {111} planes and their total absence on N-polar {111} planes is tentatively explained by the preferential growth of wurtzite GaN in the [0001] Ga-polar direction under non-optimized growth conditions.
17 June 2025 in Journal of Applied Physics
The luminescence characteristics and the relation between the distribution of impurities and stacking faults (SFs) in Mg-doped zincblende gallium nitride (zb-GaN:Mg) have been investigated by cathodoluminescence (CL) and atom probe tomography (APT). Four peaks have been identified in the CL emission spectrum, and the possible related recombination mechanisms have been proposed. The main peak at 3.23 eV is associated with excitonic transitions, while the other three, having lower energies at about 3.15, 3.02, and 2.92 eV, respectively, are related to donor-to-acceptor (DAP) transitions involving different acceptor energy levels. These DAP peaks were significantly more intense on or close to SFs compared to the surrounding defect-free material, indicating an enrichment of point defects near SFs. This finding was supported by APT measurements, where Mg showed a tendency to segregate toward SFs in zb-GaN.