Aimed at solving the problems of single control measures in the electro-spark deposition (ESD) process, difficulty controlling the micro-process using heterogeneous materials (for the electrode and matrix), and the unstable quality and reliability of repairs to the deposition layer, a method of magnetic-field-assistance electro-spark deposition (MFESD) was proposed. An MFESD device was built, and a Ni electrode was used for deposition on the surface of 45 steel under the conditions of deposition voltages of 30 V, 60 V, and 90 V, respectively. This study examined the impact of the magnetic field’s intensity and frequency on the microstructure and mechanical properties of electro-spark deposition layers. The results show that the sputtering and protrusion of the electrode material on the surface of the deposition layer gradually decrease with an increase in the magnetic field’s intensity and frequency, defects such as pores and cracks are obviously improved, and the structure is uninterrupted and compact. The surface roughness of the deposited layer decreases with an increase in the magnetic field’s intensity and frequency, and its surface roughness decreases by 44.3%. The cross-section effect of the deposited layer is improved. The thickness of the deposited layer increases with an increase in the magnetic field’s intensity and frequency; the thickness of the deposited layer increases by 13.39%, and its maximum thickness can reach 54.396 μm. At the same time, the microhardness of the deposited layer increases with an increase in the two aforementioned properties of the magnetic field, and its hardness increases by 5.32%. Using a magnetic field to control ESD can effectively control the microscopic process of deposition and obtain high-quality deposition coatings, which have important significance in the surface remanufacturing of key components of high-end equipment.
As a surface-strengthening technology, electro-spark deposition (ESD) is widely used in the strengthening and repair of key components of high-end equipment. In this paper, a fusion and solidification model of ESD coating is established. The method of heat–fluid–solid interaction is adopted to simulate the material’s flow and fusion process in the droplet dropping into the molten pool. The distribution law of the coating-matrix material inside the coating was studied. Through the heat transfer between the molten material and the matrix material, the condensation and solidification process of the coating-matrix material is simulated, the temperature change in the coating area during the solidification process is analyzed, and the solidification law of the molten material is studied. The results show that the deposition time reaches 80 μs, and the content of electrode material at the bottom of the molten pool reaches 4.5%. The content of electrode material in the upper region of the material gushing out of the molten pool is higher than that in the bottom region. The material outside the molten pool solidifies first, and the molten material in the molten pool gradually solidifies from the bottom up; the shape of the solidification interface is similar to the boundary of the molten pool. Through the single-point deposition experiment of electro-spark deposition, the surface morphology of the deposition point was observed. The depth of the concave part of the contour can reach 16 μm. The difference between the two contour curves in the horizontal direction is not much; the error of the diameter is about 4%. The element distribution of the surface and the section of the deposition point are analyzed. The diffusion distance in the depth direction of the coating is about 4μm, and the transverse diffusion distance inside the coating is 364 μm. The error is 7.6% compared with the experimental results. The cross-section structure of the deposition point was observed, and the error between the experimental results and the simulation results in diameter is about 11%. It was found that the material distribution in the sedimentary area is basically consistent with the simulation results, and the simulation results are verified from the side.
Based on the COMSOL simulation software (v.6.1), this paper systematically investigates the influence law of runner length on the velocity and pressure distribution of cathode and anode gas runners in proton exchange membrane fuel cells (PEMFCs), and experimentally verifies the measurement effect of thin-film thermocouples on the operating temperature of PEMFCs. The simulation results show that the maximum pressure of the cathode and anode increases nonlinearly with the increase in the runner length, while the velocity distribution remains stable; the shortening of the runners significantly reduces the friction loss along the flow path and optimizes the matching of the permeability of the porous medium. In addition, the NiCr/NiSi thin-film thermocouple prepared by magnetron sputtering exhibits high accuracy (Seebeck coefficient of 41.56 μV/°C) in static calibration and successfully captures the dynamic response characteristics of temperature in PEMFC operation. This study provides a theoretical basis and experimental support for the optimization of fuel cell flow channel design and temperature monitoring technology.