29 April 2014 in Journal of Metallurgy
Verified
Journal Article
Open access
PDF file
KIKhaled M Ibrahim
Khaled M Ibrahim
MIMervat M. Ibrahim
Mervat M. Ibrahim
The influence of heat treatment on microstructure and mechanical properties of high chromium white cast iron alloyed with titanium was investigated. The austenitizing temperatures of 980°C and 1150°C for 1 hour each followed by tempering at 260°C for 2 hours have been performed and the effect of these treatments on wear resistance/impact toughness combination is reported. The microstructure of irons austenitized at 1150°C showed a fine precipitate of secondary carbides (M6C23) in a matrix of eutectic austenite and eutectic carbides (M7C3). At 980°C, the structure consisted of spheroidal martensite matrix, small amounts of fine secondary carbides, and eutectic carbides. Titanium carbides (TiC) particles with cuboidal morphology were uniformly distributed in both matrices. Irons austenitized at 980°C showed relatively higher tensile strength compared to those austenitized at 1150°C, while the latter showed higher impact toughness. For both cases, optimum tensile strength was reported for the irons alloyed with 1.31% Ti, whereas maximum impact toughness was obtained for the irons without Ti-addition. Higher wear resistance was obtained for the samples austenitized at 980°C compared to the irons treated at 1150°C. For both treatments, optimum wear resistance was obtained with 1.3% Ti.

1 July 2023 in Materials
Verified
Journal Article
Open access
PDF file
HAHayam abokhasha ali
Hayam abokhasha ali
Mohamed M. El-Sayed Seleman El-NagarMohamed M. El-Sayed Seleman El-Nagar
Mohamed M. El-Sayed Seleman El-Nagar
ABAshraf Bakkar
Ashraf Bakkar
IAIbrahim Albaijan
Ibrahim Albaijan
Mohamed Mohamed Zaky AhmedMohamed Mohamed Zaky Ahmed
Mohamed Mohamed Zaky Ahmed
KIKhaled M Ibrahim
Khaled M Ibrahim
Thermal expansion measurements were used to characterize phase transformations in metastable β-Ti alloys (Ti15MoxSi) without and with various Si additions (where x = 0, 0.5, 1.0, 1.5, and 2 in wt.%) during linear heating at two heating rates of 5 and 10 °C/min up to 850 °C. For this study, five alloys were developed and examined in terms of their presence phases, microstructures, and starting and final transformation temperatures. According to the results, all of the as-cast samples primarily include an equiaxed β-Ti phase. The influence of phase transformation on the material dimensions was discussed and compared with the variations in Si contents. The transformation was investigated using a dilatometric technique for the developed alloys during continuous heating and cooling. The dilatometric curve of heating revealed two distinct reflection points as the heating temperature increased. The starting transformation temperature (Ts) to obtain the ω-phase was reported at 359 °C without Si addition; whereas the final transformation temperature (Tf) of the dissolution of α-phase was obtained at 572 °C at a heating rate of 10 °C/min. At 2 wt.% Si, the first derivative curves reported Ts and Tf transforming temperatures of 314–565 °C (at a 5 °C/min heating rate) and 270–540 °C (at a 10 °C/min heating rate), respectively. The Ts and Tf transforming temperatures were significantly decreased with Si additions, which decreased the β-transus temperature. Moreover, the thermal expansion coefficient curves of the investigated alloys without and with 2 wt.% Si were studied. The transformation heating curves have an S-shaped pattern, according to the results.

