The creep properties of directionally solidified superalloys are largely influenced by the degradation rate of the γ/γ’ microstructure and the dislocation motion, which exhibit distinct mechanisms under varying temperature and stress conditions. In this study, the creep deformation mechanisms and microstructural evolution of a directionally solidified nickel-based superalloy in the longitudinal (L) and transverse (T) orientations at 850 °C are comprehensively investigated. Creep testing and characterization of the dislocation structure revealed superior creep properties in the L direction compared to the T direction. The creep mechanism in the L direction involves the activation of multiple {111} slip systems, shearing the γ’ precipitates through antiphase boundaries (APBs). Conversely, the creep mechanism in the T direction involves the activation of {111} slip systems, shearing the γ’ precipitates through a superlattice intrinsic stacking fault (SISF) and forming slip bands inclined to the stress axis. Aluminum was identified as the controlling element for the γ’ rafting. The longitudinal specimens exhibited P-type rafting due to the activation of multiple slip systems and sufficient plastic strain flow from the dislocation motion. In contrast, the transverse specimens show little rafting due to limited slip system activation. These findings can serve as a reference for better understanding the anisotropy of directionally solidified superalloys and provide a basis for their broader application.
A new grain growth model was developed by introducing the ultimate grain size to the traditional model. The grain growth behavior and its ultimate size under the Zenner pinning force are also discussed. This model was applied to the nickel-based superalloy and integrated into an FEM code. The grain evolution of a forged third-generation powder superalloy heat treated at different temperatures and holding times was studied. A gradient heat treatment setup was designed and implemented for a full-size turbine disc based on the model prediction to meet the accurate dual-microstructure requirements of an advanced aero-engine turbine disc design. The predicted temperature was validated by thermal couple measurements. The relative error between the prediction and the measurements is less than 2%. The metallographic examination of the whole turbine disk through sectioning showed that the grain size was ASTM 7-8 at the rim area and ASTM 11-12 at the bore region, which agrees well with the prediction. The predicted values of the three measurement areas are ASTM 12.1, ASTM 9.1, and ASTM 7.1, respectively, with a maximum error of 5% compared to the measured values. The proposed model was validated and successfully applied to help manufacture a dual-microstructure aero-engine turbine disc.
Regulating the microstructure of powder metallurgy (P/M) nickel-based superalloys to achieve superior mechanical properties through heat treatment is a prevalent method in turbine disk design. However, in the case of dual-performance turbine disks, the complexity and non-uniformity of the heat treatment process present substantial challenges. The prediction of yield strength is typically derived from the analysis of microstructures under various heat treatment regimes. This method is time-consuming, expensive, and the accuracy often depends on the precision of microstructural characterization. This study successfully employed a coupled method of Artificial Neural Network (ANN) and finite element analysis (FEA) to reveal the relationship between the heat treatment process and yield strength. The coupled method accurately predicted the location specified and temperature-dependent yield strength based on the heat treatment parameters such as holding temperatures and cooling rates. The root mean square error (RMSE) and mean absolute percentage deviation (MAPD) for the training set are 50.37 and 3.77, respectively, while, for the testing set, they are 50.13 and 3.71, respectively. Furthermore, an integrated model of FEA and ANN is established using a Abaqus user subroutine. The integrated model can predict the yield strength based on temperature calculation results and automatically update material properties of the FEA model during the loading process simulation. This allows for an accurate calculation of the stress–strain state of the turbine disk during actual working conditions, aiding in locating areas of stress concentration, plastic deformation, and other critical regions, and provides a novel reliable reference for the rapid design of the turbine disk.
This study investigates the microstructural evolution and its effect on the fatigue performance of a novel nickel-based powder superalloy FGH4113A (WZ-A3) after long-term aging at 760 °C and 815 °C. The results show that long-term aging both at 760 °C and 815 °C has no significant effect on the grain size and morphology of the alloy. After aging at 760 °C for up to 2020 h, the size of the γ′ phase remains unchanged, and its morphology transitions from nearly square to nearly spherical. During long-term aging at 815 °C for 440 h, γ′ phase coarsening and spheroidizing occur simultaneously. With prolonged aging time, the size and spheroidization degree of the γ′ phase further increase. During long-term aging up to 440 h at 760 °C, the dispersed granular MC and M6C carbides dissolve and re-precipitate. By 2020 h of aging, flocculent carbides precipitate and non-continuous M6C and M23C6 accumulate at grain boundaries. After long-term aging at 815 °C for 440 h, flocculent carbides begin to precipitate within the grains. By 2020 h of aging, a large amount of flocculent carbides precipitate with significant coarsening and enrichment of the grain boundary carbides. Due to the insignificant coarsening of the γ′ phase as well as the enrichment and precipitation of the grain boundary carbides, the fatigue performance of the alloy decreases slightly after long-term aging.