One of the options for reducing harmful emissions in the production of heat energy is the use of biomass, including in combination with industrial waste (for instance, coal and coke dust). Recent studies demonstrate that a mix of biomass and coal makes it possible to obtain a bio-coal briquette with better characteristics, which is a motivating factor in the search for alternative sources of heat energy from local agricultural waste. The aim of this research is to study the properties of bio-coal briquettes from biomass (sunflower husks and leaves) and industrial waste (coal and coke dust). The raw material was grinded and used for the production of bio-coal briquettes of 20%, 30%, 40%, 50%, 60%, and 70% of biomass. The biomass was grinded to the size of no more than 2 mm for the fine fraction and no more than 6 mm for the coarse fraction. The briquettes were made mechanically using a hydraulic press with a compression pressure of 25 MPa without the use of any binder. The characteristics of the investigated bio-coal briquettes, such as density, strength, moisture content, ash content, volatile yield, calorific value, ignition time, burning duration, and burning rate, have good enough values. The fine fraction briquettes compared to the coarse fraction briquettes have a longer burning time (about threefold longer) and a lower burning rate. For all briquettes, an increase in the composition of coal dust results in a rise in the burning time, whereas the burning rate falls. The best in terms of strength, calorific value and combustion parameters are the following briquettes: 70% sunflower husk and 30% coal dust from the Karazhyra deposit; 60% sunflower husk and 40% coal dust from the Shubarkul deposit; briquettes from 70% sunflower husk and 30% coke dust; briquettes from 80% leaves and 20% coal dust from the Karazhyra deposit; and briquettes from 70% leaves and 30% coal dust from the Shubarkul deposit. The selected briquettes are suitable as an alternative source of fuel.
The energy efficiency of high-temperature batch aggregates largely depends on the modes of their heating and cooling. The modes of heating and cooling of aggregates in which thermal stress does not exceed the critical values of the ultimate strength of the refractories make it possible to increase their service life. The increase in the service life of refractories will lead to a reduction in the number of lining repairs and a decrease in the specific consumption of refractory materials per ton of technological product. Shorter warm-up and cool-down times result in lower energy consumption. Reducing the time for variable modes for casting ladles increases their turnover (the number of melt discharges into the ladle per day). Increasing ladle turnover not only reduces the number of ladles but also improves the economic performance of the enterprise. The ultimate strength of the refractory material significantly affects the rate of temperature change during heating and cooling of the refractory masonry. The purpose of this research is to study the dependence of the ultimate compression and tensile strengths of chamotte materials of the ShKU brand on temperature. The determination of the compression and tensile strengths was carried out on new samples of refractory materials as well as on samples of refractories that were in operation until the intermediate repair. To determine the ultimate compression strength of chamotte refractories, the standard technique for axial compression of the test specimen until its destruction was used. To determine the ultimate tensile strength, a three-point bending test was used with additional control of the surface temperature of the test sample during the test. The ultimate compression strength of chamotte refractories of the ShKU-32 brand increased for the new refractories by a maximum of 44%. For refractories that were in operation until the intermediate repair, the ultimate compression strength increased by a maximum of 56%. The value of the ultimate tensile strength at elevated temperatures turned out to be higher than the value at a temperature of 20 °C. For new refractories, the maximum ultimate tensile strength is 25% higher than the ultimate tensile strength under normal conditions. For refractories that were in operation until the intermediate repair, the maximum ultimate tensile strength increased by 24%. The obtained results can be used to increase the rate of heating or cooling of linings.
The combustion of briquettes made from organic and industrial residues in small boilers requires researchers to consider the characteristics of this type of fuel and methods of its combustion. For the efficient combustion of fuel briquettes, a layered combustion method with the ability to regulate the supply of combustion air is better suited. The purpose of this research is to study the thermal technical conditions of briquetted fuel combustion. In order to carry this out, a stand was created, which made it possible to determine the combustion efficiency of this type of fuel. Two types of briquettes were studied: one with 30% sunflower husks and 70% leaves, and one with and 70% sunflower husks and 30% coke breeze. The combustion results of the briquettes show that heat loss from chemical under-burning was no more than 6.25%. To determine the temperature distribution in the fuel layer, a model of unsteady heat transfer in a fixed layer was used. A calculation of the temperature fields in the layer of burned fuel briquettes was carried out, which showed that the most favorable conditions for burning briquettes were created with a layer about 15–20 cm thick for both burned briquette options. The temperature was in the range of 450–750 °C, which on the one hand corresponds to experimental data and on the other hand provides a combustion regime that occurs with a relatively low loss to the environment. This installation and mathematical model will help future studies based on the processes of other types of organic waste combustion with a grate system.
