Increasing the initial –OH group density on SiO2 surfaces improves dimethylamino-trimethylsilane passivation and increases selectivity for area-selective deposition.
The fabrication of superconducting circuits requires multiple deposition, etching, and cleaning steps, each possibly introducing material property changes and microscopic defects. In this work, we specifically investigate the process of argon milling, a potentially coherence-limiting step, using niobium and aluminum superconducting resonators as a proxy for the surface-limited behavior of qubits. We find that niobium microwave resonators exhibit an order of magnitude decrease in quality factors after surface argon milling, while aluminum resonators are resilient to the same process. Extensive analysis of the niobium surface shows no change in the suboxide composition due to argon milling, while two-tone spectroscopy measurements reveal an increase in two-level system electrical dipole moments, indicating a structurally altered niobium oxide. However, a short dry etch can fully recover the argon-milling-induced losses on niobium, offering a potential route towards state-of-the-art overlap Josephson junction qubits with niobium circuitry.
Monolayer-Si-passivated Ge nFETs with high electron mobility (175 cm 2 /Vs at Ns=5×10 12 cm -2 ) and superior PBTI reliability (max. V ov = |V g -V th | of 0.28V at 125°C) at 0.95-nm-EOT are demonstrated on a 300 mm Si wafer platform. The electron mobility is increased by optimizing the Si thickness while significant improvement in PBTI reliability is realized by band engineering using La-induced interface dipole and defect passivation using laser annealing. This is a significant step forward for the introduction of Ge nFET as high mobility device in advanced technology nodes.
A key factor enabling the reduction of the thermal budget in W2W bonding integration flows is the activation sequence, consisting of cleaning and plasma treatment, used before bonding. For hybrid bonding such activation sequence needs to be selected to fulfill multiple functions: activation of the dielectric bonding surface to obtain a high bonding energy during room temperature bonding, minimize the dielectric bonding annealing temperature while avoiding exposed Cu oxidation and reducing the required annealing temperature for proper Cu-to-Cu bonding. In this paper we discuss the effect of different wafer clean methods (Deionized (DI) water and citric acid) and the effect of different plasma treatments on SiCN and Cu surfaces before bonding. The characterization techniques used include XPS, TEM, ellipsometry, SAM, OES and wafer-to-wafer bond strength testing. It is observed that Nitrogen plasma treatment can help in reducing the CuOx and a mild passivation effect of the surface is observed. Whereas on the Cu pads citric acid, used just before bonding, appears a good option, since clear effectiveness in reducing the CuOx is observed, on the dielectric it may leave some residues which can result sometimes in bonding defects. Moreover, a metric to evaluate efficient SiCN-SiCN bonding is proposed and further understanding of the physical mechanisms involved in SiCN-SiCN bonding are suggested.
The thermal stability of thin films in contact with or during annealing up to has been studied. It is found that stacks react during annealing and a phase separation into polycrystalline Sc-rich (and relatively Si-poor) DySc silicate on top of an amorphous Dy-rich DySc silicate is observed. In contrast, is found to be thermodynamically stable in contact with and to recrystallize upon annealing. These results demonstrate that the previously reported high crystallization temperature of for is not an intrinsic material property but caused by silicate formation.