Graphene oxide (GO) incorporation in natural fiber composites has recently defined a novel class of materials with enhanced properties for applications, including ballistic armors. In the present work, the performance of a 0.5 vol % GO-incorporated epoxy matrix composite reinforced with 30 vol % fabric made of ramie fibers was investigated by stand-alone ballistic tests against the threat of a 0.22 lead projectile. Composite characterization was also performed by Fourier-transform infrared spectroscopy, thermal analysis and X-ray diffraction. Ballistic tests disclosed an absorbed energy of 130 J, which is higher than those reported for other natural fabrics epoxy composite, 74–97 J, as well as plain Kevlar (synthetic aramid fabric), 100 J, with the same thickness. This is attributed to the improved adhesion between the ramie fabric and the composite matrix due to the GO—incorporated epoxy. The onset of thermal degradation above 300 °C indicates a relatively higher working temperature as compared to common natural fiber polymer composites. DSC peaks show a low amount of heat absorbed or release due to glass transition endothermic (113–121 °C) and volatile release exothermic (~132 °C) events. The 1030 cm−1 prominent FTIR band, associated with GO bands between epoxy chains and graphene oxide groups, suggested an effective distribution of GO throughout the composite matrix. As expected, XRD of the 30 vol % ramie fabric-reinforced GO-incorporated epoxy matrix composite confirmed the displacement of the (0 0 1) peak of GO by 8° due to intercalation of epoxy chains into the spacing between GO layers. By improving the adhesion to the ramie fabric and enhancing the thermal stability of the epoxy matrix, as well as by superior absorption energy from projectile penetration, the GO may contribute to the composite effective ballistic performance.
The horse hoof wall exhibits exceptional impact resistance and fracture control due to its unique hierarchical structure which contains tubular, lamellar, and gradient configurations. In this study, structural characterization of the hoof wall was performed revealing features previously unknown. Prominent among them are tubule bridges, which are imaged and quantified. The hydration-dependent viscoelasticity of the hoof wall is described by a simplified Maxwell-Weichert model with two characteristic relaxation times corresponding to nanoscale and mesoscale features. Creep and relaxation tests reveal that the specific hydration gradient in the hoof keratin likely leads to reduced internal stresses that arise from spatial stiffness variations. To better understand realistic impact modes for the hoof wall in-vivo, drop tower tests were executed on hoof wall samples. Fractography revealed that the hoof wall's reinforced tubular structure dominates at lower impact energies while the intertubular lamellae are dominant at higher impact energies. Broken fibers were observed on the surface of the tubules after failure, suggesting that the physically intertwined nature of the tubule reinforcement and intertubular matrix improves the toughness of this natural fiber reinforced composite. The augmented understanding of the structure-mechanical property relationship in dynamic loading led to the design of additively manufactured bioinspired structures, which were evaluated in quasistatic and dynamic loadings. The inclusion of gradient structures and lamellae significantly reduced the damage sustained in drop tower tests, while tubules increased the energy absorption of samples tested in compact tension. The samples most similar to the hoof wall displayed remarkably consistent fracture control properties.
The coating of natural fiber by graphene oxide (GO) has, over, this past decade, attracted increasing attention as an effective way to improve the adhesion to polymer matrices and enhance the composite properties. In particular, the GO-functionalized 30 vol% curaua fiber (Ananas Erectifolius) reinforcing epoxy composite was found to display superior tensile and thermogravimetric properties as well as higher fiber/matrix interfacial shear strength. In this brief report, dynamic mechanical analysis (DMA) was conducted in up to 50 vol% GO-functionalized curaua fiber reinforced epoxy matrix (EM) composites. The objective was not only to extend the amount incorporated but also for the first time investigate the composite viscoelastic behavior. The GO functionalization of curaua fibers (GOCF) improved the DMA storage (E′) and loss (E″) modulus compared to the non-functionalized fiber composites. Values at 30 °C of both E′ (13.44 GPa) and E″ (0.67 GPa) for 50 vol% GO-functionalized curaua fiber reinforced epoxy matrix composites (50GOCF/EM) were substantially higher than those of 20 GOCF/EM with E′ (7.08 GPa) and E″ (0.22 GPa) as well as non-functionalized 50CF/EM with E′ (11.04 GPa) and E″ (0.45 GPa). All these results are above the neat epoxy previously reported values of E′ (3.86 GPa) and E″ (0.09 GPa). As for the tangent delta, the parameters associated with damping factor and glass transition temperature were not found to be significantly changed by GO functionalization, but decreased with respect to the neat epoxy due to chain mobility restriction.
Fiber-reinforced composites are among the most investigated and industrially applied materials. Many studies on these composites using fibers, especially with natural fibers, were made in response to an urgent action for ambient preservation. A particularly relevant situation exists nowadays in the area of materials durability. In this respect, no studies on water-immersion-accelerated aging in fique fiber–epoxy composites are reported. This work aimed to fill this gap by investigating the epoxy matrix composites reinforced with 40 vol% fique fabric. The epoxy matrix and the composite, both unaged and aged, were characterized by weight variation, water absorption, morphology, colorimetry (CIELAB method), Fourier transform infrared spectroscopy (FTIR) and dynamic–mechanical analysis (DMA). The main results were that degradation by water presents appearance of complex microfibril structures, plasticization of epoxy resin, and debonding of the fique fiber/epoxy matrix. The most intense color change was obtained for the water-immersion-aged epoxy by 1440 h. Cole–Cole diagrams revealed the heterogeneity of the materials studied.