The medical applications of degradable iron-based biomaterials have been targeted by re-searchers due to their special properties that they present after alloying with various elements and different technological methods of obtaining. Compared to other biodegradable materials, iron-based alloys are designed especially for the low production costs, the non-magnetism obtained by alloying with Mn, and the shape memory effect (SME) following the alloying with Si, which is necessary in medical applications for which it could replace nitinol successfully. Alloying with new elements could improve the mechanical properties, the degradation rate, and the transformation temperatures corresponding to the SME. This paper presents the results from the study of FeMnSi-Al alloy as a biodegradable material. The X-ray diffraction (XRD) method was used to identify the phases formed in the experimental Fe-Mn-Si-Al alloy, and the SME was studied by differential scanning calorimetry (DSC). In vitro tests were performed by immersing the samples in Ringer’s biological solution for different time intervals (1, 3, and 7 days). The chemical composition of the samples, as well as the compounds resulting from the immersion tests, were evaluated by energy dispersive X-ray (EDS). Scanning electron microscopy (SEM) was used for the microstructural analysis and for highlighting the surfaces subjected to contact with the electrolyte solution. The corrosion rate (CR, mm/yr.) was calculated after mass loss, sample surface area, and immersion time (h) (at 37 °C). Samples were subjected to electro-corrosion tests using electrochemical impedance spectroscopy (EIS) and Tafel linear and cyclic potentiometry.
An usual material, EN-GJL-250 cast iron, used for automotive braking systems, was covered with a ceramic material (105NS-1 aluminium oxide) using an industrial deposition system (Sulzer Metco). The main reason was to improve the corrosion and wear (friction) resistance properties of the cast-iron. Samples were prepared by mechanical grinding and sandblasting before the deposition. We applied two and four passes (around 12–15 µm by layer) each at 90° obtaining ceramic coatings of 30 respectively 60 µm. The surface of the samples (with ceramic coatings) was investigated using scanning electron microscopy (SEM), dispersive energy spectroscopy (EDS) and X-ray diffraction (XRD). Scratch and micro-hardness tests were performed using CETR-UMT-2 micro-tribometer equipment. The better corrosion resistance of the base material was obtained by applying the ceramic coating. The results present a better corrosion resistance and a higher coefficient of friction of the coated samples.
Finite element analysis studies have been of interest in the field of orthodontics and this is due to the ability to study the stress in the bone, periodontal ligament (PDL), teeth and the displacement in the bone by using this method. Our study aimed to present a method that determines the effect of applying orthodontic forces in bodily direction on a healthy and reduced periodontium and to demonstrate the utility of finite element analysis. Using the cone-beam computed tomography (CBCT) of a patient with a healthy and reduced periodontium, we modeled the geometric construction of the contour of the elements necessary for the study. Afterwards, we applied a force of 1 N and a force of 0.8 N in order to achieve bodily movement and to analyze the stress in the bone, in the periodontal ligament and the absolute displacement. The analysis of the applied forces showed that a minimal ligament thickness is correlated with the highest value of the maximum stress in the PDL and a decreased displacement. This confirms the results obtained in previous clinical practice, confirming the validity of the simulation. During orthodontic tooth movement, the morphology of the teeth and of the periodontium should be taken into account. The effect of orthodontic forces on a particular anatomy could be studied using FEA, a method that provides real data. This is necessary for proper treatment planning and its particularization depends on the patient’s particular situation.
The high yttria content of a stabilized zirconia (YSZ) (38 wt% Y2O3) coating was deposited by atmospheric plasma spraying (APS) from Metco 207 powders on an Inconel 718 (Ni-based superalloy) substrate. As a metal coating connection, a layer of cermet powder (Ni-20% Al—410NS) was used before the ceramic layer deposition. The electro-chemical corrosion resistance of these materials was tested using Inconel cylinders with a diameter of 10 mm and a thickness of 1 mm, with and without the ceramic layer. Linear and cyclic measurements were obtained in H2SO4 electrolyte media at pH = 2. Electro-impedance spectroscopy (EIS) experiments were performed on the sample covered with the ceramic layer to evaluate the interface behavior. Scanning electron microscopy (SEM), along with equipment to determine chemical composition, and an energy dispersive spectrometry (EDS) detector were used to characterize the material surface before and after corrosion tests. It was observed that the corrosion resistance of Inconel was influenced by the bonding layer and the ceramic coating.
Biodegradable metallic materials are gaining attention for medical applications in short-term implants (15–500 days) because of their good mechanical properties, biocompatibility, and generalized corrosion. Most medical applications involve implant wear processes, particularly for bone fractures. Parallelepipedic specimens (dimensions 50 mm × 10 mm × 3 mm) were obtained by cutting the hot-rolled material processed from cast ingots of ZnMgY. To test the tribological performance of these stationary specimens, they were placed at the upper point of the machine’s tribological contact. The rotating lower disk of the AMSLER machine (AMSLER & Co., Schaffhouse, Switzerland) is manufactured from AISI 52100 bearing steel with a 62–65 HRC hardness and a diameter of 59 mm both radially and axially. Frictional torque is the parameter that is measured. Scanning Electron Microscopy (SEM) and Energy Dispersive Spectroscopy (EDS) were used to analyze the worn areas. The material behavior in the normal and wear states upon immersion in simulated body fluid (SBF) was evaluated.
The rotors of submersible wastewater pumps, generally made of nodular graphite cast iron, are subjected to complex processes of corrosive erosion during operation. To improve the characteristics of erosion resistance by impact with solid particles in the corrosive environment of wastewater, cast iron was subjected to a chemical phosphating treatment. In the paper, the scratch test behaviour of nodular cast iron and phosphate nodular cast iron is analysed comparatively, studying the behaviour of the deposited layer and its adhesion to the substrate. The nanoindentation characteristics of nodular cast iron and phosphate nodular cast iron were also studied. It was observed that the deposited layer is not compact, but when pressed, it does not crack and does not detach from the substrate; it is impregnated in the substrate in the metal matrix, but not on the area with carbon nodules. The SEM micrographs show that the deposited phosphate layer is relatively porous and can change the behaviour of the liquid flow moving on the surface of the rotor due to its hydrophilic behaviour; this also allows the formation of a boundary layer that adheres to the surface of the rotor and protects it from the impacts of microparticles driven by the liquid stream.