Junyi Cheng

Mr. Junyi Cheng

orcid

Research Focus & Metrics

Academic Career Length

2Years (2025-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
28 April 2025 in Materials
Verified
Journal Article
Open access
PDF file
ALAnping Long
Anping Long
LSLiu Xiao Shan
Liu Xiao Shan
JCJunyi Cheng
Junyi Cheng
JXJiangying Xiong
Jiangying Xiong
GFGanjiang Feng
Ganjiang Feng
RLRutie Liu
Rutie Liu
Directionally solidified (DS) superalloys have become a primary material choice for turbine blade applications. Due to the complex shape of the blades, certain regions inevitably experience stress axes oriented orthogonally to the crystal growth direction. Therefore, this study explores the creep characteristics of a DS superalloy in different orientations (transverse (T) versus longitudinal (L) with respect to grain growth direction) under intermediate and high temperatures (980 °C and 1070 °C), while simultaneously analyzing their respective deformation mechanisms and microstructural transformation behaviors. Experimental findings reveal pronounced orientation-dependent variations in creep performance, deformation modes, and microstructural development. Notably, the T specimen exhibits higher creep resistance at 980 °C, which can provide a basis for the design of some components that require high creep resistance and maintain small deformation. At 980 °C, L specimens primarily undergo γ′ phase shearing via antiphase boundaries (APBs) pairs, whereas T specimen exhibits APB pairs and superlattice intrinsic stacking faults (SISFs) shearing mechanisms. At 1070 °C, the L specimen exhibits dislocation shearing of γ′ alongside dislocation bypassing of tertiary γ′, while the T specimen demonstrates dislocation climbing within the γ channels. Additionally, the L specimen exhibits significant N-type rafting, while the T specimen shows significant Ostwald ripening characteristics, with an Ostwald ripening rate constant of 1.04 × 10−20 m3/h.

4 April 2025 in Metals
Verified
Journal Article
Open access
PDF file
JCJunyi Cheng
Junyi Cheng
JXJiangying Xiong
Jiangying Xiong
ALAnping Long
Anping Long
LXLei Xiao
Lei Xiao
XMXiangdong Ma
Xiangdong Ma
JGJianzheng Guo
Jianzheng Guo
Precise control of forging and heat treatment parameters is essential to achieve microstructural homogeneity in turbine disks, ensuring optimal mechanical performance for aerospace applications. This study examines the influence of the hot deformation temperatures on the grain size and γ′ phase characteristics of U720Li alloy following subsequent heat treatments. Samples extracted from a hot-extruded U720Li billet were subjected to isothermal compression within the temperature range of 1100–1130 °C, followed by holding at 1100 °C and 1120 °C for 4 h and air cooling. The results demonstrate that increasing the deformation temperature from 1100 °C to 1120 °C reduces the γ′ phase volume fraction at grain boundaries from 13% to 5%, weakens pinning effects, promotes grain growth during deformation, elevates grain boundary energy, and diminishes stored deformation energy, despite maintaining an equivalent degree of dynamic recrystallization. When the sub-solvus heat treatment temperature was 20 °C below the effective deformation temperature, Ostwald ripening dominated, resulting in a multimodal γ′ phase distribution after cooling. Conversely, when the sub-solvus heat treatment temperature 20 °C exceeded the effective deformation temperature, a significant portion of the intergranular γ′ phase dissolved, leaving a bimodal distribution comprising both large- and small-sized particles.

25 February 2025 in Materials
Verified
Journal Article
Open access
PDF file
JXJiangying Xiong
Jiangying Xiong
CYChao Yin
Chao Yin
ALAnping Long
Anping Long
JCJunyi Cheng
Junyi Cheng
GFGanjiang Feng
Ganjiang Feng
JGJianzheng Guo
Jianzheng Guo
A novel nickel-based powder metallurgy superalloy was processed using two different thermal–mechanical processes, including hot isostatic pressed (As-HIP) and hipped + hot extruded + isothermally-forged (IF) heat treatments following two processed alloys, designated as As-HIP-HT and IF-HT. The objective of this study is to investigate the microstructure and mechanical property evolution in a nickel-based powder disk alloy fabricated by two processes. The findings revealed that both As-HIP and IF alloys underwent substantial recrystallization, with grains in the IF alloy being finer. Notable Prior Particle Boundaries (PPBs) were identified in the As-HIP samples. The IF-HT alloy exhibited a larger grain size due to a greater amount of stored energy. Significant differences in the secondary γ′ precipitates were observed between the two processes. More uniform substructures in the IF-HT alloy led to a higher density of finer γ′ precipitates. At temperatures of 704 °C and 760 °C, the As-HIP-HT alloy displayed a higher yield strength, but its plasticity significantly declined as temperature increased, while the IF-HT alloy showed a relatively stable plasticity. The presence of PPBs in the As-HIP-HT alloy minimally affected the alloy’s strength but reduced its plasticity. The creep property of the two processes was compared at 800 °C/330 MPa; the IF-HT alloy demonstrated lower creep rates and a longer creep life, which was attributed to its finer γ′ precipitates. Dominant creep deformation mechanisms in the As-HIP-HT alloy included Orowan dislocation loops and deformation twinning, while the primary mechanisms in the IF-HT alloy involved dislocation cutting through γ′ precipitates, dislocation slip, and micro-twins. These findings support the use of isostatic pressing + hot extrusion+ isothermally-forging process for critical high-temperature components.