We report on an experimental study and statistical optimization of the surface roughness using design of experiments and the Taguchi method for parts made of 1.2709 maraging steel. We employ a hybrid additive manufacturing approach that combines additive manufacturing by selective laser melting with subtractive manufacturing using milling in an automated process within a single machine. Input parameters such as laser power, scan speed, and hatching distance have been varied in order to improve surface quality of unmachined surfaces. Cutting speed, feed per tooth, and radial depth of cut have been varied to optimize surface roughness of the milled surfaces. The surfaces of the samples were characterized using 3D profilometry. Scan speed was determined as the most important parameter for non-machined surfaces; radial depth of cut was found to be the most significant parameter for milled surfaces. Areal surface roughness could be reduced by up to 40% for unmachined samples and by 23% for milled samples as compared to the prior state of the art.
We report on high precision high speed micromachining of Al2O3 and AlN using pulsed near infrared fiber laser. Ablation thresholds are determined to be 30 J/cm2 for alumina and 18 J/cm2 for aluminum nitride. The factors influencing the efficiency and quality of 3D micromachining, namely the surface roughness, the material removal rate and the ablation depth accuracy are determined as a function of laser repetition rate and pulse overlap. Using a fluence of 64 J/cm², we achieve a material removal rate of up to 94 mm³/h in Al2O3 and 135 mm³/h in AlN for high pulse overlaps (89% and 84%). A minimum roughness of 1.5 μm for alumina and 1.65 μm for aluminum nitride can be accomplished for medium pulse overlaps (42% to 56%). In addition, ablation depth deviation of the micromachining process of smaller than 8% for alumina and 2% for aluminum nitride are achieved. Based on these results, by structuring exemplarily 3D structures we demonstrate the potential of high quality and efficient 3D micromachining using pulsed fiber laser.
Thin film ablation with pulsed nanosecond lasers can benefit from the use of beam shaping optics to transform the Gaussian beam profile with a circular footprint into a Top-Hat beam profile with a rectangular footprint. In general, the quality of the transformed beam profile depends strongly on the beam alignment of the entire laser system. In particular, the adjustment of the beam shaping element is of upmost importance. For an appropriate alignment of the beam shaper, it is generally necessary to observe the intensity distribution near the focal position of the applied focusing optics. Systems with a low numerical aperture (NA) can commonly be qualified by means of laser beam profilers, such as a charge-coupled device (CCD) camera. However, laser systems for micromachining typically employ focus lenses with a high NA, which generate focal spot sizes of only several microns in diameter. This turns out to be a challenge for common beam profiling measurement systems and complicates the adjustment of the beam shaper strongly. In this contribution, we evaluate the quality of a Top-Hat beam profiling element and its alignment in the working area based on the ablated geometry of single pulse ablation of thin transparent conductive oxides. To determine the best achievable adjustment, we develop a quality index for rectangular laser ablation spots and investigate the influences of different alignment parameters, which can affect the intensity distribution of a Top-Hat laser beam profile.
We report on a comprehensive study of laser percussion microvia drilling of FR-4 printed circuit board material using ultrashort pulse lasers with emission in the green spectral region. Laser pulse durations in the pico- and femtosecond regime, laser pulse repetition rates up to 400 kHz and laser fluences up to 11.5 J/cm are applied to optimize the quality of microvias, as being evaluated by the generated taper, the extension of glass fiber protrusions and damage of inner lying copper layers using materialography. The results are discussed in terms of the ablation threshold for FR-4 and copper, heat accumulation and pulse shielding effects as a result of pulse to pulse interactions. As a specific result, using a laser pulse duration of 2 ps appears beneficial, resulting in small glass fiber protrusions and high precision in the stopping process at inner copper layer. If laser pulse repetition rates larger than 100 kHz are applied, we find that the processing quality can be increased by heat accumulation effects.
We compare different lattice structures with various elementary cell sizes built by laser powder bed fusion with and without hot isostatic pressing as post treatment. Cylindrical lattice structures are mechanically tested upon static and dynamic load in order to achieve high elasticity, high fracture strength and a high number of cycles to failure with respect to applications as medical implants. Evaluating the Young’s modulus, a high stiffness for the body diagonal structure and a low fracture stress for the G-structure are measured. Hot isostatic pressing results in a higher Young’s modulus and is ambiguous in terms of fractural stress. While samples without hot isostatic pressing reveal a shear fracture, the hot isostatic pressed samples have a high ductile area where the lattice layers are wrapped and pressed into the underlying layers without a fracture. Under dynamic load, the samples without hot isostatic pressing mostly are unable withstand 106 cycles at typical loads of the human body. Hot isostatic pressing has no significant influence on the strength at high loads and low cycle numbers, but at low loads all samples survived 106 cycles. As a consequence, dode-thick and rhombic dodecahedrons with 2 mm and 1.5 mm lattice size after hot isostatic pressing are recommended for medical implants because of the high elasticity, high fracture stress and high resistance against dynamic loads, which fulfill implant requirements.