Friction Stir Welding (FSW) is a feasible welding process to join dissimilar materials due to its solid-state nature. In this study the FSW of 6061-T6 aluminum with pure Cu plates was performed with the objective of evaluating the effects of the FSW parameters on the microstructure and electrical properties. The processing parameters (rotational and traverse speeds) were established to reduce the common defects in the friction-stir welding process. Therefore, the obtained results validated the better mechanical properties and a smaller increase of the electrical resistivity. The rotational speeds used were of 1000, 1150, and 1300 rpm, and the traverse speeds of 20, 40, and 60 mm/min, with the purpose of varying the heat input of the process. The microstructural characterization revealed the presence of a mixture of aluminum and copper into the weld zone, along with copper particles and the formation of intermetallic compounds. It was found that the electrical resistivity of the joints ranged from 0.029 to 0.036 μΩ. The highest electrical resistivity values were obtained at the lowest traverse speed (20 mm/min) and the lowest resistivity values were obtained at highest traverse speed (60 mm/min).
Friction stir welding is characterized as an ecological and low-cost process in comparison to traditional welding techniques, and due to its application in the solid state, it is a feasible option for joining similar and/or dissimilar materials. The present investigation seeks to determine the effect of friction stir welding’s parameters on the corrosion resistance of an Al 6061-T6–Cu C11000 dissimilar joint, with mathematical analysis to validate the results. After the welding process, the samples were exposed to a NaCl solution in an electrochemical cell to determine the corrosion rate via potentiodynamic tests. Microstructural characterization revealed a laminar structure, composed of aluminum and copper, as well as copper particles and the formation of intermetallic compounds distributed in the weld zone. The potentiodynamic tests showed that the corrosion rate increased with the rotational and traverse speeds. The mathematical model quantifies the relationship between corrosion rate and rotational and traverse speeds.
Molten steel is alloyed during tapping from the melting furnace to the argon-bottom stirred ladle. The metallic additions thrown to the ladle during the ladle filling time are at room temperature. The melting rates or kinetics of sinking-metals, like nickel, are simulated through a multiphase Euler–Lagrangian mathematical model during this operation. The melting rate of a metallic particle depends on its trajectory within regions of the melt with high or low turbulence levels, delaying or speeding up their melting process. At low steel levels in the ladle, the melting rates are higher on the opposite side of the plume zone induced by the bottom gas stirring. This effect is due to its deviation after the impact of the impinging jet on the ladle bottom. The higher melting kinetics are located on both sides at high steel levels due to the more extensive recirculation flows formed in taller baths. Making the additions above the eye of the argon plume spout increases the melting rate of nickel particles. The increase of the superheat makes the heat flux more significant from the melt to the particle, increasing its melting rate. At higher superheats, the melting kinetics become less dependent on the fluid dynamics of the melt.
This research evaluates the effect of temperature and time austempering on microstructural characteristics and hardness of ductile iron, validating the results by means of a statistical method for hardness prediction. Ductile iron was subjected to austenitization at 950 °C for 120 min and then to austempering heat treatment in a salt bath at temperatures of 290, 320, 350 and 380 °C for 30, 60, 90 and 120 min. By increasing austempering temperature, a higher content of carbon-rich austenite was obtained, and the morphology of the thin acicular ferrite needles produced at 290 °C turned completely feathery at 350 and 380 °C. A thickening of acicular ferrite needles was also observed as austempering time increased. An inversely proportional behavior of hardness values was thus obtained, which was validated through data analysis, statistical tools and a regression model taking temperature and time austempering as input variables and hardness as the output variable, which achieved a correlation among variables of about 97%. The proposal of a mathematical model for the prediction of hardness in austempered ductile iron represents a numerical approximation which validates the experimental results at 95.20%.
In this research, the effect of the interelectrode distance (d) in the electrocoagulation (EC) reactor was studied. The experiments were carried out with varying d in values of 3, 5, and 9 mm during the treatment of water contaminated with fluoride (F−). The response variables analyzed were the treatment time necessary to reduce the residual concentration of F− to 1.5 mg L−1, the number of aluminum hydroxides formed, the potential drop in the reactor terminals, and the electric power consumption of the reactor. The software FLUENT version 6.3 was employed to simulate the liquid velocity profiles achieved in the reactor chamber. The results obtained show that the liquid velocity increases in the interelectrode spaces to 0.48, 0.65, and 0.86 m s−1 for interelectrode distances of 9, 5, and 3 mm, respectively, which favors not only the formation of flocs but also the elimination of fluoride. With a shorter interelectrode distance, the EC reactor not only consumes less electrical energy but also fewer electrodes, and the dispersion of generated flocs in the reactor chamber is major, which is more important than the quantity of flocs generated in it.
The characterization of the fluid flow of liquid steel in a slab mold, using two nozzle designs under unclogged and clogged conditions, is performed using physical and mathematical simulations. Nozzle A, with an expanding and contracting geometry, yields larger sub-meniscus experimental velocities than nozzle B, with internal flow deflectors. The numerical predictions indicate quick time-changing velocity profiles in the submeniscus region between the mold’s narrow face and the nozzles. The flow deflectors in nozzle B have two effects; the high dissipation rate of kinetic energy in the upper-half length induces lower velocities in the ports than nozzle A. The neutralization of the biased flow caused by the sliding gate allows a balanced fluid through the ports. According to the results, nozzle A yields velocity profiles in the sub-meniscus region with larger standard deviations than nozzle B, leading to an unstable bath surface. The clogged nozzles produced biased-asymmetrical flow patterns in the mold, finding approximated matchings between numerical predictions and experimental measurements. The internal protrusions of the deposits lead to covariance losses of the bath surface wave heights. The use of internal deflectors helped to decrease the amount of clog material in nozzle B.