18 November 2019 in ChemSusChem
The addition of Si compounds to graphite anodes has become an attractive way of increasing the practical specific energies in Li‐ion cells. Previous studies involving Si/C anodes lacked direct insight into the processes occurring in full cells during low‐temperature operation. In this study, a powerful combination of operando neutron diffraction, electrochemical tests, and post‐mortem analysis is used for the investigation of Li‐ion cells. 18650‐type cylindrical cells in two different aging states are investigated by operando neutron diffraction. The experiments reveal deep insights and important trends in low‐temperature charging mechanisms involving intercalation, alloying, Li metal deposition, and relaxation processes as a function of charging C‐rates and temperatures. Additionally, the main aging mechanism caused by long‐term cycling and interesting synergistic effects of Si and graphite are elucidated.
22 November 2019 in Journal of the Electrochemical Society
In this paper, we present an aging study of commercial 18650-type C/LiNi0.33Mn0.33Co0.33O2 lithium-ion cells. The test procedure comprises varying charging currents, discharging currents and resting times between cycles. The cells show a nonlinear capacity fade after a few hundred equivalent full cycles, if cycled with a standard charging and discharging rate of almost 1C, and different resting times. By increasing the discharging current or decreasing the charging current, the lifetime improves and results in a linear capacity fade. The neutron diffraction experiment reveals a loss of lithium inventory as the dominant aging mechanism for both linearly- and nonlinearly-aged cells. Other aging mechanisms such as the structural degradation of anode or cathode active materials, or the deactivation of active materials, cannot be confirmed. With ongoing aging, we observe an increasing capacity loss in the edge area of the electrodes. Whereas the growth of the solid electrolyte interphase defines the early stage, linear aging, marginal lithium deposition is supposed to cause the later stage, nonlinear aging. Capacity recovery caused by lithium stripping and chemical intercalation is shown to be dependent on the cell’s state of health.
2 April 2019 in Journal of the Electrochemical Society
Silicon-graphite (SiG) electrodes are attractive candidates as anodes for Li-ion batteries due to their high theoretical specific capacity. However, repeated lithiation/delithiation during charge/discharge cycling causes significant morphological changes of the silicon particles. This results in the formation of highly porous silicon structures and severe side reactions at the silicon/electrolyte interface. To quantify these morphological changes, small-angle neutron scattering (SANS) was applied with selective contrast matching of Si nanoparticles (200 nm diameter) and the surrounding electrolyte decomposition products. Using electrolytes consisting of 1.5 M LiPF6 dissolved in either deuterated or protonated ethylene carbonate (EC) resulted in solid-electrolyte-interphase (SEI) compounds with scattering length densities either matching or mismatching that of the Si nanoparticles. SiG anodes with 35 wt% silicon nanoparticles were aged for 10 and 20 charge/discharge cycles against capacitively oversized LiFePO4 cathodes. Afterwards, the morphological changes and size distribution of the SEI compounds were evaluated by means of ex-situ SANS measurements of the SiG electrodes in their fully discharged state. Transmission electron microscopy (TEM) images of the pristine and cycled silicon nanoparticles complement the interpretation of the SANS analysis.
30 April 2015 in Nanoscale
In optoelectronic devices based on quantum dot arrays, thin nanolayers of gold are preferred as stable metal contacts and for connecting recombination centers. The optimal morphology requirements are uniform arrays with precisely controlled positions and sizes over a large area with long range ordering since this strongly affects device performance. To understand the development of gold layer nanomorphology, the detailed mechanism of structure formation are probed with time-resolved grazing incidence small-angle X-ray scattering (GISAXS) during gold sputter deposition. Gold is sputtered on a CdSe quantum dot array with a characteristic quantum dot spacing of ≈7 nm. In the initial stages of gold nanostructure growth, a preferential deposition of gold on top of quantum dots occurs. Thus, the quantum dots act as nucleation sites for gold growth. In later stages, the gold nanoparticles surrounding the quantum dots undergo a coarsening to form a complete layer comprised of gold-dot clusters. Next, growth proceeds dominantly via vertical growth of gold on these gold-dot clusters to form an gold capping layer. In this capping layer, a shift of the cluster boundaries due to ripening is found. Thus, a templating of gold on a CdSe quantum dot array is feasible at low gold coverage.
9 January 2024 in Journal of Power Sources
17 February 2023 in Journal of the American Chemical Society