Synthesis of SnO2–Fe3O4 nanocomposites was conducted. The purpose of this study was to obtain the SnO2–Fe3O4 nanocomposites, the effectiveness of photodegradation Congo red by SnO2–Fe3O4 nanocomposites and determine the kinetics of photodegradation. The XRD analysis showed that the SnO2–Fe3O4 nanocomposite best mass ratio was 1:1 based on the highest intensity of characteristic angle (2θ), which is 26.54° and had the smallest crystal size, which is 9.662 nm. Based on the UV-Vis DRS result, the SnO2–Fe3O4 nanocomposites bandgap value was 2.3 eV. The magnetization saturation value of SnO2–Fe3O4 nanocomposites was 64.96 emu/g. The morphology of SnO2–Fe3O4 nanocomposites showed by the TEM image, where the dark spots spread in the lighter areas. The surface of SnO2–Fe3O4 nanocomposites characterized by SEM with the result was bumpy surface and many pores. The EDS result of SnO2–Fe3O4 nanocomposites confirmed the presence of Fe, Sn, and O elements. The functional group of SnO2–Fe3O4 nanocomposites showed by FTIR data, the stretch band of Sn–O characteristics showed at wavenumber 590 cm−1, and the stretch band of Fe–O showed at wavenumber 563 cm−1. The optimum condition of nanocomposites at a contact time of 90 min and the optimum concentration of 18 mg/L showed that the percent of photodegradation was 50.76%. The photodegradation rate of SnO2–Fe3O4 was fitted to Pseudo-second-order.
22 May 2021 in Bulletin of Chemical Reaction Engineering & Catalysis
In this study, molybdenum nitride-bentonite was successfully employed for the reaction of hydrocracking of palm oil to produce a bio-gasoline and bio-aviation fuel. The prepared catalyst was characterized using XRD, FT-IR, and SEM-EDX. The acidity of the catalyst was determined using the pyridine gravimetric method. The result showed that the acidity of bentonite was increased after modification using molybdenum nitride. The hydrocracking study showed that the highest conversion and product fraction of bio-gasoline and bio-aviation fuel were exhibited by molybdenum nitride-bentonite 8 mEq g−1. The catalyst was later used to optimize the hydrocracking process using RSM-CCD. The effects of the process variables such as temperature, contact time, and catalyst to feed ratio, on the response variables, such as conversion, oil, gas, and coke yield, were investigated. The analysis of variance showed that the proposed quadratic model was statistically significant with adequate precision to estimate the responses. The optimum conditions in the hydrocracking process were achieved at a temperature of 731.94 K, contact time of 0.12 h, and a catalyst to feed ratio of 0.12 w/v with a conversion of 78.33%, an oil yield of 50.32%, gas yield of 44.00% and coke yield of 5.73%. The RSM-CCD was demonstrated as a suitable method for estimating the hydrocracking process of palm oil using a MoN-bentonite catalyst due to its closeness to the optimal value of the expected yield. This study provided a potential catalyst of based on bentonite modified using molybdenum nitride for the hydrocracking of palm oil.
1 January 2022 in Journal of Ecological Engineering
This study successfully synthesized a core-shell-shell in the form of CoFe2O4-SiO2-TiO2 catalyst magnetic and recyclable. The catalyst for the photocatalytic degradation of methyl orange (MO) dye. Subsequently, the catalyst was subjected to XRD, FTIR, SEM-EDS, VSM, as well as UV-DRS...
The adsorption of POME using natural clay, montmorillonite, has been investigated. The reductions of three important parameters (chemical oxygen demand, total suspended solids and colour) in various influencing factors have been determined. The optimum conditions for mixing speed of the stirrer, contact time, dosage of adsorbent, concentration of palm oil mill effluent (POME) and pH were 300 rpm, 90 min, 5 g/L, 25% POME and pH 7, respectively. The removal reached more than 95% for all parameters. The experimental data were found to fit with the Langmuir adsorption isotherm model. The intraparticle diffusion model controlled the adsorption process and, therefore, the diffusion of the solute into the inside pores of the adsorbent took places permanently (irreversible) because the particles were trapped inside the pores. This situation causes the adsorbent capacity to decrease and it cannot be used continuously prior to the regeneration or activation, both chemically and thermally.