Hailong Shang

Dr. Hailong Shang


Research Focus & Metrics

Academic Career Length

7Years (2020-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
19 February 2020 in Entropy
Verified
Journal Article
Open access
PDF file
CJChunxia Jiang
Chunxia Jiang
RLRongbin Li
Rongbin Li
XWXin Wang
Xin Wang
HSHailong Shang
Hailong Shang
Yong ZhangYong Zhang
Yong Zhang
Peter LiawPeter Liaw
Peter Liaw
In this study, high-entropy alloy films, namely, AlCrTaTiZr/AlCrTaTiZr-N, were deposited on the n-type (100) silicon substrate. Then, a copper film was deposited on the high-entropy alloy films. The diffusion barrier performance of AlCrTaTiZr/AlCrTaTiZr-N for Cu/Si connect system was investigated after thermal annealing for an hour at 600 °C, 700 °C, 800 °C, and 900 °C. There were no Cu-Si intermetallic compounds generated in the Cu/AlCrTaTiZr/AlCrTaTiZr-N/Si film stacks after annealing even at 900 °C through transmission electron microscopy (TEM) and atomic probe tomography (APT) analysis. The results indicated that AlCrTaTiZr/AlCrTaTiZr-N alloy films can prevent copper diffusion at 900 °C. The reason was investigated in this work. The amorphous structure of the AlCrTaTiZr layer has lower driving force to form intermetallic compounds; the lattice mismatch between the AlCrTaTiZr and AlCrTaTiZ-rN layers increased the diffusion distance of the Cu atoms and the difficulty of the Cu atom diffusion to the Si substrate.

21 February 2020 in Materials
Verified
Journal Article
Open access
PDF file
XQXiaoben Qi
Xiaoben Qi
HSHailong Shang
Hailong Shang
Bingyang MaBingyang Ma
Bingyang Ma
RZRulin Zhang
Rulin Zhang
LGLeyang Guo
Leyang Guo
BSBo Su
Bo Su
The interaction effect of micro arc oxidation (MAO) parameters on the microstructure and wear properties was investigated. The results showed that the electric current and oxidation time significantly influenced the thickness and grinding crack width of the ceramic coatings within the range of the selected parameters, and the interaction effect of the electrical parameters was not obvious. The surface morphology, cross-section morphology, and element distribution of the coatings were observed using scanning electron microscopy (SEM) with energy dispersive spectroscopy (EDS) and X-ray diffraction (XRD). The results showed that ceramic coatings with γ-Al2O3 and α-Al2O3 formed, which enhanced the coating performance. After that, the microhardness and wear resistance were tested. Under the optimal process, the microhardness of a coating section was up to 1200 HV0.1, and the friction coefficient was just 0.3. When wear occurred, the volcanic microstructures experienced extrusion and deformation, and then peeled off under shear stress, which led to the formation of a grinding crack. The main failure modes of the micro arc oxidation coatings were abrasive wear and spalling failure.

22 April 2021 in Materials
Verified
Journal Article
Open access
PDF file
YLYang Li
Yang Li
HSHailong Shang
Hailong Shang
Bingyang MaBingyang Ma
Bingyang Ma
XGXuqiang Guo
Xuqiang Guo
RLRongbin Li
Rongbin Li
GLGeyang Li
Geyang Li
Two kinds of Al2O3 ceramic samples with and without Al film deposited were designed respectively. The influences of temperature and high kinetic energy sputtering particles on the wettability and interface strength of Al/Al2O3 were studied by comparing the wetting behavior of molten aluminum on two samples. The results show that molten aluminum does not wet the Al2O3 sample without Al film deposited at 700 °C, the contact angle is 165°, and the interfacial shear strength is 28 MPa. With the increase of temperature, the contact angle decreases continuously, and the interface shear strength gradually increases. The fracture of the brazed joint is transferred from the interface to the brazing seam. In comparison, the sample deposited with Al film is wetted by molten aluminum at 700 °C, and the contact angle is only 12°. The interface shear strength is about 120 MPa and is less affected by temperature. The shear fracture of the joint occurs in the brazed seam of Al metal. Therefore, the high energy generated by either the temperature increase or the particle sputtering enable the Al atoms to overcome the energy barrier to form Al–O bonds with the O atoms on the Al2O3 ceramic surface, thereby improving the wettability of Al/Al2O3.

