A new approach is being considered for obtaining microfibrillated cellulose with a low degree of polymerization by sulfuric acid hydrolysis with simultaneous ultrasonic treatment under mild conditions (temperature 25 °C, 80% power control). Samples of initial cellulose, MCC, and MFC were characterized by FTIR, XRF, SEM, DLS, and TGA. It was found that a high yield of MFC (86.4 wt.%) and a low SP (94) are observed during hydrolysis with ultrasonic treatment for 90 min. It was shown that the resulting microfibrillated cellulose retains the structure of cellulose I and has an IC of 0.74. It was found that MFC particles are a network of fibrils with an average size of 91.2 nm. ζ-potential of an aqueous suspension of MFC equal to −23.3 mV indicates its high stability. It is noted that MFC has high thermal stability, the maximum decomposition temperature is 333.9 °C. Simultaneous hydrolysis process with ultrasonic treatment to isolate MFC from cellulose obtained by oxidative delignification of spruce wood allows to reduce the number of stages, reduce energy costs, and expand the scope.
В России ежегодно черепно-мозговые травмы (ЧМТ) получают около 600 тыс. человек, из них 50 тыс. погибают, а еще 50 тыс. остаются инвалидами. Смертность от ЧМТ превышает таковую от болезней сердечно-сосудистой системы. В данной публикации подробно описаны принципы хирургического лечения ЧМТ. Описаны показания к хирургическому лечению эпидуральных и субдуральных гематом, очаговых ушибов, множественных гематом, внутрижелудочковых кровоизлияний, вдавленных переломов, краниофациальных повреждений. Описаны факторы риска неблагоприятного исхода у пострадавших с тяжелой ЧМТ. Применение новых технологий в диагностике и лечении пациентов с ЧМТ, а также внедрение новых видов хирургических вмешательств в отделениях неотложной нейрохирургии позволит значительно улучшить результаты...
The effect of temperature of aspen bark pre-carbonization on evolution of a porous structure and sorption properties of the carbon sorbents prepared in results of thermo alkaline activation of carbonizats with hydroxide potassium was studied. The relationship of a sorption of methylene blue and vitamin B12 by the sorbents from aspen bark to a volume and size of pores was established. It was shown, that the carbon sorbents capacity at а methylene blue are defined by pores with width 0.86–2.95 nm, and at a vitamin B12 – 3.18–6.89 nm. Comparation of the porous structures parameters and sorption properties of the carbon sorbents from aspen bark and commercial activated carbon for medical purposes was maked. Kinetic of markers sorption onto sorbents with different porous structure was studied and the corresponding rate constants were calculated. The possibility preparation of a carbon sorbent have high rate of vitamin B12 sorption (rate constant is 3.953 min–1) was shown. The determinations of a sorption capacity of sorbents in conditions assume at enterosorbents test were carry out. It was determined, that sorbents, prepped from aspen bark, exceeds the sample of industrial activated carbon for medical purposes at sorption capacity of methylene blue and vitamin B12 in 1.7 and 1.5 time, correspondingly.
18 September 2024 in Chemistry of plant raw material
It was suggested for the first time to use tannins isolated from the bark of the Siberian cedar (Pinus sibirica) for synthesis of organic xerogels. The influence of the nature of the cross-linking agent on the characteristics of xerogels prepared by sol-gel by condensation of cedar tannins with formaldehyde, furfuryl alcohol or glutaraldehyde was studied. IR study shows an increase in the number of methylene -CH2- and methylene ether -CH2-O-CH2 bonds during the formation of xerogels. The use of furfuryl alcohol leads to an increase in the density of the tannin-furfuryl gel (T/FA) xerogel (0.348 g/cm3) compared to the low density of tannin-formaldehyde (T/F) and tannin-glutar (T/G) xerogels – 0.063 and 0.071 g/cm3. BET study indicates the microporous nature of T/FA xerogel, where the proportion of micropores with an average pore size of 1.42 nm reaches 70.75%. Xerogels prepared using formaldehyde and glutaral have a meso/macroporous structure with a mesopore width of about 25–75 nm and small contribution of micropores – 8.61 and 11.27%, respectively. The SEM method revealed the formation of a branched structure of interconnected spherical particles about 3 µm in size in tannin-formaldehyde and agglomerated particles (3-8 µm) in tannin-glutar xerogels. Tannin-furfuryl gel is similar in structure and morphology to cellular foam with cavities about 10 mm in size. Using the DTA method, it was established that initial temperature of thermal composition of the T/F gel is 216 °C, T/G gel is 272 °C and T/FA is 282 °C. It was found that tannin-formaldehyde xerogel has better efficiency compared to another gels in removing methylene blue from water solution (107 mg/g).
