Two kinds of Al2O3 ceramic samples with and without Al film deposited were designed respectively. The influences of temperature and high kinetic energy sputtering particles on the wettability and interface strength of Al/Al2O3 were studied by comparing the wetting behavior of molten aluminum on two samples. The results show that molten aluminum does not wet the Al2O3 sample without Al film deposited at 700 °C, the contact angle is 165°, and the interfacial shear strength is 28 MPa. With the increase of temperature, the contact angle decreases continuously, and the interface shear strength gradually increases. The fracture of the brazed joint is transferred from the interface to the brazing seam. In comparison, the sample deposited with Al film is wetted by molten aluminum at 700 °C, and the contact angle is only 12°. The interface shear strength is about 120 MPa and is less affected by temperature. The shear fracture of the joint occurs in the brazed seam of Al metal. Therefore, the high energy generated by either the temperature increase or the particle sputtering enable the Al atoms to overcome the energy barrier to form Al–O bonds with the O atoms on the Al2O3 ceramic surface, thereby improving the wettability of Al/Al2O3.
31 May 2024 in Journal of Materials Research and Technology
In this work, we evaluated the influence of phosphoric acid in conjunction with a tannic converter formula on the adhesion of the coating system by employing the epoxy coating as the top coating. The morphology and the composition of the rusted steel before and after treatment were determined by scanning electron microscopy (SEM) and Fourier transform infrared (FTIR) spectroscopy. The adhesion test result showed that the adhesion strength between the rust and the epoxy coating was enhanced from 1.93 MPa to 11.63 MPa with the treatment by 50 g/L phosphoric acid in conjunction with a tannic converter formula. Further investigation of the working mechanism of such treatment revealed that the adhesion improvement could be attributed to the formation of a micro-cracked and compact conversion layer. This layer could reinforce the anchoring of epoxy coating through the pinning effect. It was also found that both the pH and the phosphate radical were the important factors to improve the adhesion strength.
Closed-cell metal syntactic foam is a new material consisting of hollow spheres embedded in metal matrix syntactic foams. These foams have good physical and mechanical properties and are increasingly used worldwide in industrial and high-tech fields. Magnesium matrix syntactic foams containing hollow Al2O3 spheres ((Al2O3hs)/AZ91D) were successfully fabricated by hot press sintering at different temperatures. The fabrication of Al2O3hs/AZ91D and the effect of sintering temperature on the microstructure and properties are reported in this paper. Additionally, sandwiched magnesium matrix syntactic foams were prepared by placing magnesium plates on both sides of the syntactic foam. Some Al2O3hs particles became filled with matrix particles during preparation. Thus, the actual density was greater than the theoretically calculated value and increases with increasing sintering temperature. Above 723 K, a brittle phase MgAl2O4 formed in Al2O3hs/AZ91D. The quasistatic and dynamic compressive strengths of Al2O3hs/AZ91D first increased and then decreased with increasing sintering temperature, and the maximums were 162 MPa and 167.87 MPa, respectively. Thus, this paper reports a new strategy for the controlled preparation of metal matrix syntactic foams with predetermined porosity. The results show that this strategy improved the performance of lightweight and high-strength syntactic foam materials and shows potential for further research.
The corrosion behavior of pure Fe, Cr, and Mo was studied at 125°C and 3.5 MPa solid NH4Cl + oxygen-free water vapor environment. The corrosion kinetic rates of these three metals are obtained by a weight-loss method as pure Fe > Cr > Mo. Through scanning electron microscopy, energy dispersive spectrometer, x-ray diffraction, and electron probe microanalyzer, the corrosion products, surface morphology, cross-sectional morphology, and element distribution of metals in the environment were understood. The results show that Cl− is enriched on the surface of the substrate, and participates in the corrosion reaction by the ionic cycle, which promotes the corrosion and dissolution of the metal substrate. In an oxygen-free environment, the corrosion products of metals are mainly chlorides, and a small amount of oxides are produced by hydrolysis. The corrosion rate of metal is related to the density of its surface product layer. A corrosive medium can diffuse to the surface of the substrate through the loose product layer. The denser the product layer, the more it can protect the substrate.