10 January 2023 in Materials
Verified
Journal Article
Open access
PDF file
MOmostafa mahmoud oweis
mostafa mahmoud oweis
SEShimaa El-Hadad
Shimaa El-Hadad
MSmahmoud sherif
mahmoud sherif
KIKhaled M Ibrahim
Khaled M Ibrahim
AFAhmed I. Z. Farahat
Ahmed I. Z. Farahat
Helmi AttiaHelmi Attia
Helmi Attia
A comparative study was conducted for the machining of two α/β titanium alloys, namely Ti-6Al-4V (Ti64) and Ti-6Al-7Nb (Ti67), using wire electric discharge machining (WEDM). The influence of cutting speed and cutting mode on the machined surfaces in terms of surface roughness (Ra), recast layer (RL), and micro-hardness have been evaluated. Rough cut (RC) mode at a cutting speed of 50 µm/s resulted in thermal damage; Ra was equal to 5.68 ± 0.44 and 4.52 ± 0.35 µm for Ti64 and Ti67, respectively. Trim-cut mode using seven cuts (TRC-VII) at the same speed decreased the Ra to 1.02 ± 0.20 µm for Ti64 and 0.92 ± 0.10 µm for Ti67. At 100 µm/s, Ra reduced from 2.34 ± 0.28 µm to 0.88 ± 0.12 µm (Ti64), and from 1.42 ± 0.15 µm to 0.90 ± 0.08µm (Ti67) upon changing from TRC-III to TRC-VII. Furthermore, a thick recast layer of 30 ± 0.93 µm for Ti64 and 14 ± 0.68 µm for Ti67 was produced using the rough mode, while TRC-III and TRC-VII modes produced layers of 12 ± 1.31 µm and 5 ± 0.72 µm for Ti64 and Ti67, respectively. Moreover, rough cut and trim cut modes of WEDM played a significant role in promoting the surface hardness of Ti64 and Ti67. By employing the Response Surface Methodology, it was found that the machining mode followed by cutting speed and the interaction between them are the most influential parameters on surface roughness. Finally, mathematical models correlating machining parameters to surface roughness were successfully developed. The results strongly promote the trim-cut mode of WEDM as a promising machining route for two-phase titanium alloys.

5 February 2023 in Metals
Verified
Journal Article
Open access
PDF file
Mohamed RamadanMohamed Ramadan
Mohamed Ramadan
TSTayyab Subhani
Tayyab Subhani
Khalid Mohamed HafezKhalid Mohamed Hafez
Khalid Mohamed Hafez
NANAGLAA FATHY ABDELFATAH
NAGLAA FATHY ABDELFATAH
BABadreddine Ayadi
Badreddine Ayadi
KIKhaled M Ibrahim
Khaled M Ibrahim
Iron oxide and silica nanoparticles were individually incorporated in tin-based Babbitt alloy and combined to prepare a novel class of nanocomposites for bearing material applications. The route of liquid metallurgy in combination with the stirring technique was adopted to manufacture nanocomposites. Microstructural evolution and mechanical property evaluation were performed by optical and electron microscopy, EDS, hardness, compression, and wear tests. The morphology of the Cu6Sn5 phase was changed from elongated to spherical in the microstructures of nanocomposites. The solitary addition of 0.5 wt% iron oxide nanoparticles improved the hardness and compressive strength but adversely affected the wear properties by increasing the weight loss and friction coefficient value. In contrast, the addition of 0.5 wt% silica nanoparticles could not significantly increase the hardness and compressive strength but it could improve the tribological properties by reducing the weight loss and friction coefficient value. Tin-based Babbitt alloy showed a compressive strength of 89.22 ± 0.50 MPa after the addition of 0.5 wt% iron oxide showing a rise of ~11%. The combined effect of the addition of both types of nanoparticles showed considerable results, i.e., a rise of ~7.9% (86.75 ± 0.68 MPa). The balanced approach of incorporating dual reinforcements of 0.25 wt% iron oxide and 0.25 wt% silica nanoparticles intermediately improved the hardness, compressive strength, and decreased weight loss.

22 December 2010 in Journal of Materials Engineering and Performance
Verified
Journal Article
Closed access
PDF file
KIKhaled M Ibrahim
Khaled M Ibrahim
MMMansour Mhaede
Mansour Mhaede
LWLothar Wagner
Lothar Wagner

1 July 2012 in International Journal of Materials Research
Verified
Journal Article
Closed access
RRReham Reda
Reham Reda
ANAdel A. Nofal
Adel A. Nofal
KIKhaled M Ibrahim
Khaled M Ibrahim
AHAbdel-Hamid A. Hussien
Abdel-Hamid A. Hussien
This research studies the effect of dynamic solidification, niobium addition, and their combined action on the as-cast structure and mechanical properties of hypoeutectic 15% Cr-2% Mo white cast irons containing 2.5% C. The effect of heat treatment at different tempering temperatures was also studied. Investigations were performed by means of image analysis, scanning electron microscopy, and X-ray diffraction. Abrasion resistance and impact toughness tests were performed. Fracture and worn surfaces were studied. Results show that optimized abrasion resistance and impact toughness can be achieved in a homogeneous microstructure consisting of hard, fine, and non-interconnected carbides in a matrix that has a high fraction of metastable austenite.