The international technology roadmap of semiconductors (ITRS) is approaching the historical end point and we observe that the semiconductor industry is driving complementary metal oxide semiconductor (CMOS) further towards unknown zones. Today’s transistors with 3D structure and integrated advanced strain engineering differ radically from the original planar 2D ones due to the scaling down of the gate and source/drain regions according to Moore’s law. This article presents a review of new architectures, simulation methods, and process technology for nano-scale transistors on the approach to the end of ITRS technology. The discussions cover innovative methods, challenges and difficulties in device processing, as well as new metrology techniques that may appear in the near future.
GeSn materials have attracted considerable attention for their tunable band structures and high carrier mobilities, which serve well for future photonic and electronic applications. This research presents a novel method to incorporate Sn content as high as 18% into GeSn layers grown at 285–320 °C by using SnCl4 and GeH4 precursors. A series of characterizations were performed to study the material quality, strain, surface roughness, and optical properties of GeSn layers. The Sn content could be calculated using lattice mismatch parameters provided by X-ray analysis. The strain in GeSn layers was modulated from fully strained to partially strained by etching Ge buffer into Ge/GeSn heterostructures . In this study, two categories of samples were prepared when the Ge buffer was either laterally etched onto Si wafers, or vertically etched Ge/GeSnOI wafers which bonded to the oxide. In the latter case, the Ge buffer was initially etched step-by-step for the strain relaxation study. Meanwhile, the Ge/GeSn heterostructure in the first group of samples was patterned into the form of micro-disks. The Ge buffer was selectively etched by using a CF4/O2 gas mixture using a plasma etch tool. Fully or partially relaxed GeSn micro-disks showed photoluminescence (PL) at room temperature. PL results showed that red-shift was clearly observed from the GeSn micro-disk structure, indicating that the compressive strain in the as-grown GeSn material was partially released. Our results pave the path for the growth of high quality GeSn layers with high Sn content, in addition to methods for modulating the strain for lasing and detection of short-wavelength infrared at room temperature.
In this article, we demonstrated novel methods to improve the performance of p-i-n photodetectors (PDs) on a germanium-on-insulator (GOI). For GOI photodetectors with a mesa diameter of 10 μm, the dark current at −1 V is 2.5 nA, which is 2.6-fold lower than that of the Ge PD processed on Si substrates. This improvement in dark current is due to the careful removal of the defected Ge layer, which is formed with the initial growth of Ge on Si. The bulk leakage current density and surface leakage density of the GOI detector at −1 V are as low as 1.79 mA/cm2 and 0.34 μA/cm, respectively. GOI photodetectors with responsivity of 0.5 and 0.9 A/W at 1550 and 1310 nm wavelength are demonstrated. The optical performance of the GOI photodetector could be remarkably improved by integrating a tetraethylorthosilicate (TEOS) layer on the oxide side due to the better optical confinement and resonant cavity effect. These PDs with high performances and full compatibility with Si CMOS processes are attractive for applications in both telecommunications and monolithic optoelectronics integration on the same chip.
Stacked SiGe/Si structures are widely used as the units for gate-all-around nanowire transistors (GAA NWTs) which are a promising candidate beyond fin field effective transistors (FinFETs) technologies in near future. These structures deal with a several challenges brought by the shrinking of device dimensions. The preparation of inner spacers is one of the most critical processes for GAA nano-scale transistors. This study focuses on two key processes: inner spacer film conformal deposition and accurate etching. The results show that low pressure chemical vapor deposition (LPCVD) silicon nitride has a good film filling effect; a precise and controllable silicon nitride inner spacer structure is prepared by using an inductively coupled plasma (ICP) tool and a new gas mixtures of CH2F2/CH4/O2/Ar. Silicon nitride inner spacer etch has a high etch selectivity ratio, exceeding 100:1 to Si and more than 30:1 to SiO2. High anisotropy with an excellent vertical/lateral etch ratio exceeding 80:1 is successfully demonstrated. It also provides a solution to the key process challenges of nano-transistors beyond 5 nm node.
This work presents the growth of high-quality Ge epilayers on Si (001) substrates using a reduced pressure chemical vapor deposition (RPCVD) chamber. Based on the initial nucleation, a low temperature high temperature (LT-HT) two-step approach, we systematically investigate the nucleation time and surface topography, influence of a LT-Ge buffer layer thickness, a HT-Ge growth temperature, layer thickness, and high temperature thermal treatment on the morphological and crystalline quality of the Ge epilayers. It is also a unique study in the initial growth of Ge epitaxy; the start point of the experiments includes Stranski–Krastanov mode in which the Ge wet layer is initially formed and later the growth is developed to form nuclides. Afterwards, a two-dimensional Ge layer is formed from the coalescing of the nuclides. The evolution of the strain from the beginning stage of the growth up to the full Ge layer has been investigated. Material characterization results show that Ge epilayer with 400 nm LT-Ge buffer layer features at least the root mean square (RMS) value and it’s threading dislocation density (TDD) decreases by a factor of 2. In view of the 400 nm LT-Ge buffer layer, the 1000 nm Ge epilayer with HT-Ge growth temperature of 650 °C showed the best material quality, which is conducive to the merging of the crystals into a connected structure eventually forming a continuous and two-dimensional film. After increasing the thickness of Ge layer from 900 nm to 2000 nm, Ge surface roughness decreased first and then increased slowly (the RMS value for 1400 nm Ge layer was 0.81 nm). Finally, a high-temperature annealing process was carried out and high-quality Ge layer was obtained (TDD=2.78 × 107 cm−2). In addition, room temperature strong photoluminescence (PL) peak intensity and narrow full width at half maximum (11 meV) spectra further confirm the high crystalline quality of the Ge layer manufactured by this optimized process. This work highlights the inducing, increasing, and relaxing of the strain in the Ge buffer and the signature of the defect formation.
Semiconductor nanowires have great application prospects in field effect transistors and sensors. In this study, the process and challenges of manufacturing vertical SiGe/Si nanowire array by using the conventional lithography and novel dry atomic layer etching technology. The final results demonstrate that vertical nanowires with a diameter less than 20 nm can be obtained. The diameter of nanowires is adjustable with an accuracy error less than 0.3 nm. This technology provides a new way for advanced 3D transistors and sensors.