Explosive crystallization is a well known phenomenon occurring due to the thermodynamic instability of strongly under-cooled liquids, which is particularly relevant in pulsed laser annealing processes of amorphous semiconductor materials due to the globally exothermic amorphous-to-liquid-to-crystal transition pathway. In spite of the assessed understanding of this phenomenon, quantitative predictions of the material kinetics promoted by explosive crystallization are hardly achieved due to the lack of a consistent model able to simulate the concurrent kinetics of the amorphous-liquid and liquid-crystal interfaces. Here, we propose a multi-well phase-field model specifically suited for the simulation of explosive crystallization induced by pulsed laser irradiation in the nanosecond time scale. The numerical implementation of the model is robust despite the discontinuous jumps of the interface speed induced by the phenomenon. The predictive potential of the simulations is demonstrated by means of comparisons of the modelling predictions with experimental data in terms of in situ reflectivity measurements and ex-situ micro-structural and chemical characterization.
Doping of Si nanocrystals (NCs) has been the subject of a strong experimental and theoretical debate for more than a decade. A major difficulty in the understanding of dopant incorporation at the nanoscale is related to the fact that theoretical calculations usually refer to thermodynamic equilibrium conditions, whereas, from the experimental point of view, impurity incorporation is commonly performed during NC formation. This latter circumstance makes impossible to experimentally decouple equilibrium properties from kinetic effects. In this report, we approach the problem by introducing the dopants into the Si NCs, from a spatially separated dopant source. We induce a P diffusion flux to interact with the already-formed and stable Si NCs embedded in SiO2, maintaining the system very close to the thermodynamic equilibrium. Combining advanced material synthesis, multi-technique experimental quantification and simulations of diffusion profiles with a rate-equation model, we demonstrate that a high P concentration (above the P solid solubility in bulk Si) within Si NCs embedded in a SiO2 matrix corresponds to an equilibrium property of the system. Trapping within the Si NCs embedded in a SiO2 matrix is essentially diffusion limited with no additional energy barrier, whereas de-trapping is prevented by a binding energy of 0.9 eV, in excellent agreement with recent theoretical findings that highlighted the impact of different surface terminations (H- or O-terminated NCs) on the stability of the incorporated P atoms.
Heavy doping of Ge is crucial for several advanced micro- and optoelectronic applications, but, at the same time, it still remains extremely challenging. Ge heavily n-type doped at a concentration of 1 × 1020 cm−3 by As ion implantation and melting laser thermal annealing (LTA) is shown here to be highly metastable. Upon post-LTA conventional thermal annealing As electrically deactivates already at 350 °C reaching an active concentration of ∼4 × 1019 cm−3. No significant As diffusion is detected up to 450 °C, where the As activation decreases further to ∼3 × 1019 cm−3. The reason for the observed detrimental deactivation was investigated by Atom Probe Tomography and in situ High Resolution X-Ray Diffraction measurements. In general, the thermal stability of heavily doped Ge layers needs to be carefully evaluated because, as shown here, deactivation might occur at very low temperatures, close to those required for low resistivity Ohmic contacting of n-type Ge.
Following recent successful demonstrations of enhanced infrared absorption in Au-hyperdoped Si, there has been strong interest in fabricating other metal-hyperdoped Si systems as a highly attractive approach for Si-based infrared photodetection. In this work, we address the somewhat contentious issue in the literature as to whether it is possible, using ion implantation and nanosecond pulsed-laser melting, to achieve hyperdoping of Si with Ag and Ti at concentrations exceeding that required to form an intermediate impurity band within the Si bandgap ( ). A wide range of characterization techniques were used to investigate these material systems, especially the quality of liquid-phase epitaxy, impurity concentration distribution both in depth and laterally, and impurity lattice location. Our results indicate that the high concentrations of opto-electrically active Ag or Ti in monocrystalline Si required to form an impurity band are not achieved. In particular, the usual behavior during rapid solidification is for near-complete surface segregation of the impurity, or for it to be trapped within a highly defective subsurface layer due to filamentary breakdown. Although our measurements showed that the maximum concentration of impurities outside metal-rich filaments is comparable to for both Ag and Ti, there is no preferential Ag or Ti lattice location after pulsed-laser melting anywhere in the material. Thus, the concentration of opto-electrically active Ag and Ti that can be homogeneously incorporated into Si is expected to be well below , leaving Au as the only viable impurity to date for achieving the required level of hyperdoping in Si.