Markus Börner

Dr. Markus Börner

orcid

Research Focus & Metrics

Academic Career Length

8Years (2019-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
26 October 2021 in Batteries
Verified
Journal Article
Open access
PDF file
TBThomas Beuse
Thomas Beuse
MFMathias Fingerle
Mathias Fingerle
CWChristian Wagner
Christian Wagner
MWMartin Winter
Martin Winter
MBMarkus Börner
Markus Börner
Porosity is frequently specified as only a value to describe the microstructure of a battery electrode. However, porosity is a key parameter for the battery electrode performance and mechanical properties such as adhesion and structural electrode integrity during charge/discharge cycling. This study illustrates the importance of using more than one method to describe the electrode microstructure of LiNi0.6Mn0.2Co0.2O2 (NMC622)-based positive electrodes. A correlative approach, from simple thickness measurements to tomography and segmentation, allowed deciphering the true porous electrode structure and to comprehend the advantages and inaccuracies of each of the analytical techniques. Herein, positive electrodes were calendered from a porosity of 44–18% to cover a wide range of electrode microstructures in state-of-the-art lithium-ion batteries. Especially highly densified electrodes cannot simply be described by a close packing of active and inactive material components, since a considerable amount of active material particles crack due to the intense calendering process. Therefore, a digital 3D model was created based on tomography data and simulation of the inactive material, which allowed the investigation of the complete pore network. For lithium-ion batteries, the results of the mercury intrusion experiments in combination with gas physisorption/pycnometry experiments provide comprehensive insight into the microstructure of positive electrodes.

14 August 2023 in Journal of Materials Chemistry A
Verified
Journal Article
Open access
PDF file
TITjark T. K. Ingber
Tjark T. K. Ingber
MBMarlena M. Bela
Marlena M. Bela
FPFrederik Püttmann
Frederik Püttmann
JDJan F. Dohmann
Jan F. Dohmann
PBPeter Bieker
Peter Bieker
MSMarian Cristian Stan
Marian Cristian Stan
In zero-excess lithium metal batteries (ZELMBs), also termed “anode-free” LMBs, Li from the positive electrode is electrodeposited onto a bare current collector instead of the Li metal negative electrode commonly used in LMBs. This enables high theoretical energy density and facile, safe, and low-cost assembly. To tackle coulombic inefficiencies during Li deposition/dissolution, 3D structured current collectors can be used instead of 2D foil materials. This study elucidates the Li deposition behavior in custom-made open-porous Cu micro-foams from nucleation to large scale deposition. For the first time in ZELMBs, surface and sub-surface Li deposits in open-porous 3D materials are compared to deposits on 2D foils using cryogenic focused ion beam scanning electron microscopy (cryo-FIB-SEM). The results highlight that Cu micro-foams can store substantial amounts of dendrite-free Li in their open-porous 3D structure, minimizing detrimental volume changes during Li deposition/dissolution. Electrochemical analyses and simulations reveal that current density distribution over the large surface area of the Cu micro-foams reduces the Li nucleation overvoltage by ≈40%. Also, charge/discharge cycling in ZELMBs shows increases in coulombic efficiency, capacity retention, and cycle life. Overall, this work explains how open-porous Cu micro-foam current collectors improve the Li deposition behavior to boost the cycling characteristics of ZELMBs.


9 April 2021 in Advanced Energy and Sustainability Research
Verified
Journal Article
Open access
PDF file
IDIris Dienwiebel
Iris Dienwiebel
MDMarcel Diehl
Marcel Diehl
BHBastian Heidrich
Bastian Heidrich
XYXiaofei Yang
Xiaofei Yang
MWMartin Winter
Martin Winter
MBMarkus Börner
Markus Börner
Aqueous processing of positive electrode active materials (AMs) could enable a more economical and environmentally friendly production of lithium‐ion batteries. Intrinsically, aqueous processing of positive AMs is hampered by lithium‐proton exchange in the AM surface, leading to a poor electrochemical performance and a resulting strong increase in the pH value in the electrode paste, thereby corroding the aluminum current collector. Herein, the influence of different lithium salts as processing additive to tailor the pH value of the electrode paste, the manganese dissolution during processing, and the electrochemical performance is described for aqueous processing of LiNi0.5Mn1.5O4‐based positive electrodes. Positive electrodes, based on an aqueous LiNi0.5Mn1.5O4‐based electrode paste which is mixed with LiN(SO2CF3)2 (LiTFSI), achieve a comparable electrochemical performance to state‐of‐the‐art nonaqueous‐processed electrodes. Manganese dissolution into the electrode paste is examined by inductively coupled plasma‐mass spectrometry (ICP‐MS), showing that the addition of lithium salts to the electrode paste substantially decreases manganese leaching during processing. Furthermore, postmortem analysis shows that the addition of LiTFSI to the electrode paste has a positive effect not only during processing but also on charge/discharge cycling performance.

20 October 2022 in Journal of Power Sources
Verified
Journal Article
Closed access
KAKarina Ambrock
Karina Ambrock
MRMirco Ruttert
Mirco Ruttert
AVAndrey Vinograd
Andrey Vinograd
BBBastian Billmann
Bastian Billmann
XYXiaofei Yang
Xiaofei Yang
MBMarkus Börner
Markus Börner

9 September 2023 in World Electric Vehicle Journal
Verified
Journal Article
Open access
PDF file
SFSamuel Fink
Samuel Fink
DDDelil Demir
Delil Demir
MBMarkus Börner
Markus Börner
VGVinzenz Göken
Vinzenz Göken
CVChristian Vedder
Christian Vedder
In modern electrode manufacturing for lithium-ion batteries, the drying of the electrode pastes consumes a considerable amount of space and energy. To increase the efficiency of the drying process and reduce the footprint of the drying equipment, a laser-based drying process is investigated. Evaporation rates of up to 318 g m−2 s−1 can be measured, which is orders of magnitude higher than the evaporation rates in conventional furnace drying processes. Optical measurements of the slurry components in the visible and near-infrared spectrum are conducted. Thermal analyses the of laser-dried samples reveal that the commonly used binders carboxymethyl-cellulose (CMC) and styrene–butadiene rubber (SBR) are not affected by the laser drying process within the investigated process window. The results indicated that with the combination of a fast laser drying step and a subsequent convection drying step, high evaporation rates can be achieved while maintaining the integrity and adhesion of the anode.