For the first time, tannin-lignin-formaldehyde and tannin-lignin-furfuryl organic gels were obtained on the basis of larch bark tannins and hydrolysis lignin by sol-gel condensation with formaldehyde and furfuryl alcohol. Their physico-chemical properties were studied by varying the content of lignin (from 5 to 30 wt%) and a fixed mass ratio of polyphenolic substances to the crosslinking reagent (1 : 1.5). With an increase in the lignin content the density of tannin-lignin formaldehyde gels decreases from 0.83 to 0.53 g/ cm3, and that of tannin-lignin-furfuryl gels is from 0.32 to 0.14 g / cm3. According to the FTIR data, the structures of tannin-lignin-formaldehyde and tannin-lignin-furfuryl gels are formed by aromatic fragments cross-linked with methylene and methylene-ether bridges. Scanning electron microscopy shows that the addition of appropriate amounts of lignin to tannins (up to 10 wt% when using formaldehyde and up to 20 wt% when using furfuryl alcohol) promotes the formation of gels with a more developed porous structure. In the case of tannin-lignin-formaldehyde gel, the specific surface area and sorption of methylene blue are 12 m2 / g and 43 mg / g and for tannin-lignin-furfuryl gel – 72 m2 / g and 114.5 mg/g, respectively. It was found that an increase in the lignin content in the gel composition over 20 wt.% is accompanied by the phase localization of lignin (precipitation), which reduces the strength of the resulting gel and reduces its specific surface area.
11 December 2024 in Chemistry of plant raw material
One-pot production of xylitol from xylan seems to be more environmentally friendly and economically attractive due to the absence of intermediate stages of purification and preparation of raw materials. For this process, bifunctional catalysts containing nanodispersed ruthenium particles (0.5–3%) on the Sibunit-4 carbon support varied by different acidity (oxidized by moist-air at 400–500 °C) were synthesized and characterized. Xylan hydrolysis and xylose hydrogenation in the presence of Ru-containing carbon catalysts were considered individually. The effect of the Sibunit-4 support acidity and ruthenium content (0.5–3%) on the yield of hemicellulose hydrolysis and monosaccharide hydrogenation products, respectively, was studied. It was found that the most active catalyst in the process of xylan hydrolysis and xylose hydrogenation is the one with the support oxidized at 450 °C, providing the maximum acidity, and bearing 2 wt.% of Ru (2RuSib450). In the one-pot process of xylan hydrolysis-hydrogenation to monomers in the presence of the 2RuSib450 catalyst, the xylan hydrolysis reaction proceeds more slowly than the xylose hydrogenation reaction, with a large amounts of propylene glycol and ethylene glycol formed, indicating the low selectivity of the catalyst with respect to xylitol, the yield of which does not exceed 6 wt.%. In the one-pot process of hydrolysis-transfer hydrogenation with combination of H2SO4 and 2RuSib450 in an isopropanol-water medium, xylitol was obtained from xylan with a high yield (88 wt.%). The low amounts of H2SO4 allows the processes to be carried out in the standard stainless steel equipment instead of alloys with a high Ni content.