Heterogeneous nucleation and grain initiation are two different processes in early-stage solidification (ESS), although both are deterministic. Heterogeneous nucleation refers to the formation of a 2-dimensional (2D) nucleus (a crystal plane of the solid) that can template further growth, while grain initiation is the formation of a hemispherical cap (3D) from which isothermal growth is possible. It is both theoretically and practically beneficial to separate heterogeneous nucleation from grain initiation. This paper provides an overview of our recent understanding of grain initiation behaviour under different conditions and its consequences on grain refinement. After a brief review of the processes involved in the ESS, we present the grain initiation behaviour on a single substrate. This is followed by grain initiation behaviour in systems with a population of nucleant particles with varying particle types (corresponding to varying nucleation undercoolings), where we give detailed descriptions of progressive grain initiation, explosive grain initiation, hybrid grain initiation, grain initiation maps and grain refinement maps. We then provide a brief introduction to the rules that govern competition for heterogeneous nucleation and grain initiation among multiple types of nucleant particles with varying particles’ nucleation undercoolings and sizes. Finally, we present the practical implications of grain refinement maps to grain refinement. A key finding from this work is that more significant grain refinement can be achieved by promoting explosive grain initiation using impotent nucleant particles, which is opposite to the traditional approach for grain refinement where potent particles are used to enhance heterogeneous nucleation.
The main problem of recycling aluminium scrap is the gradual accumulation of impurities, especially iron, which tend to form undesired intermetallic compounds that affect the integrity and the mechanical performance of the castings. In this paper, we aim to provide an overview on the topic of iron removal from aluminium melts through primary intermetallic precipitation and the progress made during the LiME Hub project to understand the process and to develop a more efficient procedure. We cover both thermodynamic analysis and experimental validation. We found that high shear melt conditioning technology enhances the typically slow nucleation and growth of the dense primary intermetallics, speeding up their sedimentation and allowing a faster removal of Fe from the melt by simple gravity sedimentation. It also promotes the formation of smaller and more compact Fe-rich intermetallics, allowing an increased volume fraction recovery and mitigating their effect of being present in the final castings. The technology is not limited to batch processing, with a 90% efficiency, but can also be applied to continuous melt treatment of aluminium scrap, with currently 60% efficiency, and could be combined with other solid–liquid separation techniques to increase the purification efficiency even more.
Without the addition of any grain refiner, the inclusion particles in a melt will induce heterogeneous nucleation and grain initiation during the solidification of metallic materials. However, with grain refiner addition, the exogenous particles (from the grain refiner) and the native inclusions (e.g., oxide particles) will co-exist in the melt, and there will be competition for nucleation and grain initiation among different types of solid particles. In this paper, we analyze such competition in Al and Mg alloys using a numerical solidification model that we have developed previously. The numerical calculations show that the competition for nucleation is strongly dependent on nucleation undercooling of the different types of particles, while the competition for grain initiation is closely related to the sizes of solid particles. Based on the numerical results, the general rules of competition for nucleation and grain initiation have been developed: nucleation starts with particles of minimum nucleation undercooling, followed by particles with progressively larger nucleation undercooling; and grain initiation starts with solid particles of the largest size, followed by solid particles with progressively smaller sizes.
Grain refinement is of importance for metallic materials since it provides multiple benefits, such as improved castability, reduced casting defects and improved mechanical properties. From extensive research carried out in the past decades, it has been widely accepted that solute is one of the crucial factors for achieving grain refinement. However, grain refinement is a complex phenomenon, depending on not only solutes in the melt to provide growth restriction but also the physical and chemical nature of the nucleant particles (either endogenous or exogenous). Although significant progress has been made on the subject, some critical questions still remain open, and a comprehensive understanding of the mechanisms of solute effect on grain refinement is still desirable. In this paper, we present an overview of the solute effect on grain refinement based on our recent advances made in the LiME Research Hub. This covers the effect of solute on nucleation potency of nucleant particles due to interfacial segregation, columnar to equiaxed transition (CET), growth restriction and eventually on the overall grain refinement.
7 August 2019 in Metallography, Microstructure, and Analysis
By utilizing data from the literature, we examine the effects of superheat and solute additions on the grain size (as measured by columnar grain length) in binary copper alloys. Our investigation provides support for an Arrhenius-like behavior of the superheat on the grain size. We also find a correlation between the columnar grain length at a constant degree of superheat and the variation of the reciprocal of the true growth restriction factor (1/Q) with P, Mg, Mn, Pb, and Sn solute additions to be a power of law of 1/3, which gave a better fit than a linear one.
6 November 2020 in Metallography, Microstructure, and Analysis
The effect of dilute solute additions on growth restriction in binary Cu alloys has been assessed at different degrees of superheat. Columnar grain length values from Northcott’s work (Northcott in J Inst Metals 62:101-136, 1938) for binary Cu alloys were plotted against the corresponding undercooling parameter (P), the reciprocal of the conventional (Qconv.) and true (Qtrue) growth restriction factor (Schmid-Fetzer and Kozlov in Acta Mater 59(15):6133-6144, 2011) values. It was found that there was no correlation between the columnar grain length values and P, 1/Qconv. and 1/Qtrue values for different solutes and cast at the same degree of superheat. Unlike P, Qconv., and Qtrue values, the heuristic growth restriction parameter (β) (Fan et al. in Acta Mater 152, 248-257, 2018) modeling framework in conjunction with the critical solute content (C*) for growth restriction fitted well to binary Cu alloys.