An important element of the operation of high-temperature aggregates are modes that change over time. During these modes, maximum temperature changes are recorded in the cross-section of the lining of the aggregate. The difference in temperature leads to the formation of thermal stresses, which are the main reason for the repair of aggregates. During rapid heating, the inner layers of the lining are subjected to compressive stresses, while during rapid cooling, these layers experience tensile stresses. Under the same conditions, rapid cooling of the lining is more critical, since refractories have poor resistance to tension. The purpose of the study is to calculate and analyze the thermal stresses that arise during cooling of the casting ladle lining. The stresses are determined based on the calculation of the unsteady temperature field of the lining. Thermal stress values are necessary for analysis of the current cooling rates of casting ladles and subsequent development of optimal cooling modes for the lining. To solve the heat conductivity equation, a numerical method was chosen using an implicit four-point difference scheme. To study the cooling process of the casting ladle lining, temperature measurements were carried out in the zone of the greatest wear of the lining. Under conditions of natural convection, cooling of the casting ladle lining occurs unevenly. Cooling schedules during natural convection are characterized by significant unevenness and high rates of temperature decrease. The cooling rates of the inner surface of the lining at the initial stage of cooling significantly exceed the values recommended in the technical literature. Such cooling rates lead to the appearance of significant thermal stresses in the lining. For a refractory that has not been in service, the maximum thermal compressive stresses exceed the ultimate compressive strength by 1.27 times, and the tensile stresses exceed the corresponding limit values by 4.4 times. For refractories that have worked three fuses in the ladle lining, the maximum thermal compressive stresses exceed the ultimate compressive strength by 1.28 times, and the tensile stresses exceed the corresponding limit values by 3.19 times. The studied cooling modes for the casting ladle lining are unacceptable for operation. Cooling, taking into account the indicated rates, leads to the destruction of the lining material. To increase the resistance and duration of the working campaign of casting ladle linings, it is necessary to develop cooling modes for the lining at speeds at which the resulting thermal stresses do not exceed the strength of the refractory materials.
Drying of fragile granules of bulk materials has to be carried out in a fixed bed to prevent particle damage. This way of drying protects the granules, but the lack of mixing of the particles leads to an uneven distribution of heat and mass transfer conditions in the bed. It is necessary to be able to predict the distribution of drying conditions inside the bed to select a rational drying mode. In this paper, a mathematical model for drying bulk media in a fixed bed is proposed, its parametric identification is carried out, and the model is verified by comparison with experimental results. The numerical model is based on explicit difference schemes using the mathematical apparatus of Markov chains. The experimental study was carried out on a laboratory dryer with the detection of local drying parameters according to the height of the fixed bed. The numerical and experimental results were obtained at the fixed temperature (90 °C) and gas velocity (0.5 m∙s−1). It has been shown that at a certain bed height, areas with relative gas humidity above 100% are formed within it, which negatively affects the efficiency of the drying. The proposed model allows identifying the indicated ineffective drying modes, and has proven to be a reliable tool for predicting the moisture ratio of the material with an MAPE of less than 7%.
The refractory lining of high-temperature aggregates determines the duration of their operation before major repairs. The ability to retain technological material within the aggregate’s working area is the main factor for its continued operation. The analysis shows that the main reason for the destruction of the lining of ferroalloy production casting ladles is the occurrence of thermal stresses in the processes of heating and cooling the lining. When the stresses exceed the ultimate strength of the refractory material used, the material is destroyed. The greater the magnitude and duration of the excess thermal stresses, the faster the lining destruction occurs. Streamlining thermal regimes is the most low-cost and sufficiently effective way to increase the durability of linings. The development of lining heating and cooling regimes can be carried out on the basis of determining the thermal stress state by calculating the maximum permissible heating rates. The developed regimes allow for working at speeds at which the resulting stresses do not exceed the ultimate strength of the refractory materials. The aim of this study is to develop efficient cooling regimes for the lining of a ferroalloy production casting ladle from the standpoint of the resulting thermal stresses. A method for determining the thermal stresses in the lining has been developed and implemented using Microsoft Excel. This facilitates the use of the developed methodology in production without the need for special skills on the part of operating personnel. Using the developed methodology, the cooling schedules for the lining of ferroalloy production ladles were improved. To reduce temperature unevenness across the lining cross-section, a decision was made to initially heat the outer surface of the lining and cool the inner surface of the lining. Heating the outer surface can be achieved by using the heat of combustion of the ferroalloy gas or the heat of the exhaust gases from the stand for drying and heating casting ladles. Cooling the inner surface of the lining can be achieved by natural convection. The result of the development and implementation of an efficient cooling regime is a reduction in thermal stresses to the required level throughout almost the entire cooling process.