Rotary friction welding is one of the most crucial techniques for joining different parts in advanced industries. Experimentally measuring the history of thermomechanical and microstructural parameters of this process can be a significant challenge and incurs high costs. To address these challenges, the finite element method was used to simulate thermomechanical and microstructural aspects of the welding of identical superalloy Inconel 718 tubes. Numerical simulation results were used to compute essential mechanical and metallurgical parameters such as temperature, strain, strain rate, volume fraction of dynamic recrystallization, and grain size distribution. These parameters were subsequently verified using experimental test results. The Johnson–Avrami model was utilized in the microstructural simulation to convert thermomechanical parameters into metallurgical factors, employing a FORTRAN subroutine. The calculated thickness of the recrystallization zone in the wall was 480 and 850 μm at the tube wall’s center and edge, respectively. These values were reported from experimental measurements as 500 and 800 μm, respectively. The predicted grain size changes from the center to the edge of the wall thickness, near the weld interface, ranged from 2.07 to 2.15 μm, comparable to the experimental measurements ranging from 1.9 to 2.2 μm. Various curves are also presented to explore the correlation between thermomechanical and microstructural parameters, with the experimental results revealing predictable microstructure evolutions correlated with thermomechanical changes.
The thermo-mechanical behavior of nanosized Al2O3 particles reinforcing aluminum was analyzed in the present paper. The material was prepared by spark plasma sintering and friction stir welding. The thermal stresses affecting the composite behavior during welding were modeled through COMSOL MultiPhysics, and the results were validated by the analyses of the composites’ mechanical properties. The spark-plasma-sintered materials presented limited porosity, which was taken into account during the modeling phase. Both model and experiments revealed that higher heat input is related to better material mixing during welding and sound mechanical properties. Thermal stresses lead to residual stresses close to 300 MPa in the thermo-mechanically affected zone for processing conditions of 1900 RPM and 37 mm/min. This leads to an increase in hardness up to 72 HV.