The interaction effect of micro arc oxidation (MAO) parameters on the microstructure and wear properties was investigated. The results showed that the electric current and oxidation time significantly influenced the thickness and grinding crack width of the ceramic coatings within the range of the selected parameters, and the interaction effect of the electrical parameters was not obvious. The surface morphology, cross-section morphology, and element distribution of the coatings were observed using scanning electron microscopy (SEM) with energy dispersive spectroscopy (EDS) and X-ray diffraction (XRD). The results showed that ceramic coatings with γ-Al2O3 and α-Al2O3 formed, which enhanced the coating performance. After that, the microhardness and wear resistance were tested. Under the optimal process, the microhardness of a coating section was up to 1200 HV0.1, and the friction coefficient was just 0.3. When wear occurred, the volcanic microstructures experienced extrusion and deformation, and then peeled off under shear stress, which led to the formation of a grinding crack. The main failure modes of the micro arc oxidation coatings were abrasive wear and spalling failure.
3 October 2018 in Journal of Materials Engineering and Performance
In this study, to further improve the performance of micro-arc oxidation (MAO) coatings, ZrO2 nanoparticles at different concentrations were added to the electrolyte. The effects of ZrO2 concentration on the microstructure, mechanical properties and corrosion resistance of the MAO composite coatings were systematically investigated. The coatings mainly consisted of α-Al2O3 and γ-Al2O3. The detection of ZrO2 confirmed the incorporation of the added particles. As the concentration increased from 0 to 6 g/L, the porosity decreased from 1.352% to 0.864%, whereas further addition increased the porosity. At 6 g/L, the mean microhardness reached 623 ± 50 HV0.05. Moreover, this coating showed the lowest friction coefficient of 0.135. In addition, its corrosion potential was −0.148 V, while its corrosion current density was 2.578 × 10−7 A·cm−2. It also exhibited the highest low-frequency impedance modulus. When the ZrO2 concentration was further increased, the coating porosity increased and the improvements gradually weakened. Overall, a suitable ZrO2 concentration promoted coating growth and reduced structural defects. It also improved the hardness, wear behavior and corrosion protection of the coating. Therefore, these findings provide a reference for the concentration design of ZrO2-modified MAO coatings. They also clarify the nonmonotonic relationship between coating growth, structural defects and performance.