We have studied scintillation properties of Eu3+-doped Gd3Al2Ga3O12 single crystals. Gd3Al2Ga3O12 single crystals with different concentrations of Eu3+ (0.5%, 1.0%, 5.0%, 10.0%, and 15.0%) were grown using the floating-zone method. In photoluminescence (PL) and scintillation properties, the Eu-doped Gd3Al2Ga3O12 single crystals showed emission peaks and several millisecond decay times due to 4f–4f transitions of Eu3+ ions. Pulse height spectra of all the samples were investigated under γ-ray irradiation from 137Cs (662 keV). The 0.5%, 1.0%, 5.0%, and 10.0% Eu-doped samples showed full energy peaks. Among all the samples, the 5.0% Eu-doped Gd3Al2Ga3O12 single crystal showed the highest light yield of 36 000 photons MeV−1.
In this study, Lu2.5Y0.5(Al2.5Ga2.5)O12 (LuYAGG) single-crystal scintillators doped with terbium ions (Tb3+) at concentrations of 0.5, 1, 5, and 10 mol% were successfully synthesized using the floating zone method. The structural, optical, photoluminescence (PL), and scintillation properties of the Tb3+-doped crystals were systematically investigated with a focus on their potential for high-performance scintillator applications. X-ray diffraction (XRD) confirmed the formation of a pure garnet phase without any secondary phases, indicating the successful incorporation of Tb3+ into the LuYAGG lattice. Optical transmittance spectra revealed high transparency in the visible range. Photoluminescence measurements showed characteristic Tb3+ emission peaks, with the strongest green emission observed from the 5D4 → 7F5 transition, particularly for the 5 mol% sample. The PL decay curves further confirmed that this concentration offers a favorable balance between radiative efficiency and minimal non-radiative losses. Under γ-ray excitation, the 5 mol% Tb3+-doped crystal exhibited the highest light yield, surpassing the performance of other concentrations and even outperforming Bi4Ge3O12 (BGO) in relative comparison, with an estimated yield of approximately 60,000 photons/MeV. Scintillation decay time analysis revealed that the 5 mol% sample also possessed the fastest decay component, indicating its superior capability for radiation detection. Although 10 mol% Tb3+ still showed good performance, slight quenching effects were observed, while lower concentrations (0.5 and 1 mol%) suffered from longer decay and lower emission efficiency due to limited activator density. These findings clearly identify with 5 mol% Tb3+ as the optimal dopant level in LuYAGG single crystals, offering a synergistic combination of high light yield and excellent optical transparency. This work highlights the strong potential of LuYAGG:Tb3+ as a promising candidate for the next-generation scintillator materials used in medical imaging, security scanning, and high-energy physics applications.
28 November 2023 in Nuclear Instruments and Methods in Physics Research Section B: Beam Interactions with Materials and Atoms
The 0.1% Ag-doped ZnO translucent ceramic was synthesized by spark plasma sintering and annealed at 700 °C and 800 °C in the air for 24 h. Photoluminescence (PL) quantum yields ( QY s) and scintillation light yields ( LY s) of the annealed ceramics were increased as compared with the as-prepared ceramic because the annealing reduced self-absorption due to oxygen vacancies. The ceramic annealed at 700 °C indicated the highest LY (7000 ph/5.5 MeV- α ) among the present samples owing to the increase of the PL QY and energy-transfer efficiency from the host to the luminescence centers. In the ceramic annealed at 800 °C, scintillation LY s decreased due to the increment of the number of trap sites.