The mechanical and tribological properties of polyetheretherketone (PEEK)- and PEEK + PTFE (polytetrafluoroethylene)-based composites loaded with and four types of nanoparticles (carbonaceous, metallic, bimetal oxide, and ceramic) under metal- and ceramic-polymer tribological contact conditions were investigated. It was found that loading with the nanofillers in a small content (0.3 wt.%) enabled improvement of the elastic modulus of the PEEK-based composites by 10–15%. In the metal–polymer tribological contact, wear resistance of all nanocomposites was increased by 1.5–2.3 times. In the ceramic-polymer tribological contact, loading PEEK with metal nanoparticles caused the intensification of oxidation processes, the microabrasive counterpart wear, and a multiple increase in the wear rate of the composites. The three component “PEEK/10PTFE/0.3 nanofillers” composites provided an increase in wear resistance, up to 22 times, for the metal–polymer tribological contact and up to 12 times for the ceramic-polymer one (with a slight decrease in the mechanical properties) compared to that of neat PEEK. In all cases, this was achieved by the polymer transfer film formation and adherence on the counterparts. The various effects of the four types of nanoparticles on wear resistance were determined by their ability to fix the PTFE-containing transfer film on the counterpart surfaces.
Non-destructive monitoring methods and continuous monitoring systems based on them are crucial elements of modern systems for the management and maintenance of assets which include reinforced concrete structures. The purpose of our study was to summarise the data on the most common sensors and systems for the non-destructive monitoring of reinforced concrete structures developed over the past 20 years. We considered systems based on electrochemical (potentiometry, methods related to polarisation) and physical (electromagnetic and ultrasonic waves, piezoelectric effect, thermography) examination methods. Special focus is devoted to the existing sensors and the results obtained using these sensors, as well as the advantages and disadvantages of their setups or other equipment used. The review considers earlier approaches and available commercial products, as well as relatively new sensors which are currently being tested.
The main goal of this paper is to design and justify optimized compositions of thermoplastic–matrix wear-resistant composites based on polyetheretherketone (PEEK) and polyphenylene sulfide (PPS). Their mechanical and tribological properties have been specified in the form of bilateral and unilateral limits. For this purpose, a material design methodology has been developed. It has enabled to determine the optimal degrees of filling of the PEEK- and PPS-based composites with carbon microfibers and polytetrafluoroethylene particles. According to the results of tribological tests, the PEEK-based composites have been less damaged on the metal counterpart than the PPS-based samples having the same degree of filling. Most likely, this was due to more uniform permolecular structure and greater elasticity of the matrix. The described methodology is versatile and can be used to design various composites. Its implementation does not impose any limits on the specified properties of the material matrix or the reinforcing inclusions. The initial data on the operational characteristics can be obtained experimentally or numerically. The methodology enables to design the high-strength wear-resistant composites which are able to efficiently operate both in metal–polymer and ceramic–polymer friction units.
The marine environment is highly corrosive for mild and low alloy steels. This study aimed to enhance the corrosion resistance of the AH36 steel in a saline medium by coating it with a copper particles reinforced polyaniline (PANI) layer. PANI and Cu particles were grown on the steel surface by electrodepositing methods. Firstly, PANI was electropolymerized in the presence of oxalic acid, followed by the electrodeposition of Cu particles at different deposition times. The coating showed a well-distribution of Cu particles in the polymer matrix and excellent adhesion. Furthermore, the Cu particles and PANI-coated steels exhibited corrosion resistance significantly in the saline medium compared to the bare substrate and pristine PANI-coated samples. The improved corrosion protection of a Cu@PANI coating on the AH36 steel could contribute to forming a physical barrier by filling Cu particles on the PANI pores.
For comparative evaluation of the influence of carbon nanofiber/nanotube loading in two different thermoplastic matrices (UHMWPE and PEEK), some mechanical and tribotechnical properties of the nanocomposites have been studied. It is shown that mechanical properties of nanocomposites change in various manners with increasing loading of carbon nanofibers and nanotubes. Herewith, the wear resistance of the “UHMWPE+1 wt% CNF and PEEK + 1 wt% CNF” composites under dry sliding friction is doubled. It is shown that, regardless of various effects on permolecular structure formation, the studied nanofillers enhance the wear resistance of the composites in a similar manner. A comparative analysis of the influence of nanofillers on the modification of mechanical and tribotechnical properties of UHMWPE- and PEEK-based matrices is made.
The present study aimed to evaluate the antifouling efficacy of Piper betle leaf extracts as a bioactive additive for eco-friendly antifouling coatings. The composition of P. betle extract was determined and analyzed. Phytochemical analysis revealed that the ethanol extract of P. betle contained phenolics, tannins, proteins, carbohydrates, and flavonoids, with total phenolic content reaching 260.3 mg GAE/g dry weight and flavonoid content reaching 52.56 mg QE/g dry weight. The antibacterial test results showed that the ethanol extract of P. betle exhibited maximum antibacterial efficacy against E. coli, B. subtilis, S. aureus, and marine bacteria, with inhibition zone diameters of 28.7 ± 0.5, 27.0 ± 1.6, 22.1 ± 0.6, and 35.1 ± 0.5 mm, respectively. Based on the laboratory test results, the ethanol extract of P. betle was chosen to be added to coatings as an antifouling additive. The content of the extract was 0.5, 1.0, and 1.5 wt.%. A field test conducted in tropical seawater (at Nha Trang Bay) demonstrated that incorporating 1 wt.% of P. betle extract into an acrylic copolymer-based coating significantly enhanced its antifouling performance. After nine months of immersion in seawater, this sample maintained an antifouling efficiency of 74%. These findings highlight the potential of P. betle extract as a sustainable alternative to conventional antifouling agents in marine coatings.