TiO2-based thin layers are used to improve or change the surface properties of various materials. The work deals with the effect of TiO2 layers on the surface properties of selected substrates. The layers were prepared by the sol-gel method using the dip-coating technique on glass and stainless steel. The sol was prepared in "titanium isopropoxide-isopropyl alcohol-acetyl acetone-water-catalyst" system, whereas as catalyst was used nitric acid or acetic acid. The morphology and topography of the surfaces of the uncoated and coated substrates were evaluated by atomic force microscopy. Scanning electron microscopy was used to determine the layer thickness. The effect of TiO2 layers on the surface properties of materials was also evaluated using wetting angles, surface energy and its polar and dispersion components. Based on the results, especially the higher surface energy value, we can conclude that the TiO2 layer influenced the surface properties of the studied solid materials.
7 December 2025 in Polymer Degradation and Stability
The work deals with the influence of water corrosion on the surface properties of inorganic-organic SiO2 films, which were prepared from the sols in “tetraethoxysilane-isopropyl alcohol-water-nitric acid-triethoxy(octyl)silane” system. The atomic force microscopy and sessile drop technique was used on the characterization of surface properties. The morphology, rms-roughness, adhesion force and stiffness of prepared films were evaluated. Surface free energy and its polar and dispersion component were calculated by Owens-Wendt method using contact angles of distilled water and diiodomethane. The influence of corrosion on all of the studied properties of films was significant in the case of films prepared from sol with molar ratio of x(H2O) : x(SiO2) = 2.
Kaolinite was treated with silane and copper acetate using microwave (MW) heating at different time intervals. The prepared kaolinites were utilized as fillers (10 phr) in SMR composites. FT-IR, thermal analysis, and SEM demonstrate alterations in the spectral and structural properties after merely 30 min. of chemical/MW treatment. The application of silanized fillers resulted in a decreased vulcanization rate and facilitated the processing and curing of the composites. The favorable mechanical properties affirm the reinforcement provided by MW-modified kaolinite.