Wood is a versatile material that is used for various purposes due to its good properties, such as its aesthetic properties, acoustic properties, mechanical properties, thermal properties, etc. Its poor dimensional stability and low natural durability are the main obstacles that limit its use in mechanical applications. Therefore, modification is needed to improve these properties. The hydrothermal modification of wood exposes wood samples to elevated temperatures and pressure levels by using steam, water, or a buffer solution as the treating medium, or by using superheated steam. Abundant studies regarding hydrothermally treated wood were carried out, but the negative effect on the wood’s strength is one of the limitations. This is a method that boosts the dimensional stability and improves the decay resistance of wood with minimal decrements of the strength properties. As an ecofriendly and cost-effective method, the hydrothermal modification of wood is also a promising alternative to conventional chemical techniques for treating wood. Researchers are attracted to the hydrothermal modification process because of its unique qualities in treating wood. There are many scientific articles on the hydrothermal modification of wood, and many aspects of hydrothermal modification are summarized in review papers in this field. This paper reviews the hydrothermally modified mechanical properties of wood and their potential applications. Furthermore, this article reviews the effects of hydrothermal modification on the various properties of wood, such as the dimensional stability, chemical properties, and durability against termites and fungi. The merits and demerits of hydrothermal wood modification, the effectiveness of using different media in hydrothermal modification, and its comparison with other treating techniques are discussed.
Polymer blends is a well-established and suitable method to produced new polymeric materials as compared to synthesis of a new polymer. The combination of two different types of polymers will produce a new and unique material, which has the attribute of both polymers. The aim of this work is to analyze mechanical and morphological properties of bio-phenolic/epoxy polymer blends to find the best formulation for future study. Bio-phenolic/epoxy polymer blends were fabricated using the hand lay-up method at different loading of bio-phenolic (5 wt%, 10 wt%, 15 wt%, 20 wt%, and 25 wt%) in the epoxy matrix whereas neat bio-phenolic and epoxy samples were also fabricated for comparison. Results indicated that mechanical properties were improved for bio-phenolic/epoxy polymer blends compared to neat epoxy and phenolic. In addition, there is no sign of phase separation in polymer blends. The highest tensile, flexural, and impact strength was shown by P-20(biophenolic-20 wt% and Epoxy-80 wt%) whereas P-25 (biophenolic-25 wt% and Epoxy-75 wt%) has the highest tensile and flexural modulus. Based on the finding, it is concluded that P-20 shows better overall mechanical properties among the polymer blends. Based on this finding, the bio-phenolic/epoxy blend with 20 wt% will be used for further study on flax-reinforced bio-phenolic/epoxy polymer blends.
Thermosetting epoxies are low-density polymers with excellent adhesion, mechanical properties, and resistance to environmental degradation. They are widely used as molds and castings for manufacturing, protective coatings, and reinforcement material for aircraft. However, polymer brittleness is a major disadvantage preventing its widespread application. The addition of filler materials such as nanoparticles has attracted considerable attention. Using reinforcement materials for biocomposite derived from a natural, renewable and sustainable material will lower the manufacturing cost for epoxy composites. This study investigated the physical and mechanical properties of epoxy composites reinforced with amorphous and crystalline silica. The amorphous and crystalline silica were obtained by the precipitation method from the carbonization of rice husk at 700 °C and 1000 °C for 6 h, separately. The epoxy resin was mixed with 5 wt%, 10 wt%, and 15 wt% concentrations (by weight) of amorphous and crystalline silica, separately. Silica 10 nm to 30 nm in size was obtained, as observed by scanning electron microscopy (SEM). The epoxy nano-crystalline silica composite had a significantly lower thickness swelling value compared to the epoxy nano-amorphous silica composite. However, the epoxy nano-crystalline silica composite had significantly better mechanical properties.
Bamboo belongs to the grass family and is an important non-timber forest product in tropic and sub-tropic countries. The global trade of bamboo products is worth billions of dollars and is mainly dominant with monopodial bamboo grown in sub-tropic countries such as China and Japan. Many researchers globally discuss that in addition to species and region, bamboo quality can differ based on its rhizome types because the physiology is different for both monopodial and sympodial bamboo. However, there is a massive competition within the yearly forest products due to the challenges posed by underground root system in agroforestry. This review studied the properties of bamboo with regards to their differences in terms of monopodial and sympodial types of rhizomes. It was found that most of the structural, chemical organic, and mechanical properties are higher in monopodial bamboo, but there is a greater fibre morphology and decay resistance in the sympodial bamboo.
18 February 2017 in Materials for Renewable and Sustainable Energy
Dye-sensitized solar cells (DSSCs) are fabricated using natural sensitizers extracted from rengas (Gluta spp.) and mengkulang (Heritieraelata) wood. The natural sensitizers are extracted using a cold extraction and the Soxhlet extraction methods. This paper presents the results of the analysis of the optical characteristics of the sensitizers via ultraviolet–visible spectrophotometry and Fourier transform infrared spectroscopy. The optical band gap and the highest occupied molecular orbital (HOMO)–lowest unoccupied molecular orbital (LUMO) levels of each investigated sensitizer are calculated on the basis of the analyzed data collected from photoluminescence and cyclic voltammetry. The DSSCs with the mengkulang sensitizer have better conversion efficiency (ŋ = 0.1695%) than the DSSCs with the rengas sensitizer (ŋ = 0.109%). The performance of the DSSCs indicates an increment as the ratios of the mixed mengkulang:rengas (60%:40%) and mengkulang:rengas (40%:60%) sensitizers increase up to 0.296 and 0.292%, respectively.
Hydrothermal treatment is an efficient and environmentally friendly method of enhancing the dimensional stability and durability of wood. The destructive effects of formic and acetic acids generated during thermal treatment, on the other hand, are known to have a negative impact on wood strength. As a result, hydrothermal treatment in different buffered media (acidic, neutral, and alkaline buffer) was performed in this study to mitigate the effects of the acids. As heating media, acidic buffer (pH 4 and 6), alkaline buffer (pH 8 and 10), and tap water (pH 7.43) were used to treat rubberwood at three different temperatures (160 °C, 180 °C, and 200 °C). The effects of different buffered media and treatment temperatures on the chemical components, crystallinity, and morphological changes in treated and untreated rubberwood were studied. The results of the experiments revealed that the chemical constituents of rubberwood changed along with the pH of the buffered media and treatment temperature. Rubberwood treated in alkaline media showed the least degradation, whereas water medium caused the most severe degradation. The crystallinity of wood increased initially (from 160 to 180 °C) and then decreased further at 200 °C. In addition, minimal damage to the wood cell was observed in an alkaline medium.