The structural, chemical, and electrical properties of amorphous indium gallium zinc oxide (a-IGZO) films by magnetron sputtering and atomic layer deposition (ALD) were investigated where both a-IGZO films had a comparable cation composition. The ALD-derived a-IGZO film exhibited the higher atomic packing density, the effective suppression of trap-like oxygen vacancy defect (Vₒ), and the enhancement in the hybridization of the sp orbital of In, Ga, and Zn cations compared to those of the sputtered a-IGZO film. Hence, a significant improvement in terms of the field-effect mobility was observed for the thin-film transistors with an In0.50Ga0.34Zn0.16O channel by ALD (36.6 cm²/V· s) compared to that of the sputtered In0.48Ga0.38Zn0.14O transistor (20.1 cm²/V· s); the Ion/off ratios for both were ~ 10⁷. Simultaneously, the gate bias stress stability and photobias stress stability were also improved for the IGZO transistors with an ALD-derived channel, which can be explained by its reduced trap-like Vₒ density.
Indium–gallium–zinc oxide (IGZO) films, deposited by sputtering at room temperature, still require activation to achieve satisfactory semiconductor characteristics. Thermal treatment is typically carried out at temperatures above 300 °C. Here, we propose activating sputter- processed IGZO films using simultaneous ultraviolet and thermal (SUT) treatments to decrease the required temperature and enhance their electrical characteristics and stability. SUT treatment effectively decreased the amount of carbon residues and the number of defect sites related to oxygen vacancies and increased the number of metal oxide (M–O) bonds through the decomposition-rearrangement of M–O bonds and oxygen radicals. Activation of IGZO TFTs using the SUT treatment reduced the processing temperature to 150 °C and improved various electrical performance metrics including mobility, on-off ratio, and threshold voltage shift (positive bias stress for 10,000 s) from 3.23 to 15.81 cm2/Vs, 3.96 × 107 to 1.03 × 108, and 11.2 to 7.2 V, respectively.
Triboelectric nanogenerators (TENGs) are used as self-power sources for various types of devices by converting external waves, wind, or other mechanical energies into electric power. However, obtaining a high-output performance is still of major concern for many applications. In this study, to enhance the output performance of polydimethylsiloxane (PDMS)-based TENGs, highly dielectric TiO2−x nanoparticles (NPs) were embedded as a function of weight ratio. TiO2−x NPs embedded in PDMS at 5% showed the highest output voltage and current. The improved output performance at 5% is strongly related to the change of oxygen vacancies on the PDMS surface, as well as the increased dielectric constant. Specifically, oxygen vacancies in the oxide nanoparticles are electrically positive charges, which is an important factor that can contribute to the exchange and trapping of electrons when driving a TENG. However, in TiO2−x NPs containing over 5%, the output performance was significantly degraded because of the increased leakage characteristics of the PDMS layer due to TiO2−x NPs aggregation, which formed an electron path.