28 February 2022 in Archives of Metallurgy and Materials
This study focused on the reclamation of ash from incineration process and development of new artificial lightweight aggregate (LWA) that have comparable properties with existing natural coarse aggregate. The main objective of this study is to examine potential use of recycled municipal solid waste incineration (MSWI) ash as raw material in LWA production with a method of cold-bonded pelletization. Two types of incineration ash which is bottom ash (BA) and fly ash (FA) were collected from Cameron Highland Incineration Plant, Malaysia. The properties of BA and FA are studied by means of X-Ray Fluorescence (XRF) and microstructure of these ashes were inspected using Scanning Electron Microscope (SEM). The properties of BALA and FALA produced in this study is examined including loose bulk density, water absorption and aggregate impact value (AIV). From the results of both types of artificial LWA, the lowest loose bulk density of BALA is BALA50 with 564.14 kg/m3 and highest is at 831.19 kg/m3. For FALA50, lowest loose bulk density is 573.64 kg/m3 and highest is 703.35 kg/m3. Water absorption of BALA and FALA is quite similar with one another in with the value of 23.8% and 22.6%, respectively. Generally, FALA have better qualities of LWA comparing with BALA with lower bulk density and water absorption and can be categorized as strong aggregate. In summary, reclamation and reutilization of incinerator ash has generated acceptable qualities for artificial LWA. Both types of BA and FA shown a great potential to be recycled as additional materials in artificial aggregate production.
1 July 2023 in IOP Conference Series: Earth and Environmental Science
SMSyakirah Afizah Mohamed
+2
The substitution or addition of new supplementary cementitious materials (SCM) in the production of variety of construction materials has gained much interest. One of the examples of SCM is incineration ash which consist of fly ash (FA) and bottom ash (BA) which are the residues from the ignition of biomass and can brings applicable ecological advantages. However, the properties of this new materials need to be investigated to ensure its full potential can be developed. Therefore, this study is initiated to identify the characteristics of incineration ash from local source in Malaysia. To identify the elemental components of ashes, most widely method was adopted which is using X-Ray Fluorescence (XRF). The quantity of unburned carbon in fly ash is measured by loss on ignition, which has a major influence on the product’s characteristics. In addition, specific gravity and density were also determined and comparison has been made with cement. In this study it was found out that XRF results shows that both FA and BA consist of the same mineral composition with OPC majorly in silica, aluminium, calcium, and iron which makes is suitable to be used in the concrete. For LOI, the value for BA is much higher compared with FA due to the amount of unburnt carbon in its original compositions and the incomplete burning due to insufficient contact time in the furnace. Based on the result obtained for LOI, the average LOI value for FA and BA is 17.33 % and 44.67 %, respectively. As expected, for the specific gravity and density, FA having the lowest specific gravity and density. The density obtained for FA is 755 kg/m3 and for BA is 593 kg/m3. Overall, the use of incineration ash can be fully investigated by exploring other parameter that influence the performance of construction materials.
1 July 2023 in IOP Conference Series: Earth and Environmental Science
Study was related to the influence of the concrete properties by using different percentages of metakaolin and fixed percent of incineration bottom ash to partially replace the cement. Cement is a well-known building material and used for the construction in the world. Moreover, the used of metakaolin (MK) and incineration bottom ash (IBA) in this research would give significance to our environment as it can reduce the usage of cement in concrete. By using bottom ash, it could reduce the land filling space. The X-Ray Fluorescence (XRF) test was used to determine the chemical composition of IBA and MK. Four series of concrete have been examined, including control, IBA and MK were used as partial replacement for cement at 10%IBA + 10%MK, 10%IBA + 15%MK and 10%IBA + 20%MK of concrete mixes by volume. The curing period for the samples is 7 days and 28 days. To determine the properties of concrete, the tests such as slump test, density test, water absorption test, pulse velocity test, rebound hammer test and compression test were performed. The results proved that the strength development of 10%IBA + 10%MK concrete sample shows the highest compressive strength after 28 days of curing.