Development of fiber reinforced filaments for fused deposition modeling - FDM shifted this technology application towards load carrying applications. For polymer materials reinforced with carbon fibers, it is important to carry out annealing of printed products to improve the mechanical properties. In this paper ANOVA approach was used to evaluate the effect of temperature and time of the annealing treatment of PA 6 filament reinforced with short carbon fibers (PA 6 - CF). Results indicate that higher temperatures (between 110 °C – 170 °C) result in better effects on tensile properties while duration of the annealing effect was neglible in most cases. An increase of up to 16.7% in tensile strength and up to 35% in tensile modulus can be achieved with proper annealing parameters. In some cases, annealing results in a decrease in tensile strain at break up to 35%. The p-values for tensile strength, strain and modulus are 0.0038, 0.0054, 0.0168, respectively, which indicates that the selected model of the influence of annealing parameters is significant because the p-value must be less than 0.05. The highest improvement in tensile strength and modulus was observed at a temperature of 170 °C, but this temperature is close to the softening temperature of PA 6 - CF, which is approximately 180 °C before annealing, which risks deformation of products.
Warpage is among the most prevalent defects affecting injection molded parts. In this study, we aimed to develop methods to minimize warpage through mold design. Common strategies include matching the cavity geometry to the intended shape of the part, adjusting cavity dimensions to offset material shrinkage, and optimizing the cooling system and critical injection molding parameters. These optimization methods can offer significant improvements, but recently introduced methods that optimize the molded part and mold cavity shape result in higher levels of warpage reduction. In these methods, optimization of the shape of the molded part is achieved by shaping it in the opposite direction of warpage—a method known as inverse contouring. Inverse contouring of molded parts is a design technique in which mold cavities are intentionally modified to incorporate compensatory geometric deviations in regions anticipated to exhibit significant warpage. The final result after molded part ejection and warpage is a significant reduction in deviations between the warped and reference molded part geometries. In this study, a two-step approach for minimizing warpage was used: the first step was optimizing the most significant injection molding parameters, and the second was inverse contouring. In the first step, Response Surface Methodology (RSM) and Autodesk Moldflow Insight 2023 simulations were used to optimize molded part warpage based on three processing parameters: melt temperature, target mold temperature, and coolant temperature. For improved accuracy, a Computer-Aided Design (CAD) model of the warped molded part was exported into ZEISS Inspect 2023 software and aligned with the reference CAD geometry of the molded part. The maximal warpage value after the initial simulation was 1.85 mm based on Autodesk Moldflow Insight simulations and 1.67 mm based on ZEISS Inspect alignment. After RSM optimization, the maximal warpage was 0.73 mm. In the second step, inverse contouring was performed on the molded part, utilizing the initial injection molding simulation results to further reduce warpage. In this step, the CAD model of the redesigned, inverse-contoured molded part was imported into Moldflow Insight to conduct a second iteration of the injection molding simulation. The simulation results were exported into ZEISS Inspect software for a final analysis and comparison with the reference CAD model. The warpage values after inverse contouring were reduced within the range of ±0.30 mm, which represents a significant decrease in warpage of approximately 82%. Both steps are presented in a case study on an injection molded part made of polybutylene terephthalate (PBT) with 30% glass fiber (GF).
Additive manufacturing procedures are being increasingly developed, from prototyping to finished functional products. However, their rapid development also brings along the testing of properties with different manufacturing parameters. In selective laser sintering, the most influential manufacturing parameter is the energy density, which also consists, among other things, of the hatch distance. For better usage of the entire chamber and a reduction in the overall price of the finished product, in practice, the manufacturing of products at different heights (levels) of the working chamber with different orientations is inevitable. The study examines how hatch distance and product orientation impact the tensile strength and dimensional stability of polyamide products across two levels within the chamber. Upon analysis, it was observed that manufacturing products at different levels within the working chamber does not influence their dimensions. Achieving precise product dimensions comparable to those in the CAD model is possible. Furthermore, the same factors (orientation and hatch distance) and their combinations affect the length, thickness, and width of the product. Although all test specimens were tested, a tensile strength analysis of variance (ANOVA) of test specimens produced at the lower level of the chamber with a combination of hatch distance (ranging from 0.23 to 0.6 mm) and orientation (ranging from 0° to 60°) was not feasible in the design of the experiment. Despite this limitation, it was noted that both chamber levels had the potential to reach a maximum tensile strength of 47 N/mm2. Nevertheless, the average tensile strength of PA12, obtained through combinations of input factors, stood at only 30 N/mm2, which is quite a low value for polyamide made by selective laser sintering.
Polymer composites have various application in automotive industry. Achieving vehicle efficiency in public transportation, among other goals, is often done by lightweight materials like fibre reinforced plastics as structural elements of the vehicle. A concept solution for a V shaped structural floor element of a city bus is proposed in this paper. CAD model of floor structural element has been designed from which, in later phases, construction of complete composite floor will be optimized and designed. Test sample made of hybrid (carbon and glass) fibre composite was produced and tested under the flexural load for comparison with a FEA model. Test sample displacement was measured using a GOM Tritop optical measurement system. Comparison showed that difference between real measurement and FEA for maximal displacement is only 11.7%.
The paper presents the optimisation of mould for injection moulding as well as injection moulding process parameters using numerical computer simulation in the Moldex3D software package. The optimisation process will be applied to a specific moulded part – branching terminal block – and an already manufactured mould. The paper includes evaluation of the existing mould for injection moulding designed and manufactured without application of numerical simulation of injection moulding process. According to the shortcomings found out in evaluation process, by application of numerical simulation of injection moulding process, the optimisation of the mould design was conducted in several stages to achieve as optimal as possible moulded part quality and injection moulding process parameters without dramatic changes in already manufactured mould.