Developing cost-effective magnesium alloys with high strength and good ductility is a long-standing challenge for lightweight metals. Here we present a multimodal grain structured AZ91 Mg alloy with both high strength and good ductility, prepared through a combined processing route of low-pass ECAP with short-time aging. This multimodal grain structure consisted of coarse grains and fine grains modified by heterogeneous precipitates, which resulted from incomplete dynamic recrystallization. This novel microstructure manifested in both superior high strength (tensile strength of 360 MPa) and good ductility (elongation of 21.2%). The high strength was mainly attributed to the synergistic effect of grain refinement, back-stress strengthening, and precipitation strengthening. The favorable ductility, meanwhile, was ascribed to the grain refinement and multimodal grain structure. We believe that our microstructure control strategy could be applicable to magnesium alloys which exhibit obvious precipitation strengthening potential.
In this study, the influence of rotary-die equal channel angular pressing (RD-ECAP) processing on the mechanical properties and rolling formability of AZ91 alloys was investigated. The as-cast and pre-homogenized AZ91 alloys were pre-processed by RD-ECAP for 16 passes at 573 K and subjected to post-ECAP rolling at 573 K with a rolling speed of 10 m/min. The microstructure and deformation characteristics of the AZ91 alloys were characterized. Results demonstrated that fine-grained AZ91 alloys with improved strength and ductility were obtained via the high-pass RD-ECAP processing, indicating a good plastic formability. The ECAP-ed alloys were easily rolled at 573 K from 4.5 mm to 1.1 mm in thickness without edge cracking. After rolling, heterogeneous grain structures were observed with large numbers of twins and shear bands that created strong basal textures. The rolled AZ91 alloys exhibited higher tensile strength and appropriate elongation. The post-ECAP rolling was successfully used in the high productivity of AZ91 rolled plates with good mechanical properties.
Pure titanium was efficiently processed up to four passes at 420 °C by rotary-die equal-channel angular pressing (RD-ECAP). The deformation structure and mechanical properties of pure titanium with various RD-ECAP passes were subsequently investigated. Microstructure evolution revealed that plastic deformation was accommodated mainly by twins during the first and second passes, while the predominant deformation mechanism was dislocation slip during the third and fourth passes. { } twins were detected in the first pass, and { } twins occurred in the second pass of RD-ECAP. The ultimate tensile strength of pure titanium increased from 450 MPa in the as-received state to 627 MPa with a fracture elongation of 29% after four passes of RD-ECAP.
Mechanical properties usually take precedence for wrought magnesium alloy when it would be used as a structure material. This paper proposed an approach that achieved high strength in AZ91 Mg alloy. The main procedure combined solution heat treatment, equal channel angular pressing (ECAP), and the subsequent low temperature rolling. After solution heat treatment and ECAP, the alloy had fine grains and excellent ductility, which benefited the following rolling at low temperature. By the following rolling (at 150 °C), the strength was further increased to ~432 MPa with a moderate ductility. This approach was proved effective in refining the grains and accumulating dislocations. The ultrahigh strength was attributed to the high density of dislocations and fine structure. The uniformly distributed fine precipitates also supplied precipitate hardening. Recrystallization that happened during rolling and annealing was the main reason for the moderate ductility.
This paper investigated the cooperative effects of Li addition and warm Equal Channel Angular Pressing (ECAP) on improving the mechanical properties of an Al-Mg-Li alloy for further weight reduction. The results showed that more Li addition could obviously refine the grains of the as-cast alloy and reduce its density value to only 2.37 g/cm3 when Li content reached 2.5% (about 12.6% lighter than commercial Al alloys). It also had a pronounced influence on the precipitations in the Al-5.5Mg-xLi-0.1Zr alloy, i.e., the number density and size of Al2MgLi and δ’-Al3Li phases. The yield strength of the as-cast alloy was increased with increasing Li, but the elongation deteriorated due to primary network intergranular Al2MgLi and more δ’ particles in the high Li-containing alloy. The warm multi-pass ECAP process was found to simultaneously improve the strength and ductility of the Al-Mg-Li alloys, and greatly alleviate the detrimental effect of Li addition on the elongation, thereby making the ultrafine-grained (UFG) alloys, a good combination of lightweight and high performance, very attractive for aerospace applications for much higher specific strength than both Al matrix composites and Mg alloys.