Solar thermochemical hydrogen (STCH) production is a promising method to generate carbon neutral fuels by splitting water utilizing metal oxide materials and concentrated solar energy. The discovery of materials with enhanced water-splitting performance is critical for STCH to play a major role in the emerging renewable energy portfolio. While perovskite materials have been the focus of many recent efforts, materials screening can be time consuming due to the myriad chemical compositions possible. This can be greatly accelerated through computationally screening materials parameters including oxygen vacancy formation energy, phase stability, and electron effective mass. In this work, the perovskite Gd0.5La0.5Co0.5Fe0.5O3 (GLCF), was computationally determined to be a potential water splitter, and its activity was experimentally demonstrated. During water splitting tests with a thermal reduction temperature of 1,350°C, hydrogen yields of 101 μmol/g and 141 μmol/g were obtained at re-oxidation temperatures of 850 and 1,000°C, respectively, with increasing production observed during subsequent cycles. This is a significant improvement from similar compounds studied before (La0.6Sr0.4Co0.2Fe0.8O3 and LaFe0.75Co0.25O3) that suffer from performance degradation with subsequent cycles. Confirmed with high temperature x-ray diffraction (HT-XRD) patterns under inert and oxidizing atmosphere, the GLCF mainly maintained its phase while some decomposition to Gd2-xLaxO3 was observed.
CuCr 2 O 4 spinel is a candidate coating material for central receivers in concentrating solar power to protect structural alloys against high temperature oxidation and related degradation. Coating performance and microstructure of dip-coated and sintered coatings is dictated by the initial particle size of the CuCr 2 O 4 and sintering temperature, but can be compromised by particle agglomeration. In this study, sub-micron particles were synthesised through the Pechini and modified Pechini sol–gel methods. Phase composition was confirmed via X-ray diffraction. Particle growth during calcination of the nanoparticles at different temperatures (650°C, 750°C, 850°C) and times (between 1 and 24 h) was measured via laser diffraction and scanning electron microscopy. The modified Pechini method displayed evidence of smaller particle sizes and greater agglomeration. The kinetics of particle growth observed are consistent with a diffusion limited inhibited grain growth model.
Colorado School of Mines (Mines) led this program in collaboration with Sandia National Laboratories (Sandia) to characterize narrow-channel fluidized beds of aluminosilicate particles – supplied by Carbo Ceramics – as a means for releasing high-temperature thermal energy in particle heat exchangers and for capturing concentrated solar energy in indirect particle receivers. Single-channel, heat transfer experiments at Mines and reduced-order 1-D models and 3-D two-fluid, CFD models explored many aspects of counterflow, bubbling fluidized beds (net downward particle flow and upward gas flow) for enhancing particle-wall heat transfer at elevated temperatures. Results at Mines on single-channel test sections consistently showed that mild bubbling fluidization increases particle-wall heat transfer coefficients (hT,w) regularly by more than 4.0 over hT,w values without fluidization at similar conditions (mean particle diameter dp, bed depth zb, and bed particle temperatures Tp). Insights from lab-scale tests and modeling studies provided Nusselt number correlations for hT,w and informed the design and fabrication (by Vacuum Process Engineering) of a nominal 40-kWth, particle-sCO2 plate heat exchanger (HX) with 12 parallel narrow-channel, fluidized beds bounded by stainless-steel walls with embedded microchannels for high-pressure sCO2 flows. Tests of the 40-kWth HX at the particle-sCO2 HX test stand at Sandia's National Solar Thermal Test Facility (NSTTF) were limited, due to HX design, to particle inlet temperatures Tp,in£ 520°C with maximum sCO2 outlet temperatures TsCO2,out » 440°C, which are well below design conditions for a primary HX in a sCO2 power cycle for a Gen-3 concentrating solar power (CSP) plant. Total heat transfer Q ̇_HX remains relatively constant with increased fluidization for fixed particle and sCO2 inlet conditions because higher hT,w due to fluidization is offset by increased axial dispersion, which suppresses temperature differences between the particles and sCO2 in the counterflow configuration. The axial dispersion reduces the effective overall heat transfer coefficient U based on Tp,in to values around 200 W m-2 K-1.