13 July 2020 in IEEE Journal of Solid-State Circuits
We developed a 300-GHz-band 120-Gb/s wireless transceiver front-ends (TRX) using our in-house InP-based high-electron-mobility-transistor (InP-HEMT) technology for beyond-5G. The TRX is composed of the RF power amplifiers (PAs), mixers, and local oscillation (LO) PAs which are all packaged in individual waveguide (WG) modules by using a ridge coupler for low-loss WG-to-IC transition. RF PAs are designed using the low-impedance inter-stage-matching technique to reduce the inter-stage matching loss of the amplifier stages, and the back-side DC line (BDCL) technique is used to simplify the layout and to improve the gain of the PAs. The fabricated RF PAs show a high output 1-dB compression point of more than 6 dBm from 278 to 302 GHz. The mixers are used for both up- and down-conversion in the transmitter and receiver. These mixers are designed to have high conversion gain (CG) over the wideband even after packaging by enhancing the isolation between the RF and IF ports. The measured CG of mixer module is -15 dB, and the 3-dB IF-bandwidth is 32 GHz. The LO PAs are also designed using the BDCL technique so that they can supply the required LO power to the mixers. The TRX with these InP building blocks enables the data transmission of a 120 Gb/s 16QAM signal over a link distance of 9.8 m.
19 September 2018 in IEEE Electron Device Letters
We present our latest results on L g = 87 nm InAlAs/InGaAs high-electron-mobility transistors with an excellent combination of dc and high-frequency characteristics. We obtained a maximum transconductance of 3 S/mm at V DS = 0.9 V, an ON-resistance of 273 Ω-μm, a current gain cutoff frequency of 559 GHz, and a maximum oscillation frequency of 671 GHz. According to small-signal modeling, these outstanding device metrics are a consequence of the indium-rich InGaAs channel with very high Hall mobility, compact device design with L SD = 1 μm, and an optimized gate process that yields well-tempered behavior.
10 April 2009 in Applied Physics Express
2 May 2023 in IEEE Transactions on Electron Devices
Herein, we present a detailed analysis of the effects of O2 plasma treatment on the AlGaN barrier volume trap states in an Al0.45Ga0.45N/GaN high-electron mobility transistor. Compared to that of the as-grown sample, the single short-pulse ${I}_{D}$ – ${V}_{\text {GS}}$ characterization of the plasma-treated sample exhibited lower charge trapping inside the AlGaN barrier. The 1/ ${f}$ low-frequency noise characterization revealed a significant reduction of approximately 67% in the volume trap density of the AlGaN barrier layer after O2 plasma treatment. This was achieved by the formation of Al–O and Ga–O bonds via the penetration of oxygen ions into the AlGaN bulk, which resulted in reduced trap state density in the AlGaN barrier. In addition, the Schottky characteristics were improved notably. Consequently, the O2 plasma-treated sample did not display current collapse and showed steady drain current output under the reverse-sweep drain-stress bias conditions. Furthermore, the plasma treatment significantly reduced the RF transconductance ( ${g}_{m}$ ) collapse in the as-grown sample, and significantly increased the ${f}_{T}/{f}_{\text {max}}$ of the plasma-treated sample from 65/70 to 120/230 GHz for ${L}_{g}$ = 80 nm devices, respectively. Last, the O2 plasma-treated sample showed substantial improvements in ${P}_{\text {out}\_\max}$ , power added efficiency (PAE), and linear gain from 1.25 W/mm, 20%, and 15 dB to 2.4 W/mm, 50%, and 19 dB, respectively.
10 January 2023 in IEEE Transactions on Electron Devices
We present a systematic study on the gate length ( ${L}_{{g}}\text {)}$ scaling behavior and the impact of the side-recess spacing ( ${L}_{\text {side}}\text {)}$ on dc and high-frequency characteristics of In0.8Ga0.2As quantum-well (QW) high-electron-mobility transistors (HEMTs) with ${L}_{{g}}$ from 10 $\mu $ m to 20 nm, for the purpose of understanding the scaling limit of maximum oscillation frequency ( ${f}_{\text {max}}\text {)}$ and thereby demonstrating terahertz devices. The fabricated In0.8Ga0.2As QW HEMTs with ${L}_{{g}} =20$ nm and ${L}_{\text {side}} =150$ nm exhibited values of drain-induced-barrier-lowering (DIBL) of 60 mV/V, current-gain cutoff frequency ( ${f}_{{T}}\text {)}$ of 0.75 THz, and ${f}_{\text {max}}$ of 1.1 THz, while the device with ${L}_{\text {side}} =50$ nm showed DIBL of 110 mV/V and ${f}_{{T}}$ / ${f}_{\text {max}}$ of 0.72/0.53 THz. It was central to strictly control short-channel effects (SCEs) from the perspective of DIBL to maximize the improvement of ${f}_{\text {max}}$ , as ${L}_{{g}}$ was scaled down deeply. In an effort to understand the ${L}_{{g}}$ scaling behavior of ${f}_{\text {max}}$ , we carried out the small-signal modeling for both types of devices and found that the increase of the intrinsic output conductance ( ${g}_{\text {oi}}\text {)}$ played a critical role in determining ${f}_{\text {max}}$ in short- ${L}_{{g}}$ HEMTs. On the contrary, the fabricated devices with ${L}_{\text {side}} =150$ nm exhibited a tight control of SCEs at ${L}_{{g}}$ of 20 nm. As a result, ${f}_{\text {max}}$ in those devices was boosted to 1.1 THz, and more importantly this high ${f}_{\text {max}}$ was maintained even as ${L}_{{g}}$ was scaled down to 20 nm. The results in this work represent the best balance of ${f}_{{T}}$ and ${f}_{\text {max}}$ in any transistor technology on any material system, displaying both ${f}_{{T}}$ and ${f}_{\text {max}}$ in excess of 700 GHz simultaneously.