4 September 2023 in KSCE Journal of Civil Engineering
Verified
Journal Article
Open access
ASAli Sinan Soğancı
Ali Sinan Soğancı
YYYavuz Yenginar
Yavuz Yenginar
AOAli Orman
Ali Orman

28 March 2023 in Bulletin of Engineering Geology and the Environment
Verified
Journal Article
Closed access
PDF file
YYYavuz Yenginar
Yavuz Yenginar
MOMurat Olgun
Murat Olgun

11 July 2024 in Bulletin of Engineering Geology and the Environment
Verified
Journal Article
Open access
PDF file
YYYavuz Yenginar
Yavuz Yenginar
MOMurat Olgun
Murat Olgun
The novel approach of the study is implementing the installation procedure of fly ash (FA) replaced cement deep mixing (DM) columns to field cases aiming at managing FA waste and reducing cement utilization. FA replaced cement DM columns (diameter of 30 cm and length of 80 cm) were installed on clayey soils using a laboratory type DM machine. The effect of installation parameters such as the binder dosage, FA replacement ratio, superplasticizer content, water/binder ratio, and the liquidity index (LI) of the soil on column performance was investigated. The design of experiments and optimization process were conducted using the Taguchi method, S/N and ANOVA analyses, and the desirability function method. Observations have shown that the mixing time required for a homogeneously mixed column depends on the LI of the soil and the volume ratio (VR) of the slurry. A key parameter (LI∙VR) is defined to decide the minimum number of the mixing process. The blade rotation number should be minimum of 252 rev/m to obtain a homogeneous soil-slurry mixture. The highest strength of the column was obtained when LI of fresh soilcrete (LImix) is 1.25∙LI. Optimum installation parameters were determined as binder dosage of 425 kg/m3, FA replacement ratio is 40%, superplasticizer content is 3%, water/binder ratio is 0.8, and LI of the untreated soil is 1. In the optimum design, the mixing efficiency of the soil-slurry mixture increased and the best column performance was obtained. In addition, cement utilization and binder cost decrease 40% and 33%, respectively, in FA-replaced cement DM columns. SEM images prove the increase in column performance due to the cementation products (CSH and CAH gels) formed in the microstructure of the column.

3 April 2024 in Sustainability
Verified
Journal Article
Open access
PDF file
ASAli Sinan Soğancı
Ali Sinan Soğancı
YYYavuz Yenginar
Yavuz Yenginar
IÖIlyas Özkan
Ilyas Özkan
YGYusuf Guzel
Yusuf Guzel
AOAdnan Ozdemir
Adnan Ozdemir
Red mud (RM) is a waste material obtained during the production of aluminum from bauxite minerals. RM causes environmental pollution due to its high alkaline properties. Therefore, RM materials are stored in waste reservoirs. As production continues, the number of required waste reservoirs increases day by day. This study aims to utilize RM waste material in construction structures to contribute to the economy. The research investigates the potential use of RM waste material as road fill material. RM was improved using another waste material of fly ash (FA) since RM has low strength. Atterberg limit tests, compaction tests, unconfined compression tests, CBR tests, and SEM analyses were conducted on stabilized RM samples. In the physical properties of stabilized RM, Atterberg limits and optimum moisture content increase and density decreases since FA content increases. In the mechanical properties of stabilized RM, unconfined compressive strength, initial and secant modulus of elasticity, and California bearing ratio increase and maximum peak strain decreases since FA content and curing period increase. SEM images prove the increase in mechanical properties due to the cementation products (CSH and CAH gels) formed in the microstructure of stabilized RM. The results showed that RM waste stabilized with FA can be used as road subgrade material.

10 August 2023 in Engineering Failure Analysis
Verified
Journal Article
Closed access
YYYavuz Yenginar
Yavuz Yenginar
IÖİlYas Özkan
İlYas Özkan

15 December 2021 in International Advanced Researches and Engineering Journal
Verified
Journal Article
Open access
PDF file
YYYavuz Yenginar
Yavuz Yenginar
AMAhmed A. M. M. Mobark
Ahmed A. M. M. Mobark
MOMurat Olgun
Murat Olgun
In the present research, the optimum condition of the grout consisting of cement, fly ash, superplasticizer, and water was determined to produce the most durable and impermeable deep mixing columns (DMC) on silty soils. It is aimed to reduce the grout cost and environmental pollution by using high-rate fly ash in the grout. Superplasticizer additive was used to increase the flow consistency of grout consisting of high-rate fly ash. The design of the experiments was made using the 5-parameter and 4-level L16 orthogonal array table specific to the Taguchi method. Accordingly, the unconfined compression strength (qu) and the permeability coefficient (k) of the soil-binder mixtures at the end of the 7- and 28-days curing time were determined. According to the test results, regression analyzes were performed and models with high reliability were created for qu and k. As a result of optimization studies, to produce DMC having high strength and low permeability, grout content should be consisting of 14% cement, 14% fly ash (ratio of fly ash in the binder is 50%), 2.68% super plasticizer additive, and 0.95 water/binder ratio. The pozzolanic reactions in soil-binder samples with different grout contents were examined by SEM analysis.