Bismuth ferrite (BiFeO3, BFO) is one of the few single-phase crystalline compounds exhibiting strong multiferroic properties at room temperature, which makes it promising for use in various fields of science and technology. The remarkable characteristics of BFO at the nanoscale position it as a compelling candidate for enhancing the functionalities of polymeric nanocomposite materials. In this study, we explore the fabrication of polyvinylidene fluoride (PVDF) nanocomposites with a variable content of BFO nanopowders (0, 5, 10, 15, 20, and 25 wt%) by solution casting in the form of thin films with the thickness of ~60 µm. Our findings reveal that the presence of BFO nanoparticles slightly facilitates the formation of β- and γ-phases of PVDF, known for their enhanced piezoelectric properties, thereby potentially expanding the utility of PVDF-based materials in sensors, actuators, and energy harvesting devices. On the other hand, the increase in filler concentration leads to enlarged spherulite diameter and porosity of PVDF, as well as an increase in filler content above 20 wt% resulting in a decrease in the degree of crystallinity. The structural changes in the surface were found to increase the hydrophobicity of the nanocomposite surface. Magnetometry indicates that the magnetic properties of nanocomposite are influenced by the BFO nanoparticle content with the saturation magnetization at ~295 K ranging from ~0.08 emu/g to ~0.8 emu/g for samples with the lowest and higher BFO content, respectively.
This study investigates the effect of polyvinylidene fluoride–CoFe2O4 (PVDF-CFO) composite film thickness on their supramolecular structure, phase composition, and dielectric properties. The composites were synthesized from PVDF with CFO nanoparticles using the Dr. Blade method to obtain film thicknesses ranging from 15 to 58 μm. The data obtained show that the thinner film (15 μm) has a higher β-phase content compared to the thicker films (58 μm), as confirmed by FTIR and Raman spectroscopy. Scanning electron microscopy (SEM) showed that increasing film thickness within the studied range leads to the development of larger spherulitic structures and increased porosity. Atomic force microscopy (AFM) analysis also showed that thicker films have higher tensile strength due to their larger cross-sectional area, while thinner films exhibit lower elasticity. A more uniform microstructure and an increased electroactive phase in thin films result in increased permittivity, which is critical for PVDF-based sensors and energy devices.