In this work, the mechanism of the corrosion behavior of laser‐treated aluminum is studied. Two different laser techniques are used to fabricate the samples, direct laser interference patterning (DLIP) and direct laser writing (DLW), using nanosecond laser sources. The DLIP treatment uses a two‐beam optical configuration producing line‐like periodic structures. The DLW technique is employed to produce non‐periodic structures on the Al‐surface with the same cumulated fluences as in DLIP. The surface topography is analyzed by confocal microscopy, and the formation of oxide layers is investigated by scanning electron microscopy of cross‐sections produced using a focused ion beam. Wetting measurements performed on the laser‐treated samples exhibit a contrasting behavior, leading to either superhydrophobic or superhydrophilic states. In the case of the DLIP treatment, the static water contact angle is increased from 81° up to 158°, while for DLW, it decreases to 3°. Electrochemical tests demonstrate a decreased corrosion rate after laser treatment. Additionally, findings indicate no correlation between wettability and corrosion reduction. Therefore, the improvement in corrosion resistance is mainly attributed to the oxide layer formed by laser treatment. Although similar corrosion rates are achieved for both treatments, surfaces produced with DLIP can be beneficial when additional surface properties are required.
25 June 2025 in International Journal of Hydrogen Energy
Corrosion of aluminum alloys poses a significant challenge in the transportation and aerospace industries, where material degradation can lead to structural failure and increased maintenance costs. Yet, the corrosion performance of laser‐structured metallic surfaces exhibiting extreme wetting states under industrially relevant conditions remains largely unexplored. In this work, we investigate the competing roles of superhydrophobicity and superhydrophilicity in governing the corrosion behavior of laser‐textured AA2024‐T351 under salt‐spray conditions. Three different laser approaches were employed: direct laser interference patterning (DLIP), direct laser writing (DLW), and a modified version of DLW (DLWM). DLIP and DLWM generated line‐like periodic microstructures with spatial periods of 6 and 20 µm, respectively, both yielding saline contact angles (SCA) of 156 ± 1° and 151 ± 2°. In contrast, DLW produced a randomly textured superhydrophilic surface (SCA ≈0°). Regarding corrosion performance, the DLIP‐treated samples exhibited the highest resistance, with 95% reduction in pit density after 72 h of salt‐spray exposure relative to the reference surface. The superhydrophilic surfaces promoted the formation of larger pits due to longer electrolyte residence times, whereas superhydrophobicity confined corrosion to the microstructure. These findings highlight laser structuring as a versatile strategy for controlling wettability and extending corrosion lifetime under realistic conditions.
Air pollution, acid precipitation, ozone depletion and the gaseous emissions to the atmosphere are associated to the petroleum derivate use, currently considered the main energy source used in the world. Renewable energy sources are expected to replace them in order to solve these environmental concerns. Biofuels as biodiesel and biogas are renewable energy produced from natural matter. Studies made suggest that using the principal by-product of biodiesel’s production process, crude glycerol, is possible to obtain biogas. Biogas can be produced from an anaerobic digestion process and enhanced by using pretreatment in substrate. This work tested ultrasound pretreatment on crude glycerol as a substrate in the biogas production. Different times of pretreatment (15 and 30 minutes) were examined, to determinate the best performance and compare it to the untreated substrate. The biogas production was daily measured directly from the reactors. The results showed that ultrasound pretreatment improved methane production. The best result was obtained by using 30 minutes of pretreatment on crude glycerol.