Zining Yang

Mr. Zining Yang

East China University of Science and Technology, Shanghai, China

Research Focus & Metrics

Academic Career Length

6Years (2021-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
31 October 2023 in Coatings
Verified
Journal Article
Open access
PDF file
HLHongchen Li
Hongchen Li
WWWeize WANG
Weize WANG
ZYZining Yang
Zining Yang
YLYangguang Liu
Yangguang Liu
YWYihao Wang
Yihao Wang
WLWei Liu
Wei Liu
Thermal barrier coatings (TBCs) play a crucial role in enhancing the operating temperature of key equipment. However, when TBCs are sprayed on the internal surface of these components, there are issues related to the imperfect internal diameter atmospheric plasma spray (ID-APS) process and the unsatisfactory performance of TBCs in internal holes. Yttria-stabilized zirconia (YSZ), YSZ + Gadolinium zirconate (GZ) and YSZ + tantalate (RETaO4) TBCs were prepared using the SM F210 ID-APS gun. The thermal shock and particle erosion resistance of the coatings were compared, and the relationship between the structure and properties was investigated. The results show that the hardness, fracture toughness and erosion resistance of the three coatings are the largest in the YSZ coating and the smallest in the GZ coating. YSZ coating also has the best thermal shock resistance. These research findings have important guiding significance for the improvement of the ID-APS process.

30 November 2021 in Coatings
Verified
Journal Article
Open access
PDF file
ZYZining Yang
Zining Yang
WWWeize WANG
Weize WANG
SDShujuan Deng
Shujuan Deng
HFHuanjie Fang
Huanjie Fang
TYTing Yang
Ting Yang
TYTing Yang
Ting Yang
Gadolinium zirconate with excellent high-temperature phase stability and sintering resistance has become a very promising candidate material for a new generation of thermal barrier coatings (TBCs). However, the low fracture toughness of gadolinium zirconate greatly limits its application. In this study, gadolinium zirconate (GZ) and two kinds of toughened gadolinium zirconate (GZ/YSZ prepared by mixed powder of Gd2Zr2O7 and YSZ and GSZC prepared by (Gd0.925Sc0.075)2(Zr0.7Ce0.3)2O7 powder) double-layered TBCs were prepared by atmospheric plasma spraying (APS). The fracture toughness of the GZ/YSZ coating and GSZC coating were 9 times and 3.5 times that of GZ coating, respectively. The results of thermal shock test showed that the three TBCs exhibit different failure mechanisms. During the thermal shock test, cracking occurred at the interfaces between the YSZ layer and the BC or GZ/YSZ layer, while GSZC TBC failed due to premature cracking inside the GSZC layer. The particle erosion rate of the GZ, GZ/YSZ, and GZSC coatings were 1.81, 0.48, and 1.01 mg/g, respectively, indicating that the erosion resistance of coatings is related to their fracture toughness. Furthermore, the superior erosion resistance of the GZ/YSZ and GSZC coatings can be attributed to the conversion of crack propagation path during the erosion test.

9 June 2022 in Coatings
Verified
Journal Article
Open access
PDF file
ZYZining Yang
Zining Yang
KYKai Yang
Kai Yang
WWWeize WANG
Weize WANG
TYTing Yang
Ting Yang
HFHuanjie Fang
Huanjie Fang
CZChengcheng Zhang
Chengcheng Zhang
Gadolinium zirconate (GZ) has become a promising thermal barrier coating (TBC) candidate material for high-temperature applications because of its excellent high-temperature phase stability and low thermal conductivity compared to yttria-stabilized zirconia (YSZ). The double-ceramic-layered (DCL) coating comprised of GZ and YSZ was confirmed to possess better durability. However, the particle-erosion resistance of GZ is poor due to its low fracture toughness. In this study, a novel erosion-resistant layer, an Al2O3-GdAlO3 (AGAP) amorphous layer, was deposited as the top layer to resist erosion. Three triple-ceramic-layer (TCL) coatings comprised of an Al2O3-GAP layer as the top layer, a GZ layer, a GZ/YSZ composite layer, and a rare-earth-doped gadolinium zirconate (GSZC) layer as the intermediate layer, and a YSZ layer as the base layer. For comparison, an AGAP-YSZ DCL coating without a middle layer was prepared as well. Under the erosion speed of 200 m/s, only a small amount of spallation occurred on the surface of the Al2O3-GAP layer, indicating a superior particle-erosion resistance. In the thermal shock test, the Al2O3-GAP layer experienced glass transition and the glass transition temperature was close to 1500 °C. The hardness of the Al2O3-GAP coating after glass transition increased ~170% compared to the as-sprayed Al2O3-GAP coating. Moreover, The DCL TBC and TCL TBCs exhibited different failure mechanisms, which illustrated the necessity of the middle layer. The finite element model (FEM) simulation also shows that the introduction of the GZ layer can obviously reduce the thermal stress at the TC/BC interface. In terms of coating with a modified GZ layer, the AGAP-GZ/YSZ-YSZ coating and AGAP-GSZC-YSZ coating showed a similar failure model to the AGAP-GZ-YSZ coating, and the AGAP-GSZC-YSZ coating exhibited better thermal shock resistance.