Friction Stir Welding (FSW) is a feasible welding process to join dissimilar materials due to its solid-state nature. In this study the FSW of 6061-T6 aluminum with pure Cu plates was performed with the objective of evaluating the effects of the FSW parameters on the microstructure and electrical properties. The processing parameters (rotational and traverse speeds) were established to reduce the common defects in the friction-stir welding process. Therefore, the obtained results validated the better mechanical properties and a smaller increase of the electrical resistivity. The rotational speeds used were of 1000, 1150, and 1300 rpm, and the traverse speeds of 20, 40, and 60 mm/min, with the purpose of varying the heat input of the process. The microstructural characterization revealed the presence of a mixture of aluminum and copper into the weld zone, along with copper particles and the formation of intermetallic compounds. It was found that the electrical resistivity of the joints ranged from 0.029 to 0.036 μΩ. The highest electrical resistivity values were obtained at the lowest traverse speed (20 mm/min) and the lowest resistivity values were obtained at highest traverse speed (60 mm/min).
Friction stir welding is characterized as an ecological and low-cost process in comparison to traditional welding techniques, and due to its application in the solid state, it is a feasible option for joining similar and/or dissimilar materials. The present investigation seeks to determine the effect of friction stir welding’s parameters on the corrosion resistance of an Al 6061-T6–Cu C11000 dissimilar joint, with mathematical analysis to validate the results. After the welding process, the samples were exposed to a NaCl solution in an electrochemical cell to determine the corrosion rate via potentiodynamic tests. Microstructural characterization revealed a laminar structure, composed of aluminum and copper, as well as copper particles and the formation of intermetallic compounds distributed in the weld zone. The potentiodynamic tests showed that the corrosion rate increased with the rotational and traverse speeds. The mathematical model quantifies the relationship between corrosion rate and rotational and traverse speeds.
This research evaluates the effect of temperature and time austempering on microstructural characteristics and hardness of ductile iron, validating the results by means of a statistical method for hardness prediction. Ductile iron was subjected to austenitization at 950 °C for 120 min and then to austempering heat treatment in a salt bath at temperatures of 290, 320, 350 and 380 °C for 30, 60, 90 and 120 min. By increasing austempering temperature, a higher content of carbon-rich austenite was obtained, and the morphology of the thin acicular ferrite needles produced at 290 °C turned completely feathery at 350 and 380 °C. A thickening of acicular ferrite needles was also observed as austempering time increased. An inversely proportional behavior of hardness values was thus obtained, which was validated through data analysis, statistical tools and a regression model taking temperature and time austempering as input variables and hardness as the output variable, which achieved a correlation among variables of about 97%. The proposal of a mathematical model for the prediction of hardness in austempered ductile iron represents a numerical approximation which validates the experimental results at 95.20%.
In this research, the effect of the interelectrode distance (d) in the electrocoagulation (EC) reactor was studied. The experiments were carried out with varying d in values of 3, 5, and 9 mm during the treatment of water contaminated with fluoride (F−). The response variables analyzed were the treatment time necessary to reduce the residual concentration of F− to 1.5 mg L−1, the number of aluminum hydroxides formed, the potential drop in the reactor terminals, and the electric power consumption of the reactor. The software FLUENT version 6.3 was employed to simulate the liquid velocity profiles achieved in the reactor chamber. The results obtained show that the liquid velocity increases in the interelectrode spaces to 0.48, 0.65, and 0.86 m s−1 for interelectrode distances of 9, 5, and 3 mm, respectively, which favors not only the formation of flocs but also the elimination of fluoride. With a shorter interelectrode distance, the EC reactor not only consumes less electrical energy but also fewer electrodes, and the dispersion of generated flocs in the reactor chamber is major, which is more important than the quantity of flocs generated in it.
The investment casting process, also known as lost-wax casting, is widely used for producing ferrous and non-ferrous metal parts due to its excellent surface finish and dimensional accuracy. In recent years, the use of Co-Cr-Mo alloy has increased due to its high corrosion resistance, good biocompatibility, and relatively high wear resistance. Laser melting of materials has been demonstrated to refine the surface grain structure, reduce surface roughness, and improve both wear and corrosion resistance. The ability to fine-tune parameters such as laser power density and scanning speed facilitates the optimization of the treated layers’ thickness and homogeneity, thereby addressing many of the shortcomings inherent in conventional methods. This study investigates the microstructural, mechanical wear and bioactive behavior of investment-cast Co-Cr-Mo parts subjected to a Nd:YAG laser surface treatment. The effects of different processing parameters were analyzed quantitatively and comprehensively. The specimens were characterized using metallographic techniques, bioactivity evaluation, scanning electron microscopy (SEM), energy-dispersive X-ray spectroscopy (EDX), wear testing (Pin-on-Disk), and hardness testing. Our results demonstrate that Nd:YAG laser melting significantly enhances the surface properties and maintains the dimensional accuracy of complex Co-Cr-Mo biomedical components, through microstructural refinement, increased hardness, improved wear resistance, and preserved biocompatibility. The specific combination of investment casting with precisely controlled laser surface modification represents a significant advancement for improving the longevity and performance of biomedical implants.
Industrial wastewater can be reused in other everyday processes to help combat water scarcity worldwide. One contaminant in industrial wastewater is hexavalent chromium, which is highly toxic and can cause kidney, liver, and respiratory problems, making its removal vital. In this study, PLA-based films containing modified zirconia nanoparticles were developed via a solution-mixing process for hexavalent chromium adsorption. Obtaining the films involved two stages: the first was the chemical modification of ZrO2 nanoparticles with thiamine hydrochloride (vitamin B1) using fixed-frequency ultrasound at an output of 750 W and 50% amplitude for 60 min. The second stage involved preparing the films by mixing them in the solution using an ultrasonic bath. The nanoparticle concentrations were 0.25, 0.5, and 1 wt%. The results obtained from characterization using Fourier-transform infrared spectroscopy (FT-IR) revealed the characteristic bands of PLA and the characteristic peak of the Zr-O bond corresponding to the ZrO2 nanoparticles. Thermogravimetric analysis (TGA) showed that the ZrO2 nanoparticles provided thermal stability to the PLA polymer. X-ray diffraction (XRD) showed a broad peak of amorphous PLA at 16.8° and signals corresponding to the crystalline phase of ZrO2. The morphology of a cross-section of the films was observed using scanning electron microscopy (SEM), revealing a rough surface with pores. Finally, hexavalent chromium adsorption tests were carried out, measuring the adsorption efficiency under the parameters of pH, concentration, and contact time. The PLAZrO2 sample achieved an adsorption efficiency of 83% at pH 2.