6 November 2023 in Coatings
Verified
Journal Article
Open access
PDF file
Bingyang MaBingyang Ma
Bingyang Ma
HYHaitian Yuan
Haitian Yuan
ZHZongqian He
Zongqian He
HSHailong Shang
Hailong Shang
YHYanjie Hou
Yanjie Hou
Filipe FernandesFilipe Fernandes
Filipe Fernandes
In this paper, TiN-Ni nanostructured composite films with different Ni contents are prepared using the magnetron sputtering method. The composition, microstructure, and mechanical properties of composite films are analyzed using an X-ray energy spectrometer (EDS), a scanning electron microscope (SEM), X-ray diffraction technology (XRD), a transmission electron microscope (TEM), and nanoindentation. All the films grow in a columnar crystal structure. There are only TiN diffraction peaks in the XRD spectrum, and no diffraction peaks of Ni and its compounds are observed. The addition of the Ni element disrupts the integrity of TiN lattice growth, resulting in a decrease in the grain size from 60 nm in TiN to 25 nm at 20.6% Ni. The film with a Ni content of 12.4 at.% forms a nanocomposite structure in which the nanocrystalline TiN phase (nc-TiN) is surrounded by the amorphous Ni (a-Ni) phase. The formation of nc-TiN/a-Ni nanocomposite structures relies on the good wettability of Ni on TiN ceramics. The hardness and elastic modulus of the film gradually decrease with the increase in Ni content, but the toughness is improved. The hardness and elastic modulus decrease from 19.9 GPa and 239.5 GPa for TiN film to 15.4 GPa and 223 GPa at 20.6 at.% Ni film, respectively, while the fracture toughness increases from 1.5 MPa·m1/2 to 2.0 MPa·m1/2. The soft and ductile Ni phase enriched at the TiN grain boundaries hinders the propagation of cracks in the TiN phase, resulting in a significant increase in the film’s toughness. The research results of this paper provide support for the design of TiN-Ni films with high strength and toughness and the understanding of the formation mechanism of nanocomposite structures.

5 April 2022 in Materials
Verified
Journal Article
Open access
PDF file
ZRZhun Ran
Zhun Ran
HSHailong Shang
Hailong Shang
Bingyang MaBingyang Ma
Bingyang Ma
RLRongbin Li
Rongbin Li
FSFujun Shangguan
Fujun Shangguan
DYDayi Yu
Dayi Yu
This paper presents a magnetron sputtering Al/Cu bilayer film solder to realize the brazing of AlN ceramic and Al metal. The effect of different temperatures on the structure and mechanical properties of brazed joints is studied. The results show that the sputtered Al particles have a sputtering wetting effect on AlN ceramic. The contact angle of molten Al on AlN ceramic with Al film deposited at 700 °C is as low as about 30°. While the contact angle of molten Al on AlN ceramic without Al film deposited at 1000 °C is about 89°. There is a large amount of Cu enrichment in brazed joints at 600 °C. The weld structure is a mixture of Al solid solution and AlCu compound. The shear strength of the brazed joint is only 70.6 MPa, and the joint fracture shows a large number of brittle fracture morphologies. With the increase of brazing temperature, the phenomenon of Cu enrichment in the joint gradually weakens, and the weld structure gradually transforms into a solid solution of Cu in Al. The shear strength of the brazed joint continues to increase, and the joint fracture morphology gradually changes from brittle fracture to furrow-like plastic fracture morphology. When the brazing temperature is increased to 660 °C, the distribution of Cu in the joint is evenly dispersed, and the shear strength of the brazed joint reaches the highest value of 107.8 MPa. The joint fracture is completely furrow-like plastic fracture morphological composition.

1 March 2021 in Journal of Alloys and Compounds
Verified
Journal Article
Closed access
Bingyang MaBingyang Ma
Bingyang Ma
XQXiaoben Qi
Xiaoben Qi
RLRongbin Li
Rongbin Li
RZRulin Zhang
Rulin Zhang
HSHailong Shang
Hailong Shang